# US 2023/0416887 A1 · Stainless steel alloys, turbocharger components formed from the stainless steel alloys, and methods for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0416887 A1
- Document ID: US20230416887A1
- Status: Published application
- Kind: A1
- Application number: 17/808,137
- Filed: 2022-06-22
- Published: 2023-12-28
- Earliest claimed: 2022-06-22
- Assignees: Garrett Transportation I Inc.
- Applicants: Garrett Transportation I Inc
- Inventors: Pavan Kumar Chintalapati; Philippe Renaud; Ragupathy Kannusamy
- Web page: https://patentgrep.com/patent/US20230416887A1

## CPC

- C22C 38/48: with niobium or tantalum
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D 6/004: {containing Cr and Ni}
- C22C 38/001: {containing N}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- F01D 25/007: {Preventing corrosion}
- F02B 37/18: by bypassing exhaust {from the inlet to the outlet of turbine or to the atmosphere}
- C21D 2211/001: Austenite
- F01D 25/005: {Selecting particular materials}
- F01D 25/24: Casings (modified for heating or cooling F01D25/14); Casing parts, e.g. diaphragms, casing fastenings (casings for rotary machines or engines in general F16M {; special arrangements in stators dealing with breaking-off of part of rotor F01D21/045})
- F05D 2220/40: in turbochargers
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F02B: INTERNAL-COMBUSTION PISTON ENGINES; COMBUSTION ENGINES IN GENERAL (gas-turbine plants F02C; hot-gas or combustion-product positive-displacement engine plants F02G)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

An austenitic stainless steel alloy includes, by weight, about 23.0% to about 25.0% chromium, about 8.5% to about 10.0% nickel, about 4.0% to about 5.0% manganese, about 0.8 to about 0.9% niobium, about 0.5% to about 1.5% silicon, about 0.35% to about 0.45% carbon, about 0.2% to about 0.3% nitrogen, and a balance of iron with inevitable/unavoidable impurities. The elements tungsten and molybdenum are excluded beyond impurity levels. In one example, a turbocharger turbine housing is made of the stainless steel alloy.

## Claims

### Claim 1

An austenitic stainless steel alloy, comprising, by weight:
23.0% to 25.0% chromium;
8.5% to 10.0% nickel;
4.0% to 5.0% manganese;
0.8% to 0.9% niobium;
0.8% to 1.2% silicon;
0.35% to 0.45% carbon;
0.22% to 0.28% nitrogen; and
a balance of iron with inevitable/unavoidable impurities,
wherein molybdenum, and tungsten are excluded from the alloy beyond impurity levels, wherein the austenitic stainless steel alloy has a nitrogen solubility at a temperature of 1700° C. that is defined by N=0.01*(−2.57+1.571*Cr−0.388*Ni+0.593*Mn−2.918*Si) and that is greater than 0.28% by weigh to prevent nitrogen porosity formation during the casting process, wherein N indicates % nitrogen by weight, Cr indicates % chromium by weight, Ni indicates % nickel by weight, Mn indicates % manganese by weight, and Si indicates % silicon by weight.

### Claim 2 (depends on 1)

The austenitic stainless steel alloy of claim 1, comprising 23.5% to 24.5% chromium.

### Claim 3 (depends on 1)

The austenitic stainless steel alloy of claim 1, comprising 8.8% to 9.7% nickel.

### Claim 4 (depends on 1)

The austenitic stainless steel alloy of claim 1, comprising 4.1% to 4.9% manganese.

### Claim 5

(canceled)

### Claim 6 (depends on 1)

The austenitic stainless steel alloy of claim 1, comprising 0.37% to 0.43% carbon.

### Claim 7

(canceled)

### Claim 8 (depends on 1)

The austenitic stainless steel alloy of claim 1, consisting of, by weight:
23.0% to 25.0% chromium;
8.5% to 10.0% nickel;
4.0% to 5.0% manganese;
0.8% to 0.9% niobium;
0.8% to 1.2% silicon;
0.35% to 0.45% carbon;
0.22% to 0.28% nitrogen; and
a balance of iron with inevitable/unavoidable impurities.

### Claim 9

A turbocharger turbine component comprising:
an austenitic stainless steel alloy, wherein the austenitic stainless steel alloy comprises, by weight:
23.0% to 25.0% chromium;
8.5% to 10.0% nickel;
4.0% to 5.0% manganese;
0.8% to 0.9% niobium;
0.8% to 1.2% silicon;
0.35% to 0.45% carbon;
0.22% to 0.28% nitrogen; and
a balance of iron with inevitable/unavoidable impurities,
wherein molybdenum, and tungsten are excluded from the alloy beyond impurity levels, wherein the austenitic stainless steel alloy has a nitrogen solubility at a temperature of 1700° C. that is defined by N=0.01*(−2.57+1.571*Cr−0.388*Ni+0.593*Mn−2.918*Si) and that is greater than 0.28% by weigh to prevent nitrogen porosity formation during the casting process, wherein N indicates % nitrogen by weight, Cr indicates % chromium by weight, Ni indicates % nickel by weight, Mn indicates % manganese by weight, and Si indicates % silicon by weight.

### Claim 10 (depends on 9)

The turbocharger turbine component of claim 9, wherein the austenitic stainless steel comprises 23.5% to 24.5% chromium.

### Claim 11 (depends on 9)

The turbocharger turbine component of claim 9, wherein the austenitic stainless steel alloy comprises 8.8% to 9.7% nickel.

### Claim 12 (depends on 9)

The turbocharger turbine component of claim 9, wherein the austenitic stainless steel alloy comprises 4.1% to 4.9% manganese.

### Claim 13

(canceled)

### Claim 14 (depends on 9)

The turbocharger turbine component of claim 9, wherein the austenitic stainless steel alloy comprises 0.37% to 0.43% carbon.

### Claim 15

(canceled)

### Claim 16 (depends on 9)

The turbocharger turbine component of claim 9, wherein the austenitic stainless steel alloy consists of, by weight:
23.0% to 25.0% chromium;
8.5% to 10.0% nickel;
4.0% to 5.0% manganese;
0.8% to 0.9% niobium;
0.8% to 1.2% silicon;
0.35% to 0.45% carbon;
0.22% to 0.28% nitrogen; and
a balance of iron with inevitable/unavoidable impurities.

### Claim 17 (depends on 9)

The turbocharger turbine component of claim 9, wherein the turbocharger turbine component comprises a turbocharger turbine housing.

### Claim 18 (depends on 9)

A vehicle comprising the turbocharger turbine component of claim 9.

### Claim 19

A method of making a turbocharger turbine component comprising forming the turbocharger turbine component using an austenitic stainless steel alloy, wherein the austenitic stainless steel alloy comprises, by weight:
23.0% to 25.0% chromium;
8.5% to 10.0% nickel;
4.0% to 5.0% manganese;
0.8% to 0.9% niobium;
0.8% to 1.2% silicon;
0.35% to 0.45% carbon;
0.22% to 0.28% nitrogen; and
a balance of iron with inevitable/unavoidable impurities,
wherein molybdenum, and tungsten are excluded from the alloy beyond impurity levels, wherein the austenitic stainless steel alloy has a nitrogen solubility at a temperature of 1700° C. that is defined by N=0.01*(−2.57+1.571*Cr−0.388*Ni+0.593*Mn−2.918*Si) and that is greater than 0.28% by weigh to prevent nitrogen porosity formation during the casting process, wherein N indicates % nitrogen by weight, Cr indicates % chromium by weight, Ni indicates % nickel by weight, Mn indicates % manganese by weight, and Si indicates % silicon by weight.