# US 2023/0411446 A1 · Gate trench power semiconductor devices having trench shielding patterns formed during the well implant and related methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411446 A1
- Document ID: US20230411446A1
- Status: Published application
- Kind: A1
- Application number: 17/845,120
- Filed: 2022-06-21
- Published: 2023-12-21
- Earliest claimed: 2022-06-21
- Assignees: Wolfspeed, Inc.
- Applicants: Wolfspeed, Inc.
- Inventors: Madankumar Sampath; Sei-Hyung Ryu; Naeem Islam; Woongsun Kim
- Web page: https://patentgrep.com/patent/US20230411446A1

## CPC

- H10D 30/0297: {using recessing of the gate electrodes, e.g. to form trench gate electrodes}
- H10D 62/109: {Reduced surface field [RESURF] PN junction structures}
- H10D 12/031: {of IGBTs}
- H10D 12/038: {having a recessed gate, e.g. trench-gate IGBTs}
- H10D 30/668: {having trench gate electrodes, e.g. UMOS transistors}
- H10D 62/107: {Buried supplementary regions, e.g. buried guard rings (multi-RESURF H10D62/111)}
- H10D 62/393: {Body regions of DMOS transistors or IGBTs (cell layout of DMOS H10D62/127)}
- H10D 62/8325: {Silicon carbide}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10P 14/6308: {of Group IV semiconductors}
- H10P 30/2042: {into crystalline silicon carbide}
- H10P 30/21: {of electrically active species}
- H10P 30/222: {characterised by the angle between the ion beam and the crystal planes or the main crystal surface (characterised by the angle between the ion beam and the mask H10P30/221)}
- H10P 30/28: characterised by an annealing step, e.g. for activation of dopants
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A wide band-gap semiconductor layer structure is provided that comprises a drift region having a first conductivity type and a plurality of source regions having the first conductivity type on the drift region. A plurality of trenches are provided in an upper surface of the wide band-gap semiconductor layer structure. Second conductivity type dopants are implanted into the wide band-gap semiconductor layer structure to simultaneously form well regions underneath the source regions and trench shielding regions underneath the trenches, the well regions and the trench shielding regions each having a second conductivity type.

## Claims

### Claim 1

A method of fabricating a semiconductor device, the method comprising:
providing a wide band-gap semiconductor layer structure that comprises a drift region having a first conductivity type and a source region having the first conductivity type on the drift region, the wide band-gap semiconductor layer structure comprising a trench therein; and
implanting second conductivity type dopants into the wide band-gap semiconductor layer structure to simultaneously form both a well region underneath the source region and a trench shielding region underneath the trench, the well region and the trench shielding region each having a second conductivity type.

### Claim 2 (depends on 1)

The method of claim 1, wherein the trench extends through the source region and into the drift region.

### Claim 3 (depends on 1)

The method of claim 1, wherein implanting second conductivity type dopants into the wide band-gap semiconductor layer structure comprises implanting the second conductivity type dopants through the source region into the drift region.

### Claim 4 (depends on 1)

The method of claim 1, wherein the well region is formed by converting a portion of the drift region having the first conductivity type into the well region having the second conductivity type.

### Claim 5 (depends on 1)

The method of claim 1, wherein the well region separates the source region from the drift region.

### Claim 6 (depends on 1)

The method of claim 1, wherein the source region forms an upper portion of both a first sidewall and a second sidewall of the trench and the drift region forms a lower portion of the first sidewall and the second sidewall, wherein the first sidewall faces the second sidewall.

### Claim 7 (depends on 6)

The method of claim 6, wherein the first sidewall of the trench is exposed when the second conductivity type dopants are implanted into the wide band-gap semiconductor layer structure.

### Claim 8 (depends on 7)

The method of claim 7, the method further comprising:
performing an oxidation process to convert at least the first and second sidewalls and a bottom of the trench into an oxide material; and
removing the oxide material to convert the trench into an enlarged trench.

### Claim 9 (depends on 1)

The method of claim 1, wherein the wide band-gap semiconductor layer structure extends in a length direction, a width direction and a depth direction that are perpendicular to each other, and a lower surface of the wide band-gap semiconductor layer structure extends in the length and width directions.

### Claim 10 (depends on 9)

The method of claim 9, wherein the source region extends a first distance in the depth direction and the shielding region extends a second distance in the depth direction, where the second distance exceeds the first distance.

### Claim 11

(canceled)

### Claim 12 (depends on 10)

The method of claim 10, wherein the second distance is at least twice the first distance.

### Claim 13 (depends on 10)

The method of claim 10, wherein a portion of the well region that extends to an upper surface of the wide band-gap semiconductor layer structure extends a third distance in the depth direction, and the third distance is substantially the same as the second distance.

### Claim 14 (depends on 1)

The method of claim 1, wherein a concentration of second conductivity type dopants in the source region is at least 5×1015/cm3.

### Claim 15 (depends on 1)

The method of claim 1, wherein a doping profile of a lower portion of the trench shielding region that is taken along a first axis that extends in the depth direction through a center of the bottom of the gate trench varies by less than 15% from a doping profile of the well region that is taken along a second axis that is parallel to the first axis and that extends through the well region.

### Claim 16 (depends on 1)

The method of claim 1, the method further comprising implanting additional second conductivity type dopants into the wide band-gap semiconductor layer structure underneath the trench.

### Claim 17 (depends on 16)

The method of claim 16, wherein the second conductivity type dopants and the additional second conductivity type dopants are implanted using a same ion implantation mask.

### Claim 18 (depends on 16)

The method of claim 16, wherein the additional second conductivity type dopants are implanted before the second conductivity type dopants are implanted.

### Claim 19 (depends on 16)

The method of claim 16, the method further comprising forming a mask on sidewalls of the trench before implanting the additional second conductivity type dopants into the wide band-gap semiconductor layer structure.

### Claim 20 (depends on 16)

The method of claim 16, wherein an upper surface of the source region is exposed when the additional second conductivity type dopants are implanted into the wide band-gap semiconductor layer structure.

### Claim 21 (depends on 8)

The method of claim 8, the method further comprising implanting additional second conductivity type dopants into the wide band-gap semiconductor layer structure underneath the trench.

### Claim 22 (depends on 16)

The method of claim 16, wherein the additional second conductivity type dopants are implanted before an oxidation process is performed to convert at least the first and second sidewalls and a bottom of the trench into an oxide material.

### Claim 23 (depends on 1)

The method of claim 1, wherein an upper surface of the source region is exposed when the second conductivity type dopants are implanted into the wide band-gap semiconductor layer structure.

### Claim at position 24

24-45. (canceled)