# US 2023/0415405 A1 · Stereolithography additive manufacturing of photoaligned liquid crystal elastomers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0415405 A1
- Document ID: US20230415405A1
- Status: Published application
- Kind: A1
- Application number: 18/237,836
- Filed: 2023-08-24
- Published: 2023-12-28
- Earliest claimed: 2022-06-23
- Assignees: Lawrence Livermore National Security, LLC
- Applicants: Lawrence Livermore National Security, LLC
- Inventors: Bryan D. Moran; Elaine Lee; Caitlyn Christian Krikorian; Logan Bekker
- Web page: https://patentgrep.com/patent/US20230415405A1

## CPC

- B29C 64/129: characterised by the energy source therefor, e.g. by global irradiation combined with a mask
- B29C 64/124: using layers of liquid which are selectively solidified
- B33Y 10/00: Processes of additive manufacturing
- B33Y 30/00: Apparatus for additive manufacturing; Details thereof or accessories therefor
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B33Y 80/00: Products made by additive manufacturing
- B29K 2105/0079: {Liquid crystals}
- C09K 19/52: characterised by components which are not liquid crystals, e.g. additives {with special physical aspect: solvents, solid particles}
- C09K 2019/0448: {the end chain group being a polymerizable end group, e.g. -Sp-P or acrylate}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A product includes a three-dimensional structure having a plurality of sequentially-formed layers comprised of liquid crystal elastomers. The liquid crystal elastomers in a portion of a first of the layers are substantially aligned in a predefined first orientation and the liquid crystal elastomers in a portion of a second of the layers are substantially aligned in a predefined second orientation that is different than the first orientation. Each of the portions of the three-dimensional structure is characterized as exhibiting a shape change in response to a stimulus, wherein the shape change is reversible. The product includes a contiguous region of aligned liquid crystal elastomers in one of the portions having a maximum dimension of less than 60 microns.

## Claims

### Claim 1

A product, comprising:
a three-dimensional structure having a plurality of sequentially-formed layers comprised of liquid crystal elastomers,
wherein the liquid crystal elastomers in a portion of a first of the layers are substantially aligned in a predefined first orientation,
wherein the liquid crystal elastomers in a portion of a second of the layers are substantially aligned in a predefined second orientation that is different than the first orientation,
wherein each of the portions of the three-dimensional structure is characterized as exhibiting a shape change in response to a stimulus, wherein the shape change is reversible,
wherein a contiguous region of aligned liquid crystal elastomers in one of the portions has a maximum dimension of less than 60 microns.

### Claim 2 (depends on 1)

The product as recited in claim 1, wherein the predefined first orientation of alignment is different than the orientation of the as-deposited alignment of the liquid crystal elastomers.

### Claim 3 (depends on 1)

The product as recited in claim 1, wherein a second portion of the first of the layers has liquid crystal elastomers aligned in a predefined third orientation that is different than the first orientation.

### Claim 4 (depends on 1)

The product as recited in claim 1, wherein the three-dimensional structure comprises at least three layers, each layer having a cured portion of cured liquid crystal elastomers, the cured portions being stacked upon one another in a direction perpendicular to a plane of the layers.

### Claim 5 (depends on 4)

The product as recited in claim 4, wherein the orientation of the aligned liquid crystal elastomers in each of the cured portions is different from the respective orientations of the aligned liquid crystal elastomers in the other cured portions.

### Claim 6 (depends on 1)

The product as recited in claim 1, wherein the three-dimensional structure is a printed three-dimensional structure formed using a lithography-based additive manufacturing system.

### Claim 7 (depends on 1)

A method of forming the product recited in claim 1,
contacting a first layer of resin with a layer of photoalignment material, the resin comprising liquid crystal oligomers and a photoinitiator;
exposing a first portion of the layer of photoalignment material to a first light for aligning the first portion of the layer of photoalignment material in a first orientation corresponding to a polarity of the first light,
wherein the liquid crystal oligomers adjacent the illuminated first portion of the layer of photoalignment material align to the first orientation of the first portion of the layer of photoalignment material;
exposing the aligned liquid crystal oligomers of the first layer of resin for curing the aligned liquid crystal oligomers thereby forming the portion of the first of the layers;
creating a relative movement of the first layer away from the photoalignment material;
contacting a second layer of the resin positioned between the previously-formed layer of resin and the layer of photoalignment material with the layer of photoalignment material;
exposing another portion of the layer of photoalignment material to the first light for aligning the another portion of the layer of photoalignment material in an orientation that is different than the first orientation,
wherein the liquid crystal oligomers adjacent the illuminated another portion of the layer of photoalignment material align to the orientation of the another portion of the layer of photoalignment material; and
exposing the aligned liquid crystal oligomers of the second of the layers for curing the aligned liquid crystal oligomers thereby forming the portion of the second of the layers of resin.

### Claim 8 (depends on 7)

The method as recited in claim 7, wherein the orientation(s) of alignment in each layer of resin correspond to a predefined pattern of an associated layer of a three-dimensional model, wherein molecules of the photoalignment material are aligned in the respective orientation corresponding to a polarity of the first light applied thereto as defined, at least in part, by a rotational orientation of the polarizer in the path of the first light.

### Claim 9 (depends on 8)

The method as recited in claim 8, wherein a polarization angle of the first light is selected to specify each orientation of alignment corresponding to the predefined pattern of an associated layer of the three-dimensional model.

### Claim 10 (depends on 9)

The method as recited in claim 9, wherein a minimum difference between the polarization angles of two respective orientations is at least one degree.

### Claim 11 (depends on 7)

The method as recited in claim 7, comprising, after exposing the first portion of the layer of photoalignment material to the first light and before curing the aligned liquid crystal oligomers of the first layer:
changing a polarity of the first light; and
exposing a next portion of the layer of the photoalignment material to the first light for aligning the next portion of the layer of photoalignment material in a different orientation than the first orientation,
wherein the liquid crystal oligomers adjacent the illuminated next portion of the layer of the photoalignment material align to the different orientation of the next portion of the layer of photoalignment material.

### Claim 12 (depends on 11)

The method as recited in claim 11, wherein the next portion of the layer of photoalignment material is located by moving the layer of photoalignment material in an x-direction and/or a y-direction, and the x-y directions are in a plane that is perpendicular to a z-direction, wherein the next portion of the layer of photoalignment material comprises unaligned molecules.

### Claim 13 (depends on 7)

The method as recited in claim 7, wherein a wavelength of the first light for aligning molecules of the photoalignment material is in a range of greater than about 390 nanometers to about 500 nanometers.

### Claim 14 (depends on 7)

The method as recited in claim 7, wherein the curing the aligned liquid crystal oligomers comprises exposing the aligned liquid crystal oligomers to a second light at a wavelength in a range of greater than about 350 nanometers to about 390 nanometers.

### Claim 15 (depends on 7)

The method as recited in claim 7, wherein the photoinitiator does not initiate polymerization of the resin at a wavelength of the first light.

### Claim 16 (depends on 7)

The method as recited in claim 7, wherein a composition of the photoalignment material includes at least one component selected from the group consisting of: azobenzene and an organogel.

### Claim 17 (depends on 7)

The method as recited in claim 7, comprising heating the resin to a temperature below the nematic-to-isotropic transition temperature of the liquid crystal oligomers for lowering a viscosity of the resin.

### Claim 18 (depends on 7)

The method as recited in claim 7, comprising using a digital micromirror device to define the portions of the layer of photoalignment material for exposure to the first light.

### Claim 19 (depends on 7)

The method as recited in claim 7, wherein each cured portion comprises at least one voxel.

### Claim 20 (depends on 7)

The method as recited in claim 7, wherein the resin includes a photoinhibitor.