# US 2023/0416506 A1 · Nitrile rubber-based composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0416506 A1
- Document ID: US20230416506A1
- Status: Published application
- Kind: A1
- Application number: 18/036,962
- Filed: 2021-11-04
- Published: 2023-12-28
- Earliest claimed: 2020-11-16
- Assignees: Nok Corporation
- Applicants: Nok Corporation
- Inventors: Shunsuke ABE
- Web page: https://patentgrep.com/patent/US20230416506A1

## CPC

- C08L 9/02: Copolymers with acrylonitrile
- H01F 1/0533: {in a bonding agent}
- C08K 3/08: Metals
- C08K 5/5419: containing at least one Si—C bond
- C08K 9/06: with silicon-containing compounds
- H01F 1/117: Flexible bodies
- H01F 41/0273: {Imparting anisotropy (methods and devices for magnetising permanent magnets H01F13/003)}
- C08K 2003/0856: {Iron}
- C08K 2201/005: Additives being defined by their particle size in general
- C08K 2201/01: Magnetic additives
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A nitrile rubber-based composition comprising 1,000 to 2,500 parts by weight of a magnetic powder or silylated magnetic powder having a compressed density of 3.4 to 3.7 g/cm3, 0.5 to 20 parts by weight of alkoxyalkylsilane, and 8 to 40 parts by weight of a plasticizer, based on 100 parts by weight of nitrile rubber, hydrogenated nitrile rubber, or blend rubber thereof. The nitrile rubber-based composition that does not cause deterioration in roll processability and in adhesion between an adhesive applied to a metal plate and the rubber, even when a magnetic powder is added at a ratio as high as 1,000 parts by weight or more based on 100 parts by weight of nitrile rubber, hydrogenated nitrile rubber, or blend rubber thereof.

## Claims

### Claim 1

A nitrile rubber-based composition comprising 1,000 to 2,500 parts by weight of a magnetic powder or silylated magnetic powder having a compressed density of 3.4 to 3.7 g/cm3, 0.5 to 20 parts by weight of alkoxyalkylsilane, and 8 to 40 parts by weight of a plasticizer, based on 100 parts by weight of nitrile rubber, hydrogenated nitrile rubber, or blend rubber thereof.

### Claim 2 (depends on 1)

The nitrile rubber-based composition according to claim 1, wherein alkoxyalkylsilane is used at a ratio of 0.5 to 1.0 parts by weight based on 1,000 parts by weight to less than 1300 parts by weight of the magnetic powder.

### Claim 3 (depends on 1)

The nitrile rubber-based composition according to claim 1, wherein alkoxyalkylsilane is used at a ratio of 1.0 to 2.0 parts by weight based on 1,300 parts by weight to less than 1700 parts by weight of the magnetic powder.

### Claim 4 (depends on 1)

The nitrile rubber-based composition according to claim 1, wherein alkoxyalkylsilane is used at a ratio of 2.0 to 10 parts by weight based on 1,700 parts by weight to less than 2,000 parts by weight of the magnetic powder.

### Claim 5 (depends on 1)

The nitrile rubber-based composition according to claim 1, wherein alkoxyalkylsilane is used at a ratio of 10 to 20 parts by weight based on 2,000 to 2,500 parts by weight of the magnetic powder.

### Claim 6 (depends on 1)

The nitrile rubber-based composition according to claim 1, wherein millable type nitrile rubber having a Mooney viscosity ML1+4 (100° C.) of 20 to 50 is used.

### Claim 7 (depends on 1)

The nitrile rubber-based composition according to claim 1, wherein a magnetic powder having two particle size distribution peaks at 1 to 2 m and 2 to 4 m is used.

### Claim 8 (depends on 1)

The nitrile rubber-based composition according to claim 1, wherein the magnetic powder having a compressed density of 3.4 to 3.7 g/cm3 is at least one of a ferrite magnet and a rare-earth magnet.

### Claim 9 (depends on 8)

The nitrile rubber-based composition according to claim 8, wherein the ferrite magnet is a strontium ferrite or a barium ferrite.

### Claim 10 (depends on 1)

The nitrile rubber-based composition according to claim 1, wherein alkoxyalkylsilane is trialkoxyoctylsilane.

### Claim 11 (depends on 1)

The nitrile rubber-based composition according to claim 1, which is applied as a vulcanization molding material of rubber magnet for sensor used in magnetic encoders.

### Claim 12 (depends on 11)

A rubber magnet for sensor, which is a vulcanization-molded product of the nitrile rubber-based composition according to claim 11.

### Claim 13 (depends on 12)

A magnetic encoder composed of the rubber magnet for sensor according to claim 12.

### Claim 14 (depends on 13)

The magnetic encoder according to claim 13, which is used in an encoder part of a wheel speed sensor.

### Claim 15 (depends on 14)

The magnetic encoder according to claim 14, wherein the encoder comprises an annular magnetic rubber molded product mounted on a support member capable of being attached to a rotating body, and single or multiple N pole and S pole are magnetized in the circumferential direction.

### Claim 16

A method for producing a rubber magnet for sensor, comprising vulcanizing a nitrile rubber-based composition in a mold to which a magnetic field is applied, wherein the composition comprises 1,000 to 2,500 parts by weight of a magnetic powder or silylated magnetic powder having a compressed density of 3.4 to 3.7 g/cm3, 0.5 to 20 parts by weight of alkoxyalkylsilane, and 8 to 40 parts by weight of a plasticizer, based on 100 parts by weight of nitrile rubber, hydrogenated nitrile rubber, or blend rubber thereof.