# US 2023/0415127 A1 · Methods of Preparing a Catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0415127 A1
- Document ID: US20230415127A1
- Status: Published application
- Kind: A1
- Application number: 18/242,799
- Filed: 2023-09-06
- Published: 2023-12-28
- Earliest claimed: 2015-09-18
- Assignees: Chevron Phillips Chemical Company LP
- Applicants: Chevron Phillips Chemical Company LP
- Inventors: Jeremy M. PRAETORIUS; Eric D. SCHWERDTFEGER; Max P. MCDANIEL; Ted H. CYMBALUK; Connor D. BOXELL; Alan L. SOLENBERGER; Kathy S. CLEAR
- Web page: https://patentgrep.com/patent/US20230415127A1

## CPC

- B01J 23/26: Chromium
- B01J 21/08: Silica
- B01J 35/615: {100-500 m2/g}
- B01J 35/617: {500-1000 m2/g}
- B01J 35/638: {more than 1.0 ml/g}
- B01J 37/0203: {the impregnation liquid containing organic compounds}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C08F 10/02: Ethene
- C08F 110/02: Ethene
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A method comprising a) drying a support material comprising silica at temperature in the range of from about 150° C. to about 220° C. to form a dried support; b) contacting the dried support with methanol to form a slurried support; c) subsequent to b), cooling the slurried support to a temperature of less than about 60° C. to form a cooled slurried support; d) subsequent to c), contacting the cooled slurried support with a titanium alkoxide to form a titanated support; and e) thermally treating the titanated support by heating to a temperature of equal to or greater than about 150° C. for a time period of from about 5 hours to about 30 hours to remove the methanol and yield a dried titanated support.

## Claims

### Claim 1

A method comprising:
a) drying a silica support at a temperature in a range of from about 150° C. to about 220° C. to form a dried support;
b) contacting the dried support with a chromium-containing compound to form a chrominated support;
c) contacting the chrominated support with a solvent to form a slurried support;
d) cooling the slurried support to a temperature of less than about 60° C. to form a cooled support;
e) contacting the cooled support with a titanium-containing compound to form a titanated support;
f) thermally treating the titanated support by increasing the temperature of the titanated support to the boiling point of the solvent;
g) prior to removing all of the solvent, contacting the titanated support with water in an amount ranging from about 0.1 moles to about 10 moles per mole of titanium to produce a mixture;
h) thermally treating the mixture by heating the mixture to a temperature of about 150° C. for a time period of from about 5 hours to about 30 hours to form a precatalyst; and
i) calcining the precatalyst at a temperature in the range of from about 400° C. to about 1000° C. for a time period of from about 30 minutes to about 24 hours to form a polymerization catalyst.

### Claim 2 (depends on 1)

The method of claim 1 wherein the solvent comprises methanol having less than about 0.1 wt. % water.

### Claim 3 (depends on 1)

The method of claim 1 wherein the titanium-containing compound comprises titanium n-propoxide.

### Claim 4 (depends on 2)

The method of claim 2 wherein the titanium-containing compound comprises titanium n-propoxide.

### Claim 5 (depends on 1)

The method of claim 1 wherein the chromium-containing compound comprises basic chromium acetate.

### Claim 6 (depends on 4)

The method of claim 4 wherein the chromium-containing compound comprises basic chromium acetate.

### Claim 7 (depends on 6)

The method of claim 6 wherein the slurried support is cooled to a temperature of less than about 50° C. to form the cooled support.

### Claim 8 (depends on 6)

The method of claim 6 wherein the slurried support is cooled to a temperature of less than about 40° C. to form the cooled support.

### Claim 9 (depends on 1)

The method of claim 1 wherein step (e) is performed under vigorous mixing conditions suitable to provide for efficient dispersal of the titanium-containing compound.

### Claim 10 (depends on 8)

The method of claim 8 wherein step (e) is performed under vigorous mixing conditions suitable to provide for efficient dispersal of the titanium-containing compound.

### Claim 11 (depends on 2)

The method of claim 2 wherein the solvent is present in an amount ranging from about 2 times to about 3 times weight of the dried support.

### Claim 12 (depends on 10)

The method of claim 10 wherein the solvent is present in an amount ranging from about 2 times to about 3 times weight of the dried support.

### Claim 13 (depends on 11)

The method of claim 11 wherein the support material is dried for a time period ranging from about 5 hours to about 24 hours.

### Claim 14 (depends on 12)

The method of claim 12 wherein the support is dried in an inert atmosphere.

### Claim 15 (depends on 1)

The method of claim 1 wherein step (c) is repeated from about 2 to about 10 times.

### Claim 16 (depends on 1)

The method of claim 1 wherein the silica support contains greater than about 50% silica and the silica support is characterized by a surface area of from about 250 m2/g to about 1000 m2/g and a pore volume of from about 1.0 cm3/gram to about 2.5 cm3/gram.

### Claim 17 (depends on 1)

The method of claim 1 wherein calcining the precatalyst is in air, oxygen, inert gases, carbon monoxide or a combination thereof.

### Claim 18 (depends on 1)

The method of claim 1 wherein the amount of water added in step g) is from about 2 moles to about 5 moles per mole of titanium.

### Claim 19 (depends on 1)

The method of claim 1 wherein an amount of volatile organic compounds (VOC) emitted during the calcining is reduced by from about 50% to about 100% when compared to the amount of VOC emitted during calcining of a similar precatalyst prepared without the addition of water to the titanated slurried support.

### Claim 20 (depends on 1)

The method of claim 1 wherein an amount of volatile organic compounds (VOC) emitted during calcining is less than about 2 wt. %.