# US 2023/0411673 A1 · Producing method for lithium-ion secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411673 A1
- Document ID: US20230411673A1
- Status: Published application
- Kind: A1
- Application number: 18/135,382
- Filed: 2023-04-17
- Published: 2023-12-21
- Earliest claimed: 2022-05-26
- Assignees: Prime Planet Energy & Solutions, Inc.
- Applicants: Prime Planet Energy & Solutions, Inc.
- Inventors: Kazuma MIMA
- Web page: https://patentgrep.com/patent/US20230411673A1

## CPC

- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/049: {Processes for forming or storing electrodes in the battery container}
- H01M 10/0568: characterised by the solutes
- H01M 10/058: Construction or manufacture
- H01M 10/446: {Initial charging measures}
- H01M 50/10: Primary casings; Jackets or wrappings
- H01M 50/609: Arrangements or processes for filling with liquid, e.g. electrolytes
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/139: Processes of manufacture
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A producing method for a lithium-ion secondary battery includes a positive-electrode-plate producing step of producing a positive electrode plate having a positive active material layer on a surface of a positive current collecting foil, an electrode-body producing step of producing an electrode body provided with the positive electrode plate and a negative electrode plate, a housing step of housing the electrode body inside a battery case, an injecting step of injecting non-aqueous electrolytic solution into the battery case housed with the electrode body to produce an injection-completed battery, and an initial charging step of initially charging the injection-completed battery. The injecting step is to inject the non-aqueous electrolytic solution into the battery case housed with the electrode body in which a water content of the positive active material layer is 100 ppm or more.

## Claims

### Claim 1

A producing method for a lithium-ion secondary battery comprising a positive electrode plate provided with a positive active material layer on a surface of a positive current collecting foil formed of an aluminum foil, a negative electrode plate, non-aqueous electrolytic solution including LiPF6, and a battery case to house the positive electrode plate, the negative electrode plate, and the non-aqueous electrolytic solution, the producing method including:
positive-electrode-plate producing of producing the positive electrode plate having the positive active material layer on the surface of the positive current collecting foil;
electrode-body producing of producing an electrode body provided with the positive electrode plate and the negative electrode plate;
housing the electrode body in the battery case;
injecting the non-aqueous electrolytic solution into the battery case housed with the electrode body to produce an injection-completed battery; and
initial charging of initially charging the injection-completed battery, wherein
the injecting is to inject the non-aqueous electrolytic solution into the battery case housed with the electrode body, in which a water content of the positive active material layer is 100 ppm or more.

### Claim 2 (depends on 1)

The producing method for the lithium-ion secondary battery according to claim 1, wherein the injecting is to inject the non-aqueous electrolytic solution into the battery case housed with the electrode body in which the water content of the positive active material layer is within a range from 100 ppm or more to less than 500 ppm.

### Claim 3 (depends on 2)

The producing method for the lithium-ion secondary battery according to claim 2, wherein the producing method includes water-content adjusting between the positive-electrode-plate producing and the injecting to adjust the water content of the positive active material layer to be within the range of 100 ppm or more to less than 500 ppm.