# US 2023/0415101 A1 · Metal-organic framework material separation membrane, preparation method therefor, and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0415101 A1
- Document ID: US20230415101A1
- Status: Published application
- Kind: A1
- Application number: 18/248,754
- Filed: 2020-10-28
- Published: 2023-12-28
- Earliest claimed: 2020-10-15
- Assignees: China Petroleum & Chemical Corporation; Beijing Research Institute of Chemical Industry, China Petroleum & Chemical Corporation
- Applicants: China Petroleum & Chemical Corporation; Beijing Research Institute of Chemical Industry, China Petroleum & Chemical Corporation
- Inventors: Changjiang WU; Xin WEI; Hesheng LI; Xinmiao ZHANG; Jie SUN; Chenghong WANG; Yujie WANG; Fanning MENG
- Web page: https://patentgrep.com/patent/US20230415101A1

## CPC

- B01D 67/0079: {Manufacture of membranes comprising organic and inorganic components}
- C08G 83/001: {Macromolecular compounds containing organic and inorganic sequences, e.g. organic polymers grafted onto silica}
- B01D 53/228: {characterised by specific membranes}
- B01D 67/0051: {by controlled crystallisation, e,.g. hydrothermal growth}
- B01D 67/0083: {Thermal after-treatment}
- B01D 67/0088: {Physical treatment with compounds, e.g. swelling, coating or impregnation}
- B01D 67/00933: {by addition of a layer chemically bonded to the membrane}
- B01D 69/02: characterised by their properties
- B01D 69/08: Hollow fibre membranes (manufacture of hollow fibres D01D5/24, D01F1/08)
- B01D 69/12: Composite membranes; Ultra-thin membranes
- B01D 71/028: {Molecular sieves (carbon B01D71/021)}
- B01D 71/261: {Polyethylene}
- B01D 71/262: {Polypropylene}
- B01D 71/301: {Polyvinylchloride}
- B01D 71/70: Polymers having silicon in the main chain, with or without sulfur, nitrogen, oxygen or carbon only
- C07C 7/144: using membranes, e.g. selective permeation
- C07F 7/003: {without C-Metal linkages}
- B01D 2257/7022: Aliphatic hydrocarbons
- B01D 2323/081: Heating
- B01D 2323/10: Specific pressure applied
- B01D 2323/30: Cross-linking
- B01D 2323/385: involving radiation
- B01D 2325/02831: less than 1 nm
- B01D 2325/02832: 1-10 nm
- B01D 2325/02833: more than 10 and up to 100 nm
- B01D 2325/02834: more than 0.1 and up to 1 µm
- B01D 2325/22: Thermal or heat-resistance properties
- B01D 2325/24: Mechanical properties, e.g. strength
- B01D 2325/30: Chemical resistance
- B01D 2325/38: Hydrophobic membranes
- Y02A 20/131: Reverse-osmosis
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- C07F: ACYCLIC, CARBOCYCLIC OR HETEROCYCLIC COMPOUNDS CONTAINING ELEMENTS OTHER THAN CARBON, HYDROGEN, HALOGEN, OXYGEN, NITROGEN, SULFUR, SELENIUM OR TELLURIUM (metal-containing porphyrins C07D487/22)
- Y02A: TECHNOLOGIES FOR ADAPTATION TO CLIMATE CHANGE

## Abstract

A metal-organic framework material separation membrane and a preparation method for the metal-organic framework material separation membrane are provided. The metal-organic framework material separation membrane has a base membrane and a metal-organic framework material functional layer. The metal-organic framework material functional layer comprises has an inter-embedded polyhedron structure. The preparation metal-organic framework material separation membrane includes the steps of: (1) preparing a solution containing a first organic solvent, an organic ligand, a metal compound, and an auxiliary agent; (2) subjecting a base membrane to a pretreatment, involving introducing, on the surface of the base membrane, metal atoms from the metal compound of step (1); and (3) mixing the pretreated base membrane of step (2) with the solution of step (1) to obtain a first mixture, and then heating the first mixture for reaction, so as to prepare a metal-organic framework material separation membrane.

## Claims

### Claim 1

A metal-organic framework material separation membrane, comprising a base membrane and a metal-organic framework material functional layer which comprises a plurality of inter-embedded polyhedron structures;
preferably, the polyhedron is composed of a plurality of crystal lattices, and among the inter-embedded polyhedron structures, two adjacent polyhedrons share crystal lattices and/or a distance between centers of the two adjacent polyhedrons is less than an average value L of lengths of the two adjacent polyhedrons, preferably less than 0.95 L, and more preferably is 0.2-0.9 L;
preferably, at least 20% of the polyhedrons in the metal-organic framework material functional layer are inter-embedded, preferably at least 30%, preferably at least 40%, preferably at least 50%, preferably at least 60%, and preferably at least 80% of the polyhedrons are inter-embedded;
preferably, the polyhedron includes hexahedron and/or octahedron, and preferably, a length of the polyhedron is 50-2000 nm; and
preferably, the crystal lattice is composed of a metal atom and organic ligands; preferably, the metal atom is selected from zirconium atom, niobium atom, molybdenum atom or cobalt atom; and preferably, the organic ligand is selected from terephthalic acid and/or nitroterephthalic acid.

### Claim 2 (depends on 1)

The separation membrane according to claim 1, characterized in that, a length of the hexahedron is 50-1000 nm, wherein the hexahedrons with a length of 400-600 nm account for 50-80%.

### Claim 3 (depends on 1)

The separation membrane according to claim 1, characterized in that, a length of the octahedron is 200-2000 nm, wherein the octahedrons with a length of 800-1200 nm account for 60-80%.

### Claim 4 (depends on 1)

The separation membrane according to claim 1, characterized in that, the metal-organic framework material functional layer has an average pore size of 0.1-2.0 nm, preferably 0.30-0.96 nm; and/or,
the metal-organic framework material functional layer has a thickness of 200-5000 nm, preferably 1000-5000 nm.

### Claim 5 (depends on 1)

The separation membrane according to claim 1, characterized in that, the base membrane is selected from one or more of polypropylene membrane, polyethylene membrane, polyvinyl chloride membrane or polytetrafluoroethylene membrane; and/or,
the base membrane has a pore size of 10-10000 nm, preferably 50-5000 nm, more preferably 200-1000 nm.

### Claim 6 (depends on 1)

The separation membrane according to claim 1, characterized in that, the separation membrane further comprises an organosilicon layer on the surface of the metal-organic framework material functional layer.

### Claim 7

A preparation method for a metal-organic framework material separation membrane, comprising the following steps:
(1) preparing a solution containing a first organic solvent, an organic ligand, a first metal compound, and an auxiliary agent selected from water or glacial acetic acid;
(2) subjecting a base membrane to a pretreatment, involving introducing, on the surface of the base membrane, metal atoms of the first metal compound in step (1);
(3) mixing the pretreated base membrane in step (2) with the solution in step (1) to obtain a first mixture, and heating the first mixture for reaction, so as to obtain the metal-organic framework material separation membrane, and
(4) optionally, subjecting the separation membrane to a cleaning treatment.

### Claim 8 (depends on 7)

The method according to claim 7, characterized in that, in step (1), a molar ratio of the first organic solvent, the organic ligand and the first metal compound is (10-1000):(1-100):(1-100), preferably (100-1000):(1-10):(1-10), more preferably (100-700):1:1, further preferably (400-600):1:1, and/or a molar ratio of the first organic solvent and the auxiliary agent water is 100:(0.001-0.05), and a molar ratio of the first organic solvent and the auxiliary agent glacial acetic acid is 100:(20-60);
preferably, the first organic solvent is selected from one or more of N-methylpyrrolidone, N,N-dimethylformamide and dimethylacetamide,
preferably, the organic ligand is selected from terephthalic acid and/or nitroterephthalic acid; and
preferably, the first metal compound is selected from one or more of zirconium compound, niobium compound, molybdenum compound and cobalt compound, preferably zirconium tetrachloride.

### Claim 9 (depends on 7)

The method according to claim 7, characterized in that, the base membrane is selected from one or more of polypropylene membrane, polyethylene membrane, polyvinyl chloride membrane or polytetrafluoroethylene membrane;
and/or, the base membrane has a pore size of 10-10000 nm, preferably 50-5000 nm, more preferably 200-1000 nm.

### Claim 10 (depends on 7)

The method according to claim 7, characterized in that, the step (2) comprises the following steps:
(2A-1) preparing a solution containing polyacrylic acid, polyvinyl alcohol and a second metal compound, and
(2A-2) coating the solution of step (2A-1) onto the base membrane;
preferably, the polyacrylic acid includes polyacrylic acid and partially hydrolyzed polyacrylic acid, and/or a mass concentration of the polyacrylic acid and the polyvinyl alcohol in the solution is 500-2000 mg/L, and a molar ratio of a sum of polyacrylic acid and polyvinyl alcohol to the metal compound is 1-3:1;
preferably, a metal atom in the second metal compound is the same as a metal atom in the first metal compound in step (1), and preferably, the second metal compound is selected from one or more of zirconium compound, niobium compound, molybdenum compound and cobalt compound, preferably zirconium tetrachloride; and
preferably, in step (2A-2), a ratio of a surface area of the base membrane to a volume of the solution obtained in step (2A-1) is 0.1-10 m2/L, preferably 0.5-5 m2/L, more preferably 1-2 m2/L.

### Claim 11 (depends on 7)

The method according to claim 7, characterized in that, the step (2) comprises the following steps:
(2B-1) preparing a solution containing a metal complex represented by formula I and a second organic solvent,
(2B-2) mix the base membrane with the solution of step (2B-1), and
(2B-3) cleaning the mixed base membrane in step (2B-2) by using a third solvent;
in formula I, Q is selected from acylamino, carbonyl or C1-C6 alkylene; R1 is selected from hydrogen, C1-C6 alkyl, C1-C6 alkoxy or halogen; M1 is the same as a metal atom in the first metal compound in step (1), and preferably, M1 is selected from zirconium atom, niobium atom, molybdenum atom or cobalt atom; m is 5-20; and n is 1-10;
preferably, the second organic solvent is selected from one or more of organic solvents capable of allowing the base membrane to swell, is preferably selected from one or more of C5-C10 aliphatic hydrocarbon, C1-C10 halogenated aliphatic hydrocarbon, C6-C20 aromatic hydrocarbon and C6-C20 halogenated aromatic hydrocarbon, and is more preferably selected from one or more of n-pentane, n-hexane, trichloromethane, carbon tetrachloride, benzene and toluene; and the third solvent is selected from one or more solvents capable of allowing the swollen base membrane to deswell, and is preferably selected from water;
preferably, in the solution of step (2B-1), a mass concentration of the metal complex represented by formula I is 500-2000 mg/L; and
preferably, in step (2B-2), a ratio of a surface area of the base membrane to a volume of the solution obtained in step (2B-1) is 0.1-10 m2/L, preferably 0.5-5 m2/L, more preferably 1-2 m2/L.

### Claim 12 (depends on 7)

The method according to claim 7, characterized in that, the step (2) comprises the following steps:
(2C-1) preparing a solution containing a metal complex represented by formula II, and
(2C-2) mixing the base membrane with the solution of step (2C-1) to obtain a mixture, and subjecting the mixture to polymerization reaction under microwave radiation conditions;
in formula II, X is selected from acylamino, carbonyl or C1-C6 alkylene; R2, R3 and R4 are the same or different, each independently selected from hydrogen, C1-C6 alkyl, C1-C6 alkoxy or halogen; and M2 is the same as a metal atom in the first metal compound in step (1), and preferably, M2 is selected from zirconium atom, niobium atom, molybdenum atom or cobalt atom;
preferably, the solution of the metal complex in step (2C-1) is an aqueous solution of the metal complex, and/or a mass concentration of the metal complex represented by formula II is 500-20000 mg/L;
preferably, in step (2C-2), a ratio of a surface area of the base membrane to a volume of the solution obtained in step (2C-1) is 0.1-10 m2/L, preferably 0.5-5 m2/L, more preferably 1-2 m2/L; and
preferably, in step (2C-2), the microwave radiation has a microwave intensity of 500-2000 μW/cm2, and a frequency of 1000-200000 Hz.

### Claim 13 (depends on 7)

The method according to claim 7, characterized in that, in step (3), a ratio of a surface area of the pretreated base membrane in step (2) to a volume of the solution obtained in step (1) is (0.01-100) m2/L.

### Claim 14 (depends on 7)

The method according to claim 7, characterized in that, in the step (3), a reaction temperature is 50-300° C., a reaction pressure is MPa, and a reaction time is 1-100 h, preferably 10-72 h, more preferably 15-30 h.

### Claim 15 (depends on 7)

The method according to claim 7, characterized in that, the method further comprises the following step:
(5) subjecting the metal-organic frame material separation membrane obtained in step (3) or (4) to a repairing treatment for one or more time(s).

### Claim 16 (depends on 7)

The method according to claim 7, characterized in that, the repairing treatment comprises the following steps:
(A) mixing the metal-organic framework material separation membrane with a solution containing a first organic solvent, an organic ligand, a first metal compound and an auxiliary agent to obtain a second mixture, wherein the auxiliary agent is selected from water or glacial acetic acid;
(B) heating the second mixture for reaction to obtain the metal-organic framework material separation membrane; and
(C) optionally, subjecting the separation membrane to a cleaning treatment; preferably, in step (B), a reaction temperature is 50-300° C., a reaction pressure is 0.01-0.5 MPa, and a reaction time is 1-100 h, preferably 5-50 h, more preferably 10-20 h.

### Claim 17

(canceled)

### Claim 18 (depends on 16)

The method according to claim 16, characterized in that, the method further comprises the following steps: coating a silane coating liquid onto a surface of the metal-organic framework material separation membrane prepared in step (3) or (4) or (B) or (C), heating the metal-organic framework material separation membrane coated with the silane coating liquid to subject the silane coating liquid to crosslinking reaction, so as to obtain a metal-organic frame material separation membrane including an organosilicon layer; and
preferably, a temperature of the crosslinking reaction is 50-300° C., and a time therefor is 0.1-20 h.

### Claim 19 (depends on 7)

A metal-organic framework material separation membrane prepared by the method according to claim 7.

### Claim 20 (depends on 19)

Use of the metal-organic framework material separation membrane according to claim 19 in organic separations.

### Claim 21 (depends on 1)

Use of the metal-organic framework material separation membrane according to claim 1 in organic separations.