# US 2023/0416556 A1 · Laminate and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0416556 A1
- Document ID: US20230416556A1
- Status: Published application
- Kind: A1
- Application number: 18/241,465
- Filed: 2023-09-01
- Published: 2023-12-28
- Earliest claimed: 2021-03-05
- Assignees: Kaneka Corporation
- Applicants: Kaneka Corporation
- Inventors: Hanako Hasebe; Haruki Koyama; Yukihiro Shimamoto
- Web page: https://patentgrep.com/patent/US20230416556A1

## CPC

- C08J 7/042: {with two or more layers, where at least one layer of a composition contains a polymer binder}
- C09D 133/18: Homopolymers or copolymers of nitriles
- B05D 1/00: Processes for applying liquids or other fluent materials (B05D5/00, B05D7/00 take precedence)
- B32B 27/08: of synthetic resin
- B32B 27/16: specially treated, e.g. irradiated
- B32B 27/20: using fillers, pigments, thixotroping agents
- B32B 27/30: comprising vinyl {(co)polymers; comprising acrylic (co)polymers}
- B32B 27/308: {comprising acrylic (co)polymers}
- C08J 7/0427: {with only one layer of a composition containing a polymer binder (with more layers C08J7/042)}
- C08J 7/046: Forming abrasion-resistant coatings; Forming surface-hardening coatings
- C08K 3/36: Silica
- C09D 4/00: Coating compositions, e.g. paints, varnishes or lacquers, based on organic non-macromolecular compounds having at least one polymerisable carbon-to-carbon unsaturated bond {; Coating compositions, based on monomers of macromolecular compounds of groups C09D183/00 - C09D183/16}
- B05D 7/04: to surfaces of films or sheets (producing layered products by applying coatings of pasty or pulverulent plastics B29C41/00)
- B05D 7/546: {each layer being cured, at least partially, separately}
- B05D 2201/04: Laminate
- B05D 2502/00: Acrylic polymers
- B32B 2255/10: on synthetic resin layer or on natural or synthetic rubber layer
- B32B 2255/26: Polymeric coating
- B32B 2307/412: Transparent
- B32B 2307/536: Hardness
- C08J 2333/12: Homopolymers or copolymers of methyl methacrylate
- C08J 2433/04: esters
- C08J 2451/06: grafted on to homopolymers or copolymers of aliphatic hydrocarbons containing only one carbon-to-carbon double bond
- C08J 2475/14: Polyurethanes having carbon-to-carbon unsaturated bonds
- C08K 7/26: Silicon- containing compounds
- C08K 2201/011: Nanostructured additives
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A laminate having excellent moldability and including an acrylic-based resin film is provided. A method for producing a laminate having a specific crack elongation, includes a step (A) of forming, on at least one side of a specific acrylic-based resin film, a hard coat layer that contains a urethane acrylate resin, and a step (B) of forming, on the hard coat layer obtained in the step (A), a low refractive index layer that contains, in an amount of not less than 40%, hollow fine silica particles having a particle size of less than 100 nm and that contains an acrylate-based resin.

## Claims

### Claim 1

A method for producing a laminate, comprising:
a hard coat layer forming step (A1) of irradiating a resin layer, containing a urethane acrylate resin, that has been applied to at least one side of an acrylic-based resin film, with an active energy ray to cure the resin layer containing the urethane acrylate resin thereby obtaining a hard coat layer; and
a low refractive index layer forming step (B1) of applying, an acrylate-based resin containing hollow fine silica particles having a particle size of less than 100 nm in an amount of not less than 40%, onto the hard coat layer obtained in the step (A1) and irradiating a resultant resin layer that contains the acrylate-based resin with an active energy ray to cure the resin layer that contains the acrylate-based resin,
wherein
the acrylic-based resin film has a tensile breaking elongation of not less than 170% at 120° C., and
the laminate has a crack elongation of not less than 80% at 120° C.

### Claim 2 (depends on 1)

The method according to claim 1, wherein:
the acrylic-based resin film is obtained by molding an acrylic resin composition that contains a thermoplastic acrylic polymer and polymer particles containing a crosslinked elastomer; and
the thermoplastic acrylic polymer is constituted by 50% by mass to 100% by mass of a methyl methacrylate unit and 0% by mass to 50% by mass of another structural unit, and a total amount of the methyl methacrylate unit and said another structural unit in the thermoplastic acrylic polymer is 100% by mass.

### Claim 3 (depends on 2)

The method according to claim 2, wherein:
the crosslinked elastomer contains not less than 50% by mass of an acrylic ester unit in 100% by mass of the crosslinked elastomer; and
the polymer particles are graft copolymer particles containing the crosslinked elastomer and a graft polymer layer located closer to a surface layer than the crosslinked elastomer.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the resin layer containing the urethane acrylate resin further contains particles.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the particles are inorganic oxide particles and/or crosslinked organic resin particles.

### Claim 6 (depends on 4)

The method according to claim 4, wherein the particles are at least one selected from the group consisting of silica, alumina, zirconia, a crosslinked silicone resin, a crosslinked acrylic resin, and a crosslinked aromatic vinyl resin.

### Claim 7 (depends on 4)

The method according to claim 4, wherein at least a part of the particles contains, on a surface thereof, a reactive functional group that has reactivity with the urethane acrylate resin.

### Claim 8 (depends on 4)

The method according to claim 4, wherein:
the particles are contained in an amount of 2.0% by weight to 5.0% by weight with respect to the hard coat layer that has been cured;
d≤r is satisfied, where r (μm) is an average dispersed particle size of the particles, and d (μm) is a thickness of the hard coat layer;
the laminate has a pencil hardness of not less than H, a haze of not less than 3%, and a crack elongation of not less than 170% at 120° C.; and
a laminated film obtained by laminating a resin layer not containing the particles on the acrylic-based resin film has a crack elongation of not less than 80% at 120° C.

### Claim 9 (depends on 1)

The method according to claim 1, wherein a cumulative light amount in an irradiation with the active energy ray in the step (A1) is 150 mJ/cm2 to 500 mJ/cm2.

### Claim 10 (depends on 1)

The method according to claim 1, further comprising:
an additional step (B1′) of preparing the acrylate-based resin that contains the hollow fine silica particles having a particle size of less than 100 nm in an amount of not less than 40% by adding solvent to the acrylate-based resin which is a material for a low refractive index layer before the step (B1), wherein
the solvent contains one or more types of solvents, and a solvent having a highest boiling point among the one or more types of solvents has a boiling point of 115° C. to 180° C.

### Claim 11 (depends on 1)

The method according to claim 1, wherein, in a laminated film obtained by laminating the low refractive index layer on the acrylic-based resin film, a Δhaze after 20% stretching at 120° C. is not more than 30%.

### Claim 12

A method for producing a laminate, comprising:
a hard coat layer forming step (A1) of irradiating a resin layer, containing urethane acrylate resin, that has been applied to at least one side of an acrylic-based resin film, with an active energy ray to cure the resin layer containing the urethane acrylate resin thereby obtaining a hard coat layer;
wherein
the acrylic-based resin film has a tensile breaking elongation of not less than 170% at 120° C., and the hard coat layer contains the urethane acrylate resin, and
the laminate has a crack elongation of not less than 80% at 120° C.

### Claim 13 (depends on 12)

The method according to claim 12, wherein, in the laminate, a Δhaze is less than 8.0% when a stretching ratio is 80% at 120° C.

### Claim 14 (depends on 12)

The method according to claim 12, wherein:
the acrylic-based resin film is obtained by molding an acrylic resin composition that contains a thermoplastic acrylic polymer and polymer particles containing a crosslinked elastomer; and
the thermoplastic acrylic polymer is constituted by 50% by mass to 100% by mass of a methyl methacrylate unit and 0% by mass to 50% by mass of another structural unit, and a total amount of the methyl methacrylate unit and said another structural unit in the thermoplastic acrylic polymer is 100% by mass.

### Claim 15 (depends on 14)

The method according to claim 14, wherein:
the crosslinked elastomer contains not less than 50% by mass of an acrylic ester unit in 100% by mass of the crosslinked elastomer; and
the polymer particles are graft copolymer particles containing the crosslinked elastomer and a graft polymer layer which is located closer to a surface layer than the crosslinked elastomer.

### Claim 16

A laminate comprising:
an acrylic-based resin film; and
a hard coat layer that is laminated on at least one side of the acrylic-based resin film,
wherein
the acrylic-based resin film has a tensile breaking elongation of not less than 170% at 120° C.,
the hard coat layer contains a urethane acrylate resin, and
the laminate has a pencil hardness of not less than H, and a crack elongation of not less than 80% at 120° C.

### Claim 17 (depends on 16)

The laminate according to claim 16, wherein the hard coat layer further contains particles.

### Claim 18 (depends on 17)

The laminate according to claim 17, wherein the particles are inorganic oxide particles and/or crosslinked organic resin particles.

### Claim 19 (depends on 17)

The laminate according to claim 17, wherein the particles are at least one selected from the group consisting of silica, alumina, zirconia, a crosslinked silicone resin, a crosslinked acrylic resin, and a crosslinked aromatic vinyl resin.

### Claim 20 (depends on 17)

The laminate according to claim 17, wherein at least a part of the particles contains, on a surface thereof, a reactive functional group that has reactivity with the urethane acrylate resin.

### Claim 21 (depends on 16)

The laminate according to claim 16, further comprising a low refractive index layer on the hard coat layer, wherein the low refractive index layer contains an acrylate-based resin that contains hollow fine silica particles having a particle size of less than 100 nm in an amount of not less than 40%.

### Claim 22 (depends on 21)

The laminate according to claim 21, wherein the laminate has a luminous reflectance of not more than 2.0%.

### Claim 23 (depends on 21)

The laminate according to claim 21, wherein an in-plane phase difference (Re) is not more than 10 nm, and an absolute value of a thickness-direction phase difference (Rth) is not more than 30 nm.

### Claim 24 (depends on 16)

The laminate according to claim 16, wherein a Δhaze is less than 8.0% when a stretching ratio at 120° C. is 80%.

### Claim 25 (depends on 16)

The laminate according to claim 16, wherein a Δhaze is not more than 3.0% when a stretching ratio at 120° C. is 80%.

### Claim 26 (depends on 21)

The laminate according to claim 21, wherein when a stretching ratio is 80% at 120° C., a microcrack width in a direction parallel to tensile stress of the low refractive index layer is not more than 2.0 μm.

### Claim 27 (depends on 21)

The laminate according to claim 21, wherein when a stretching ratio is 80% at 120° C., a depth of a groove of a microcrack from a low refractive index layer-side surface of the laminate at a microcrack part in a direction parallel to tensile stress of the low refractive index layer is not more than 1.0 μm.

### Claim 28 (depends on 16)

A molded product comprising the laminate according to claim 16.

### Claim 29 (depends on 16)

A molded product, wherein the molded product is obtained by laminating the laminate according to claim 16 on at least part of a surface of a molded product which at least partially has a non-planar shape.

### Claim 30

A method for producing a laminate, comprising:
a hard coat layer forming step (A2) of irradiating a resin layer, containing a urethane acrylate resin and particles, that has been applied to at least one side of an acrylic-based resin film with an active energy ray to cure the resin layer containing the urethane acrylate resin and the particles, thereby obtaining a hard coat layer;
wherein
the acrylic-based resin film has a tensile breaking elongation of not less than 170% at 120° C.,
the particles are contained in an amount of 2.0% by weight to 5.0% by weight with respect to the hard coat layer that has been cured,
d≤r is satisfied, where r (μm) is an average dispersed particle size of the particles, and d (μm) is a thickness of the hard coat layer,
the laminate has a pencil hardness of not less than H, a haze of not less than 3%, and a crack elongation of not less than 170% at 120° C., and
a laminated film obtained by laminating, on the acrylic-based resin film, a resin layer not containing the particles has a crack elongation of not less than 80% at 120° C.

### Claim 31 (depends on 30)

The method according to claim 30, wherein in the laminate, a Δhaze is less than 8.0% when a stretching ratio at 120° C. is 80%.

### Claim 32

A laminate comprising:
an acrylic-based resin film; and
a hard coat layer that is laminated on at least one side of the acrylic-based resin film, wherein
the acrylic-based resin film has a tensile breaking elongation of not less than 170% at 120° C.,
the hard coat layer contains a urethane acrylate resin and particles,
d≤r is satisfied, where r (μm) is an average dispersed particle size of the particles, and d (μm) is a thickness of the hard coat layer,
the laminate has a pencil hardness of not less than H and a haze of not less than 3%, and
a laminated film obtained by laminating, on the acrylic-based resin film, a resin layer not containing the particles has a crack elongation of not less than 80% at 120° C.

### Claim 33 (depends on 32)

The laminate according to claim 32, wherein in the laminate, a Δhaze is less than 8.0% when a stretching ratio is 80% at 120° C.