# US 2023/0411602 A1 · Nanostructured battery active materials and methods of producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411602 A1
- Document ID: US20230411602A1
- Status: Published application
- Kind: A1
- Application number: 18/111,549
- Filed: 2023-02-18
- Published: 2023-12-21
- Earliest claimed: 2011-07-26
- Assignees: OneD Material, Inc.
- Applicants: OneD Material, Inc.
- Inventors: Wanqing CAO; Virginia ROBBINS; Yimin ZHU
- Web page: https://patentgrep.com/patent/US20230411602A1

## CPC

- H01M 4/366: {as layered products}
- B01J 21/18: Carbon
- B01J 23/72: Copper
- B01J 37/0211: {using a colloidal suspension}
- C01B 33/02: Silicon (forming single crystals or homogeneous polycrystalline material with defined structure C30B)
- C01B 33/021: Preparation (chemical coating from the vapour phase C23C16/00)
- C01B 33/029: by decomposition of monosilane
- C30B 11/12: Vaporous components, e.g. vapour-liquid-solid-growth
- C30B 25/005: {Growth of whiskers or needles}
- C30B 29/06: Silicon
- C30B 29/60: characterised by shape
- H01M 4/0428: {Chemical vapour deposition}
- H01M 4/0495: {Chemical alloying}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/622: {being polymers}
- C01P 2004/16: Nanowires or nanorods, i.e. solid nanofibres with two nearly equal dimensions between 1-100 nanometer
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Methods for producing nanostructures from copper-based catalysts on porous substrates, particularly silicon nanowires on carbon-based substrates for use as battery active materials, are provided. Related compositions are also described. In addition, novel methods for production of copper-based catalyst particles are provided. Methods for producing nanostructures from catalyst particles that comprise a gold shell and a core that does not include gold are also provided.

## Claims

### Claim 1

A method comprising:
providing a carbon-based porous substrate comprising a population of particles comprising at least one of natural graphite particles, synthetic graphite particles, graphene particles, or carbon black particles;
mixing deionized water with a copper source and a chelating agent to form a first aqueous solution comprising copper ions, wherein the copper source comprises at least one of copper sulfate, copper nitrate, copper chloride, or copper acetate and wherein the chelating agent comprises at least one of potassium sodium tartrate, EDTA, or polyols;
mixing deionized water with a reducing agent to form a second aqueous solution, wherein the reducing agent comprises at least one of sodium ascorbate or ascorbic acid;
mixing the first aqueous solution with the second aqueous solution to form Cu2O colloidal nanoparticles in an alkaline plating solution, the Cu2O colloidal nanoparticles formed via chemical reduction of the copper source, and wherein the pH and concentrations are adjusted to control the size distribution of the Cu2O colloidal nanoparticles;
depositing the Cu2O colloidal nanoparticles onto a surface of the carbon-based porous substrate by stirring a solution comprising the Cu2O colloidal nanoparticles and the carbon-based porous substrate until the solution is substantially depleted of the Cu2O colloidal nanoparticles; and
recovering, by filtration, the carbon-based porous substrate with the Cu2O nanoparticles deposited thereon.

### Claim 2 (depends on 1)

The method of claim 1 further comprising, prior to immersing, setting the copper ions concentration to at most 10 millimolar.

### Claim 3 (depends on 2)

The method of claim 2 further comprising, prior to immersing, setting the pH of the alkaline plating solution between 8 and 11 and setting the copper ions concentration up to 5 millimolar.

### Claim 4 (depends on 1)

The method of claim 1, wherein the particles in the population of particles in the carbon-based porous substrate have an average diameter between 0.5 μm and 50 μm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the particles in the population of particles in the carbon-based porous substrate have an average diameter between 2 μm and 10 μm.

### Claim 6 (depends on 1)

The method of claim 1, wherein depositing further comprises depositing the formed Cu2O colloidal nanoparticles onto the surface of the carbon-based porous substrate until the concentration of copper ions in the alkaline plating solution is less than 1 ppm.

### Claim 7 (depends on 1)

The method of claim 1, wherein the formed Cu2O nanoparticles in the alkaline plating solution have an average size between 5 nm and 100 nm as measured by a light scattering measurement or by electron microscopy.

### Claim 8 (depends on 1)

The method of claim 1, wherein the formed Cu2O nanoparticles in the alkaline plating solution have an average size between 20 nm and 50 nm as measured by a light scattering measurement or by electron microscopy.

### Claim 9 (depends on 1)

The method of claim 1, wherein the formed Cu2O nanoparticles in the alkaline plating solution have an average size between 20 nm and 40 nm as measured by a light scattering measurement or by electron microscopy.

### Claim 10 (depends on 1)

The method of claim 1, wherein removing further comprises filtering the plating solution to recover the carbon-based porous substrate with the Cu2O nanoparticles deposited thereon and drying the carbon-based porous substrate in an oven.

### Claim 11 (depends on 1)

The method of claim 1, further comprising, after recovering, drying the carbon-based porous substrate with the nanoparticles deposited thereon in an oven at 120° C. for at least 12 hours.

### Claim 12 (depends on 1)

The method of claim 1, further comprising setting the copper ions concentration up to 5 millimolar.

### Claim 13 (depends on 1)

The method of claim 1, further comprising:
loading the carbon-based porous substrate with the Cu2O nanoparticles deposited thereon into a reaction vessel, wherein the carbon-based porous substrate with the Cu2O nanoparticles deposited thereon form a packed bed in the reaction vessel; and
growing, in the reaction vessel, nanostructures on the carbon-based porous substrate from the Cu2O nanoparticles via a Vapor-Solid-Solid (VSS) synthesis technique, wherein the growing comprises mixing the packed bed while flowing one or more reactant gases in the reaction vessel during the nanostructure growing process; and wherein the nanostructures comprise silicon, germanium or a combination thereof.

### Claim 14 (depends on 13)

The method of claim 13, wherein the nanostructures comprise at least one of nanowires or nanoparticles.

### Claim 15 (depends on 13)

The method of claim 13, wherein the one or more reactant gas comprises silane (SiH4).

### Claim 16 (depends on 13)

The method of claim 13, further comprising, after growing, applying a carbon coating or an oxide coating to the nanostructures.

### Claim 17 (depends on 13)

The method of claim 13, further comprising, after growing, incorporating the carbon-based porous substrate with the nanostructure grown thereon into a battery slurry.

### Claim 18 (depends on 13)

The method of claim 13, further comprising, after growing, incorporating the carbon-based porous substrate with the nanostructure grown thereon into a battery anode.

### Claim 19 (depends on 13)

The method of claim 13, further comprising, after growing, incorporating the carbon-based porous substrate with the nanostructure grown thereon into a battery.