# US 2023/0411220 A1 · Post gate dielectric processing for semiconductor device fabrication

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411220 A1
- Document ID: US20230411220A1
- Status: Published application
- Kind: A1
- Application number: 18/357,864
- Filed: 2023-07-24
- Published: 2023-12-21
- Earliest claimed: 2020-09-30
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chih-Yu Hsu; Jian-Hao Chen; Chia-Wei Chen; Shan-Mei Liao; Hui-Chi Chen; Cheng Hong Yang; Shih-Hao Lin; Kuo-Feng Yu; Feng-Cheng Yang; Yen-Ming Chen
- Web page: https://patentgrep.com/patent/US20230411220A1

## CPC

- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 84/0181: {Manufacturing their gate insulating layers}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/853: {comprising FinFETs}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Semiconductor device and the manufacturing method thereof are disclosed. An exemplary semiconductor device comprises a first semiconductor stack and a second semiconductor stack over a substrate, wherein each of the first and second semiconductor stacks includes semiconductor layers stacked up and separated from each other; a dummy spacer between the first and second semiconductor stacks, wherein the dummy spacer contacts a first sidewall of each semiconductor layer of the first and second semiconductor stacks; and a gate structure wrapping a second sidewall, a top surface, and a bottom surface of each semiconductor layer of the first and second semiconductor stacks.

## Claims

### Claim 1

A method of forming a semiconductor device, comprising:
forming an active region over a substrate;
forming a dummy gate structure over a channel region of the active region;
forming a first gate spacer and a second gate spacer along sidewalls of the dummy gate structure;
removing the dummy gate structure to form a gate trench defined between the first gate spacer and the second gate spacer
forming an interfacial layer over the active region;
depositing a high-K dielectric layer in the gate trench and over the interfacial layer;
forming a capping layer over the high-K dielectric layer;
after the forming of the capping layer, performing a first annealing process to the capping layer;
after the first annealing process, completely removing the capping layer to expose the high-K dielectric layer; and
forming a metal gate electrode over the high-K dielectric layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the depositing of the capping layer comprises:
depositing a high-k capping layer in the gate trench; and
depositing a silicon capping layer over the high-k capping layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the depositing of the high-k capping layer and depositing of the silicon capping layer are performed in a single processing tool such that the high-k capping layer is not oxidized.

### Claim 4 (depends on 2)

The method of claim 2, wherein the high-k capping layer comprises a metal nitride.

### Claim 5 (depends on 2)

The method of claim 2, wherein the high-k capping layer comprises titanium nitride (TiN), tantalum nitride (TaN), or tennessine nitride (TsN).

### Claim 6 (depends on 2)

The method of claim 2, wherein the depositing of the silicon capping layer comprises use of silane (SiH4).

### Claim 7 (depends on 1)

The method of claim 1, wherein the first annealing process comprises a spike anneal process and an annealing temperature between about 850° C. and about 950° C.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
after the removing of the capping layer, performing a second annealing process to densify the high-k dielectric layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the second annealing process comprises a spike annealing process and an annealing temperature between about 850° C. and about 900° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the removing of the capping layer comprises a wet only process.

### Claim 11 (depends on 10)

The method of claim 10, wherein the wet only process comprises:
a first etching step that includes use of dilute hydrogen fluoride; and
a second etching step that includes use of ammonium hydroxide (NH4OH), hydrogen peroxide (H2O2), or water (H2O).

### Claim 12

A method of forming a semiconductor device, comprising:
forming an active region over a substrate;
forming a dummy gate structure over a channel region of the active region;
forming a first gate spacer and a second gate spacer along sidewalls of the dummy gate structure;
removing the dummy gate structure to form a gate trench defined between the first gate spacer and the second gate spacer
forming an interfacial layer over the active region;
depositing a high-K dielectric layer in the gate trench and over the interfacial layer;
forming a capping layer over the high-K dielectric layer, the capping layer comprising a high-k capping layer and a silicon capping layer,
after the forming of the capping layer, performing a first annealing process to the capping layer;
after the first annealing process, completely removing the capping layer to expose the high-K dielectric layer;
after the completely removing, performing a second annealing process to densify the high-k dielectric layer; and
forming a metal gate electrode over the high-K dielectric layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the first annealing process comprises a spike anneal process and an annealing temperature between about 850° C. and about 950° C.

### Claim 14 (depends on 12)

The method of claim 12, wherein the second annealing process comprises a spike annealing process and an annealing temperature between about 850° C. and about 900° C.

### Claim 15 (depends on 12)

The method of claim 12, wherein the removing of the capping layer comprises a wet only process.

### Claim 16 (depends on 15)

The method of claim 15, wherein the wet only process comprises:
a first etching step that includes use of dilute hydrogen fluoride; and
a second etching step that includes use of ammonium hydroxide (NH4OH), hydrogen peroxide (H2O2), or water (H2O),
wherein the second etching step lasts longer than the first etching step.

### Claim 17

A method of forming a semiconductor device, comprising:
forming an active region over a substrate;
forming a dummy gate structure over a channel region of the active region;
forming a first gate spacer and a second gate spacer along sidewalls of the dummy gate structure;
removing the dummy gate structure to form a gate trench defined between the first gate spacer and the second gate spacer
forming an interfacial layer over the active region;
after the forming of the interfacial layer, performing a first annealing process to enhance a quality of the interfacial layer;
depositing a high-K dielectric layer in the gate trench and over the interfacial layer;
after the depositing of the high-k dielectric layer, performing a second annealing process to densify the high-k dielectric layer;
forming a capping layer over the high-K dielectric layer, the capping layer comprising a high-k capping layer and a silicon capping layer,
after the forming of the capping layer, performing a third annealing process;
after the third annealing process, completely removing the capping layer to expose the high-K dielectric layer; and
forming a metal gate electrode over the high-K dielectric layer.

### Claim 18 (depends on 17)

The method of claim 17, wherein the first annealing process is performed in an ambience comprising nitrogen (N2), hydrogen (H2), or ammonia (NH3).

### Claim 19 (depends on 17)

The method of claim 17, wherein the second annealing process comprises a spike annealing process and an annealing temperature between about 850° C. and about 900° C.

### Claim 20 (depends on 17)

The method of claim 17, wherein the third annealing process comprises a spike anneal process and an annealing temperature between about 850° C. and about 950° C.