# US 2023/0416575 A1 · Method for manufacturing foldable backplate film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0416575 A1
- Document ID: US20230416575A1
- Status: Published application
- Kind: A1
- Application number: 18/254,786
- Filed: 2022-02-21
- Published: 2023-12-28
- Earliest claimed: 2021-02-24
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Hui Je LEE; Hyun Cheol KIM; In Hwan JEON; Sa Young JUNG; Jin Ho SON
- Web page: https://patentgrep.com/patent/US20230416575A1

## CPC

- C09J 7/201: {characterised by the release coating composition on the carrier layer}
- C09J 7/405: {characterised by the substrate of the release liner}
- B32B 7/06: permitting easy separation
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 27/08: of synthetic resin
- B32B 27/28: comprising synthetic resins not wholly covered by any one of the sub-groups {B32B27/30 - B32B27/42}
- B32B 37/12: characterised by using adhesives
- B32B 38/00: Ancillary operations in connection with laminating processes
- C09J 7/38: Pressure-sensitive adhesives [PSA]
- C09J 7/403: {characterised by the structure of the release feature}
- C09J 2301/122: the adhesive layer being present only on one side of the carrier, e.g. single-sided adhesive tape
- C09J 2301/302: the adhesive being pressure-sensitive, i.e. tacky at temperatures inferior to 30°C
- C09J 2301/312: parameters being the characterizing feature
- C09J 2301/50: characterized by process specific features
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

The present application relates to a method for manufacturing a foldable backplate film, and according to one aspect of the present invention, a method for manufacturing a foldable backplate film that the foldable backplate film is manufactured by a method of cutting it in a direction from the release film to the protective film upon half-cutting, and then release-changing the release film to an extended release film, whereby by improving a half-cutting process, the release film is not peeled off due to the sticking-out of the pressure-sensitive adhesive upon product handling and transportation, or the foldable backplate does not fall off upon the release film peeling, is provided.

## Claims

### Claim 1

A method for manufacturing a foldable backplate film comprising steps of:
preparing a foldable backplate comprising a base film and a pressure-sensitive adhesive layer provided on one side of the base film;
attaching a first release film to the opposite side of the side of the pressure-sensitive adhesive layer that is in contact with the base film;
attaching a protective film to the opposite side of the side of the base film that is in contact with the pressure-sensitive adhesive layer;
half-cutting the foldable backplate in a direction from the first release film to the protective film along a cutting line dividing a body part and a pad part;
peeling the first release film from the pressure-sensitive adhesive layer after the half-cutting step; and
attaching a non-cut second release film to the position where the first release film has been peeled off to manufacture the foldable backplate film,
wherein at least one width of the second release film is greater than the width of the foldable backplate.

### Claim 2 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein a difference between the at least one width of the second release film and the width of the foldable backplate is in a range of 0.1 mm to 20 mm.

### Claim 3 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein an edge of the non-cut second release film is extended to the outside of the foldable backplate, and the extended length is in a range of 0.1 mm to 10 mm.

### Claim 4 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein in the half-cut foldable backplate,
each of the first release film, the base film and the pressure-sensitive adhesive layer comprises a penetration regions penetrated along the cutting line, and
the protective film has a groove formed along the cutting line.

### Claim 5 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein the foldable backplate film has a structure in which the second release film, the pressure-sensitive adhesive layer, the base film and the protective film are sequentially laminated,
each of the pressure-sensitive adhesive layer and the base film comprises a penetration regions along the cutting line,
the protective film comprises a groove along the cutting line, and
the second release film does not comprise a penetration region or a groove formed along the cutting line.

### Claim 6 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein the base film has an elongation at break of 20% or more and 200% or less at 20° C.

### Claim 7 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein the base film has a thermal contraction rate of 0.1% or less at 200° C.

### Claim 8 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein the base film is a polyimide base film.

### Claim 9 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein the base film has a thickness of 20 μm or more and 120 μm or less.

### Claim 10 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein the peel force of the first release film from the pressure-sensitive adhesive layer is 12 gf/inch or less at 23° C.

### Claim 11 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein the first release film and the second release film are silicone series.

### Claim 12 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein the first release film and the second release film have a surface resistance of 1010 Ω/sq or less under a condition of 500V or less.

### Claim 13 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein the protective film has a groove formed along the cutting line.

### Claim 14 (depends on 5)

The method for manufacturing a foldable backplate film according to claim 5, wherein the penetration region of the base film is a first penetration region that is in communication with groove in the protective film and the penetration region of the pressure-sensitive adhesive layer is a second penetration region that is in communication with the first penetration region.

### Claim 15 (depends on 1)

The method for manufacturing a foldable backplate film according to claim 1, wherein the base film has a storage elastic modulus of 1 GPa to 5 GPa at 20° C.