# US 2023/0411604 A1 · Lithium Iron Manganese Phosphate Cathode Material, Preparation Method and Application Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411604 A1
- Document ID: US20230411604A1
- Status: Published application
- Kind: A1
- Application number: 18/241,231
- Filed: 2023-08-31
- Published: 2023-12-21
- Earliest claimed: 2023-02-10
- Assignees: Eve Power Co., Ltd.
- Applicants: Eve Power Co., Ltd.
- Inventors: Xiaohan Deng; Haitao Wei; Weihua Zhu; Hao Cheng
- Web page: https://patentgrep.com/patent/US20230411604A1

## CPC

- H01M 4/366: {as layered products}
- C01B 25/45: containing plural metal, or metal and ammonium
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/625: {Carbon or graphite}
- C01P 2004/03: obtained by SEM
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Specifically disclosed in the present application is a lithium iron manganese phosphate cathode material, preparation method and application thereof. The lithium iron manganese phosphate cathode material includes a lithium iron manganese phosphate substrate and a coating layer on a surface of the lithium iron manganese phosphate substrate; the coating layer includes carbon quantum dots containing amino groups; and a mass ratio of manganese ions to carbon quantum dots containing amino groups is (4.5˜5.5):1 in the lithium iron manganese phosphate cathode material.

## Claims

### Claim 1

A lithium iron manganese phosphate cathode material, wherein the lithium iron manganese phosphate cathode material comprises a lithium iron manganese phosphate substrate and a coating layer on a surface of the lithium iron manganese phosphate substrate; the coating layer comprises carbon quantum dots containing amino groups; and a mass ratio of manganese ions to carbon quantum dots containing amino groups is (4.5˜5.5):1 in the lithium iron manganese phosphate cathode material.

### Claim 2 (depends on 1)

The lithium iron manganese phosphate cathode material according to claim 1, wherein the lithium iron manganese phosphate substrate is prepared by following steps: dissolving a lithium source, an iron source, a manganese source, and a phosphorus source in deionized water to obtain a mixed solution and adjusting pH of the mixed solution; then adding polyvinylpyrrolidone to obtain a lithium iron manganese phosphate precursor solution; heating the lithium iron manganese phosphate precursor solution; and drying to obtain a lithium iron manganese phosphate substrate.

### Claim 3 (depends on 2)

The lithium iron manganese phosphate cathode material according to claim 2, wherein a mass ratio of manganese to iron in the lithium iron manganese phosphate precursor solution is (5.5˜6.5):4.

### Claim 4 (depends on 2)

The lithium iron manganese phosphate cathode material according to claim 2, wherein a heating process of the lithium iron manganese phosphate precursor solution is carried out at a heating temperature of 160° C.˜200° C. and a heating duration of 10 min˜30 min.

### Claim 5 (depends on 1)

The lithium iron manganese phosphate cathode material according to claim 1, wherein a mass ratio of the carbon quantum dots containing amino groups in the coating layer is 0.5˜4%.

### Claim 6 (depends on 5)

The lithium iron manganese phosphate cathode material according to claim 5, wherein the carbon quantum dots containing amino groups are prepared by following steps: mixing organic material containing amino groups with citric acid solution and preparing by hydrothermal reaction to obtain the carbon quantum dots containing amino groups.

### Claim 7 (depends on 1)

The lithium iron manganese phosphate cathode material according to claim 1, wherein a particle size of the carbon quantum dots containing amino groups is 1.5˜3.5 nm.

### Claim 8

A preparation method of a lithium iron manganese phosphate cathode material, wherein the lithium iron manganese phosphate cathode material comprises a lithium iron manganese phosphate substrate and a coating layer on a surface of the lithium iron manganese phosphate substrate; the coating layer comprises carbon quantum dots containing amino groups; and a mass ratio of manganese ions to carbon quantum dots containing amino groups is (4.5˜5.5):1 in the lithium iron manganese phosphate cathode material, the preparation method comprising following steps:
Step one: Mixing the lithium iron manganese phosphate substrate with chitosan in a liquid phase; adding the carbon quantum dots containing amino groups simultaneously; and spray-drying to obtain coated lithium iron manganese phosphate powder; and
Step two: Drying and grinding the coated lithium iron manganese phosphate powder to obtain an organic polymer-coated lithium iron manganese phosphate precursor; heating up and cooling down the organic polymer-coated lithium iron manganese phosphate precursor to obtain a cathode material of lithium iron manganese phosphate powder coated with carbon quantum dots.

### Claim 9 (depends on 8)

The preparation method of the lithium iron manganese phosphate cathode material according to claim 8, wherein the lithium iron manganese phosphate substrate is prepared by following steps: dissolving a lithium source, an iron source, a manganese source, and a phosphorus source in deionized water to obtain a mixed solution and adjusting pH of the mixed solution; then adding polyvinylpyrrolidone to obtain a lithium iron manganese phosphate precursor solution; heating the lithium iron manganese phosphate precursor solution; and drying to obtain a lithium iron manganese phosphate substrate.

### Claim 10 (depends on 9)

The preparation method of the lithium iron manganese phosphate cathode material according to claim 9, wherein a mass ratio of manganese to iron in the lithium iron manganese phosphate precursor solution is (5.5˜6.5):4.

### Claim 11 (depends on 9)

The preparation method of the lithium iron manganese phosphate cathode material according to claim 9, wherein a heating process of the lithium iron manganese phosphate precursor solution is carried out at a heating temperature of 160° C.˜200° C. and a heating duration of 10 min˜30 min.

### Claim 12 (depends on 8)

The preparation method of the lithium iron manganese phosphate cathode material according to claim 8, wherein in a process of heating up and cooling down the organic polymer-coated lithium iron manganese phosphate precursor, temperature is first raised to 500° C.˜900° C. at a heating speed of 1° C./min˜35° C./min, then thermally insulated and kept for 1 hour to 16 hours, and then cooled down to room temperature at a cooling speed of 1° C./min˜35° C./min.

### Claim 13

A positive electrode sheet, wherein the positive electrode sheet comprises a lithium iron manganese phosphate cathode material, wherein the lithium iron manganese phosphate cathode material comprises a lithium iron manganese phosphate substrate and a coating layer on a surface of the lithium iron manganese phosphate substrate; the coating layer comprises carbon quantum dots containing amino groups; and a mass ratio of manganese ions to carbon quantum dots containing amino groups is (4.5˜5.5):1 in the lithium iron manganese phosphate cathode material.

### Claim 14 (depends on 13)

The positive electrode sheet according to claim 13, wherein the lithium iron manganese phosphate substrate is prepared by following steps: dissolving a lithium source, an iron source, a manganese source, and a phosphorus source in deionized water to obtain a mixed solution and adjusting a pH of the mixed solution; then adding polyvinylpyrrolidone to obtain a lithium iron manganese phosphate precursor solution; heating the lithium iron manganese phosphate precursor solution; and drying to obtain a lithium iron manganese phosphate substrate.

### Claim 15 (depends on 14)

The positive electrode sheet according to claim 14, wherein a mass ratio of manganese to iron in the lithium iron manganese phosphate precursor solution is (5.5˜6.5):4.

### Claim 16 (depends on 14)

The positive electrode sheet according to claim 14, wherein a heating process of the lithium iron manganese phosphate precursor solution is carried out at a heating temperature of 160° C.˜200° C. and a heating duration of 10 min˜30 min.

### Claim 17 (depends on 13)

The positive electrode sheet according to claim 13, wherein a mass ratio of the carbon quantum dots containing amino groups in the coating layer is 0.5˜4%.

### Claim 18 (depends on 17)

The positive electrode sheet according to claim 17, wherein the carbon quantum dots containing amino groups are prepared by following steps: mixing an organic material containing amino groups with citric acid solution and preparing by hydrothermal reaction to obtain the carbon quantum dots containing amino groups.

### Claim 19 (depends on 13)

The positive electrode sheet according to claim 13, wherein a particle size of the carbon quantum dots containing amino groups is 1.5˜3.5 nm.