Abstract
The present invention relates to a continuous process for the production of polyol modified polyalkenylene terephthalates and the application of such polyol modified polyalkylene therephtalate on wire enamels.
Claims12
A process for dissolving a polyol modified polyalkylene terephthalate, the process comprising:
- dissolving a polyol modified polyalkylene terephthalate in a solvent to produce a dissolved polyol modified polyalkylene terephthalate,
- the polyol modified polyalkylene terephthalate having been obtained by a continuous process comprising:
- introducing components in a continuous reactor comprising a reaction zone, the components including a polyalkylene terephthalate, a polyol, and a transesterification catalyst;
- reacting the components in the reaction zone of the reactor at a temperature in the range of 180° C. to 350° C. to produce the polyol modified polyalkylene terephthalate;
- wherein the polyol includes one or more of tris(2-hydroxyethyl) isocyanurate and glycerine, and
- wherein reacting the components is performed in a melt of the polyalkylene terephthalate.
3 more elements
A process for applying a polyol modified polyalkylene terephthalate on a wire, the process comprising:
- applying a polyol modified polyalkylene terephthalate on a wire,
- the polyol modified polyalkylene terephthalate having been obtained by a continuous process comprising:
- introducing components in a continuous reactor comprising a reaction zone, the components including a polyalkylene terephthalate, a polyol, and a transesterification catalyst;
- reacting the components in the reaction zone of the reactor at a temperature in the range of 180° C. to 350° C. to produce the polyol modified polyalkylene terephthalate;
- wherein the polyol includes one or more of tris(2-hydroxyethyl) isocyanurate and glycerine, and
- wherein reacting the components is performed in a melt of the polyalkylene terephthalate.
3 more elements
A polyol modified polyalkylene terephthalate prepared by a continuous process comprising:
- introducing components in a continuous reactor comprising a reaction zone, the components including a polyalkylene terephthalate, a polyol, and a transesterification catalyst;
- reacting the components in the reaction zone of the reactor at a temperature in the range of 180° C. to 350° C. to produce the polyol modified polyalkylene terephthalate;
- wherein the polyol includes one or more of tris(2-hydroxyethyl) isocyanurate and glycerine, and
- wherein reacting the components is performed in a melt of the polyalkylene terephthalate.
1 more element