# US 2023/0411607 A1 · Modified lithium manganese iron phosphate positive electrode material and preparation method and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411607 A1
- Document ID: US20230411607A1
- Status: Published application
- Kind: A1
- Application number: 18/459,744
- Filed: 2023-09-01
- Published: 2023-12-21
- Earliest claimed: 2022-12-14
- Assignees: Eve Power Co., Ltd.
- Applicants: Eve Power Co., Ltd.
- Inventors: Shengyao WEN; Lin ZHANG; Fanfen LIU; Dingding YUAN
- Web page: https://patentgrep.com/patent/US20230411607A1

## CPC

- H01M 4/366: {as layered products}
- C01B 25/45: containing plural metal, or metal and ammonium
- C01G 33/00: Compounds of niobium
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- C01P 2002/52: containing elements as dopants
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A modified lithium manganese iron phosphate positive electrode material and a preparation method and an application thereof are provided. The modified lithium manganese iron phosphate positive electrode material includes a doped lithium manganese iron phosphate core; and a coating layer disposed on a surface of the doped lithium manganese iron phosphate core. The doped lithium manganese iron phosphate core comprises an Nb element, and the coating layer comprises LiNbO3 and Nb2O5.

## Claims

### Claim 1

A modified lithium manganese iron phosphate positive electrode material, comprising:
a doped lithium manganese iron phosphate core; and
a coating layer disposed on a surface of the doped lithium manganese iron phosphate core,
wherein the doped lithium manganese iron phosphate core comprises an Nb element, and the coating layer comprises LiNbO3 and Nb2O5.

### Claim 2 (depends on 1)

The modified lithium manganese iron phosphate positive electrode material according to claim 1, wherein the doped lithium manganese iron phosphate core has a chemical formula of LiNbaMnxFe1-xPO4, wherein 0<a≤0.05, and 0<x<1.

### Claim 3 (depends on 1)

The modified lithium manganese iron phosphate positive electrode material according to claim 1, wherein the coating layer has a thickness of 10-50 nm; and
the molar ratio of LiNbO3 to Nb2O5 in the coating layer is 1:(0.1-0.4).

### Claim 4 (depends on 2)

The modified lithium manganese iron phosphate positive electrode material according to claim 2, wherein the coating layer has a thickness of 10-50 nm; and
the molar ratio of LiNbO3 to Nb2O5 in the coating layer is 1:(0.1-0.4).

### Claim 5

A preparation method for the modified lithium manganese iron phosphate positive electrode material that comprises a doped lithium manganese iron phosphate core and a coating layer disposed on a surface of the doped lithium manganese iron phosphate core, wherein the doped lithium manganese iron phosphate core comprises an Nb element and the coating layer comprises LiNbO3 and Nb2O5, the method comprising:
(1) mixing a lithium source, a manganese source, an iron source and a phosphorus source with a solvent to obtain a mixed salt solution, mixing the mixed salt solution, a niobium source and a complexing agent, and drying and sintering the mixture of the mixed salt solution, the niobium source and the complexing agent to obtain a primary sintered material;
(2) mixing the primary sintered material obtained in step (1), LiNbO3, Nb2O5 with an organic solvent, and grinding; and
(3) baking the material obtained after the grinding in step (2) to obtain the modified lithium manganese iron phosphate positive electrode material.

### Claim 6 (depends on 5)

The preparation method according to claim 5, wherein the lithium source in step (1) comprises lithium carbonate and/or lithium dihydrogen phosphate;
the manganese source comprises any one of or a combination of at least two of manganese sulfate, manganese carbonate, manganese nitrate, manganese acetate, or manganese oxalate;
the iron source comprises iron phosphate and/or iron powder;
the phosphorus source comprises phosphoric acid and/or ammonium dihydrogen phosphate;
the molar ratio of elements in the mixed salt solution is Li:Mn:Fe:P=(1-1.6):x:(1-x):1, wherein 0<x<1;
the niobium source comprises any one of or a combination of at least two of niobium oxide, niobium hydroxide, niobium chloride, niobium sulfate, niobium nitrate or niobium acetate; and
the complexing agent comprises sodium alginate.

### Claim 7 (depends on 5)

The preparation method according to claim 5, wherein the drying in step (1) comprises spray drying;
the temperature of the sintering is 600-900° C.;
the time of the sintering is 6-15 h; and
the atmosphere for the sintering comprises a nitrogen atmosphere.

### Claim 8 (depends on 6)

The preparation method according to claim 6, wherein the drying in step (1) comprises spray drying;
the temperature of the sintering is 600-900° C.;
the time of the sintering is 6-15 h; and
the atmosphere for the sintering comprises a nitrogen atmosphere.

### Claim 9 (depends on 5)

The preparation method according to claim 5, wherein the organic solvent in step (2) comprises ethanol;
the speed of the grinding is 500-1000 rpm;
the time of the grinding is 0.3-1 h;
the ratio of the total mass of LiNbO3 and Nb2O5 to the mass of the primary sintered material is 0.1-10:100.

### Claim 10 (depends on 6)

The preparation method according to claim 6, wherein the organic solvent in step (2) comprises ethanol;
the speed of the grinding is 500-1000 rpm;
the time of the grinding is 0.3-1 h;
the ratio of the total mass of LiNbO3 and Nb2O5 to the mass of the primary sintered material is 0.1-10:100.

### Claim 11 (depends on 7)

The preparation method according to claim 7, wherein the organic solvent in step (2) comprises ethanol;
the speed of the grinding is 500-1000 rpm;
the time of the grinding is 0.3-1 h;
the ratio of the total mass of LiNbO3 and Nb2O5 to the mass of the primary sintered material is 0.1-10:100.

### Claim 12 (depends on 9)

The preparation method according to claim 9, wherein the ratio of the total mass of LiNbO3 and Nb2O5 to the mass of the primary sintered material is 0.5-2:100.

### Claim 13 (depends on 5)

The preparation method according to claim 5, wherein the temperature of the baking in step (3) is 200-650° C.; and
the time of the baking is 2-15 h.

### Claim 14 (depends on 6)

The preparation method according to claim 6, wherein the temperature of the baking in step (3) is 200-650° C.; and
the time of the baking is 2-15 h.

### Claim 15 (depends on 7)

The preparation method according to claim 7, wherein the temperature of the baking in step (3) is 200-650° C.; and
the time of the baking is 2-15 h.

### Claim 16 (depends on 8)

The preparation method according to claim 8, wherein the temperature of the baking in step (3) is 200-650° C.; and
the time of the baking is 2-15 h.

### Claim 17

A positive electrode, comprising the modified lithium manganese iron phosphate positive electrode material,
wherein the modified lithium manganese iron phosphate positive electrode material comprises:
a doped lithium manganese iron phosphate core; and
a coating layer disposed on a surface of the doped lithium manganese iron phosphate core,
wherein the doped lithium manganese iron phosphate core comprises an Nb element, and the coating layer comprises LiNbO3 and Nb2O5.

### Claim 18 (depends on 16)

The positive electrode according to claim 16, wherein the doped lithium manganese iron phosphate core has a chemical formula of LiNbaMnxFe1-xPO4, wherein 0<a≤0.05, and 0<x<1.

### Claim 19 (depends on 17)

The positive electrode according to claim 17, wherein the coating layer has a thickness of 10-50 nm; and
the molar ratio of LiNbO3 to Nb2O5 in the coating layer is 1:(0.1-0.4).

### Claim 20 (depends on 18)

The positive electrode according to claim 18, wherein the coating layer has a thickness of 10-50 nm; and
the molar ratio of LiNbO3 to Nb2O5 in the coating layer is 1:(0.1-0.4).