# US 2023/0411347 A1 · Cu-cu direct welding for packaging application in semiconductor industry

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411347 A1
- Document ID: US20230411347A1
- Status: Published application
- Kind: A1
- Application number: 18/267,492
- Filed: 2021-12-14
- Published: 2023-12-21
- Earliest claimed: 2020-12-16
- Assignees: The University of Hong Kong
- Applicants: The University of Hong Kong
- Inventors: Mingxin Huang; Shien Ping Feng
- Web page: https://patentgrep.com/patent/US20230411347A1

## CPC

- H10W 72/073: {of die-attach connectors}
- H10W 72/90: Bond pads, in general
- H10W 72/072: {of bump connectors}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/01235: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01271: {Cleaning, e.g. oxide removal or de-smearing}
- H10W 72/01335: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01371: {Cleaning, e.g. oxide removal or de-smearing}
- H10W 72/016: {of strap connectors}
- H10W 72/07232: {Compression bonding, e.g. thermocompression bonding}
- H10W 72/07311: {Treating the bonding area before connecting, e.g. by applying flux or cleaning}
- H10W 72/07331: {Connecting techniques}
- H10W 72/07332: {Compression bonding, e.g. thermocompression bonding}
- H10W 72/07341: {Controlling the bonding environment, e.g. atmosphere composition or temperature}
- H10W 72/241: {Dispositions, e.g. layouts}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/352: {comprising metals or metalloids, e.g. solders}
- H10W 80/312: {characterised by the direct bonding of electrically conductive pads}
- H10W 80/314: {characterized by direct bonding of pads or other interconnections}
- H10W 90/722: {between stacked chips}
- H10W 90/732: {between stacked chips}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Disclosed is a method of bonding two copper structures involving compressing a first copper structure with a second copper structure under a stress from 0.1 MPa to 50 MPa and under a temperature of 250° C. or less so that a bonding surface of the first copper structure is bonded to a bonding surface of the second copper structure; at least one of the bonding surface of the first copper structure and the bonding surface of the second copper structure have a layer of nanograins of copper having an average grain size of 5 nm to 500 nm, the layer of the nanograins of copper having a thickness of 10 nm to 10 μm.

## Claims

### Claim 1

A method of bonding two copper structures, comprising:
compressing a first copper structure with a second copper structure under a stress from MPa to 50 MPa and under a temperature from 100° C. to 250° C. so that a bonding surface of the first copper structure is bonded to a bonding surface of the second copper structure;
at least one of the bonding surface of the first copper structure and the bonding surface of the second copper structure have a layer of nanograins of copper having an average grain size of 5 nm to 500 nm, the layer of the nanograins of copper having a thickness of 10 nm to 10 μm.

### Claim 2 (depends on 1)

The method according to claim 1, wherein both of the bonding surface of the first copper structure and the bonding surface of the second copper structure have a layer of nanograins of copper having an average grain size of 5 nm to 500 nm, the layer of the nanograins of copper having a thickness of 10 nm to 10 μm.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the nanograins of copper have an average grain size of 10 nm to 250 nm.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the nanograins of copper have an average grain size of 10 nm to 250 nm.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the nanograins of copper have an average grain size of 10 nm to 250 nm.

### Claim 6 (depends on 2)

The method according to claim 2, wherein the nanograins of copper have an average grain size of 15 nm to 100 nm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the first copper structure and the second copper structure are compressed under a stress from 1 MPa to 20 MPa.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the first copper structure and the second copper structure are compressed under a temperature from 120° C. to 200° C.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the first copper structure and the second copper structure are compressed for a time from 0.5 to 60 minutes.

### Claim 10 (depends on 1)

The method according to claim 1, with the proviso that a CMP process associated with the method of bonding two copper structures is not conducted.

### Claim 11

A method of bonding two copper structures within a 5G chipset, comprising:
compressing a first copper structure within a wireless chipset with a second copper structure within a wireless chipset under a stress from 0.1 MPa to 50 MPa and under a temperature from 100° C. to 250° C. so that a bonding surface of the first copper structure is bonded to a bonding surface of the second copper structure;
at least one of the bonding surface of the first copper structure and the bonding surface of the second copper structure have a layer of nanograins of copper having an average grain size of 5 nm to 500 nm, the layer of the nanograins of copper having a thickness of 10 nm to 10 μm.

### Claim 12 (depends on 11)

The method according to claim 11, wherein both of the bonding surface of the first copper structure and the bonding surface of the second copper structure have a layer of nanograins of copper having an average grain size of 5 nm to 500 nm, the layer of the nanograins of copper having a thickness of 10 nm to 10 μm.

### Claim 13 (depends on 11)

The method according to claim 11, wherein the nanograins of copper have an average grain size of 10 nm to 250 nm.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the nanograins of copper have an average grain size of 10 nm to 250 nm.

### Claim 15 (depends on 11)

The method according to claim 11, wherein the nanograins of copper have an average grain size of 10 nm to 250 nm.

### Claim 16 (depends on 12)

The method according to claim 12, wherein the nanograins of copper have an average grain size of 15 nm to 100 nm.

### Claim 17 (depends on 11)

The method according to claim 11, wherein the first copper structure and the second copper structure are compressed under a stress from 1 MPa to 20 MPa.

### Claim 18 (depends on 11)

The method according to claim 11, wherein the first copper structure and the second copper structure are compressed under a temperature from 120° C. to 200° C.

### Claim 19 (depends on 11)

The method according to claim 11, wherein the first copper structure and the second copper structure are compressed for a time from 0.5 to 60 minutes.

### Claim 20 (depends on 11)

The method according to claim 11, with the proviso that a CMP process associated with the method of bonding two copper structures is not conducted.