# US 2023/0411686 A1 · Layered gel-polymer electrolytes and methods of forming thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411686 A1
- Document ID: US20230411686A1
- Status: Published application
- Kind: A1
- Application number: 18/460,893
- Filed: 2023-09-05
- Published: 2023-12-21
- Earliest claimed: 2019-12-03
- Assignees: GRU Energy Lab Inc.
- Applicants: Gru Energy Lab Inc.
- Inventors: Song Han; Sa Zhou; Xinghua Meng
- Web page: https://patentgrep.com/patent/US20230411686A1

## CPC

- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/056: characterised by the materials used as electrolytes, e.g. mixed inorganic/organic electrolytes
- H01M 50/431: Inorganic material
- H01M 50/449: having a layered structure
- H01M 50/457: comprising three or more layers
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0082: Organic polymers
- H01M 2300/0085: Immobilising or gelification of electrolyte
- H01M 2300/0094: in the form of layered products, e.g. coatings
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided are layered gel-polymer electrolytes and electrochemical cells comprising these electrolytes as well as methods of forming the electrolytes and the cells. A gel-polymer electrolyte comprises a support core and one or two interface layers on the core surface. The interface layers are relied on to conform to electrode surfaces with high surface roughness, while the support core prevents any physical penetration and electrical shorts through the gel-polymer electrolyte, e.g., by electrode protruding peaks. Specifically, the interface layer redistributes around these protruding peaks and forms a continuous interface with the electrode surface. When the stack is compressed, the gel-polymer electrolyte also releases some liquid electrolyte, which soaks the electrode and enhances ionic transfer within the electrode and through the electrolyte-electrode interface. The gel-polymer electrolyte is formed by coating interface layers on the support core and soaking this assembly in a liquid electrolyte.

## Claims

### Claim 1

A method of fabricating an electrochemical cell, the method comprising:
dissolving one or more polymer materials in one or more solvents, thereby forming a polymer solution;
coating the polymer solution onto a support core comprising a first surface and a second surface, opposite of the first surface, wherein the polymer solution is coated on at least the first surface thereby forming at least a first interface layer on the the first surface of the support core;
introducing a liquid electrolyte into at least one of the support core and the first interface layer, thereby forming a layered gel-polymer electrolyte; and
after introducing the liquid electrolyte, laminating a stack comprising a positive electrode, the layered gel-polymer electrolyte, and a negative electrode such that the layered gel-polymer electrolyte layer is positioned between the positive electrode and the negative electrode,
wherein, after laminating, the first interface layer conforms to one of the positive electrode and the negative electrode, and
wherein a portion of the liquid electrolyte is transferred from the layered gel-polymer electrolyte at least one of to the positive electrode and the negative electrode.

### Claim 2 (depends on 1)

The method of claim 1, further comprising adding one or more fillers to the polymer solution.

### Claim 3 (depends on 2)

The method of claim 2, wherein the one or more fillers comprise one or more of titanium dioxide (TiO2) particles, silicon dioxide (SiO2), aluminum oxide (Al2O3), sulfide compounds (e.g., argyrodite, LGPS, LPS, etc.), garnet structure oxides (e.g., LLZO with various dopants), NASICON-type phosphate glass ceramics (LAGP), oxynitrides (e.g., lithium phosphorus oxynitride or LIPON), and AB3-type hydrogen storage alloy.

### Claim 4 (depends on 1)

The method of claim 1, further comprising adding water to the polymer solution.

### Claim 5 (depends on 1)

The method of claim 1, wherein introducing the liquid electrolyte into at least one of the support core and the first interface layer comprises degassing the support core and the first interface layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the liquid electrolyte comprises an electrolyte solvent and an electrolyte salt.

### Claim 7 (depends on 1)

The method of claim 1, wherein the support core comprises at least one of polypropylene (PP), polyethylene (PE), poly(ethylene-co-tetrafluoroethylene (PETFE), poly(ethylenechloro-co-trifluoroethylene), polystyrene, polyvinyl chloride polypropylene, polyamide, polyimide, polyacrylic, polyacetal, polycarbonate, polyester, polyetherimide, polyimide, polyketone, polyphenylene ether, or polyphenylene sulfide.

### Claim 8 (depends on 1)

The method of claim 1, wherein the support core has a porosity of between 30% and 60%.

### Claim 9 (depends on 1)

The method of claim 1, wherein the support core comprises a surface layer, forming at least one of the first surface or the second surface of the support core, wherein the surface layer comprises one or more ceramic materials.

### Claim 10 (depends on 9)

The method of claim 9, wherein the one or more ceramic materials of the surface layer of the support core comprise at least one of Al2O3, SiO2, or MgO.

### Claim 11 (depends on 1)

The method of claim 1, wherein the first interface layer comprises at least one of polyvinylidene fluoride-co-hexafluoropropylene (PVDF-HFP), polyacrylonitrile (PAN), poly(methyl methacrylate) (PMMA), or polyethylene oxide (PEO).

### Claim 12 (depends on 1)

The method of claim 1, wherein the first interface layer has a porosity of between 30% and 60%.

### Claim 13 (depends on 1)

The method of claim 1, wherein the liquid electrolyte is distributed within both the support core and the first interface layer.

### Claim 14 (depends on 1)

The method of claim 1, wherein the first interface layer has a thickness of at least about micrometers.

### Claim 15 (depends on 1)

The method of claim 1, wherein the first interface layer has a thickness of at least about 50 micrometers.

### Claim 16 (depends on 1)

The method of claim 1, wherein the first interface layer conforms to the surface of the negative electrode.

### Claim 17 (depends on 16)

The method of claim 16, wherein the support core directly interfaces the positive electrode.

### Claim 18 (depends on 16)

The method of claim 16, wherein the layered gel-polymer electrolyte further comprises a second interface layer, disposed on the support core and directly interfacing the second surface of the support core, wherein the second interface layer conforms to a surface of the positive electrode.

### Claim 19 (depends on 18)

The method of claim 18, wherein the second interface layer has a different thickness than the first interface layer.

### Claim 20 (depends on 16)

The method of claim 16, wherein a thickness of the first interface layer is greater than a surface roughness of the surface of the negative electrode.