# US 2023/0411211 A1 · Interconnect structure and method of forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411211 A1
- Document ID: US20230411211A1
- Status: Published application
- Kind: A1
- Application number: 17/842,804
- Filed: 2022-06-17
- Published: 2023-12-21
- Earliest claimed: 2022-06-17
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Ming-Yang Li; Chih-Piao Chuu; Szuya Liao; Han Wang
- Web page: https://patentgrep.com/patent/US20230411211A1

## CPC

- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/033: {in openings in dielectrics}
- H10W 20/037: {the barrier, adhesion or liner layers being on top of a main fill metal}
- H10W 20/048: {by using plasmas or gaseous environments, e.g. by nitriding}
- H10W 20/062: {by smoothing of conductive parts, e.g. by planarisation}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/082: {the openings being tapered via holes}
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W 20/435: {Cross-sectional shapes or dispositions of interconnections}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Provided are an interconnect structure and a method of forming the same. The method includes: forming an opening in a dielectric layer; forming a 2D material layer to conformally cover a surface of the opening; performing a nitridation treatment on the 2D material layer to form a nitrided 2D material layer; forming a metal layer on the nitrided 2D material layer and filling in the opening; and performing a planarization process on the metal layer and the nitrided 2D material layer to expose a top surface of the dielectric layer.

## Claims

### Claim 1

A method of forming an interconnect structure, comprising:
forming an opening in a dielectric layer;
forming a 2D material layer to conformally cover a surface of the opening;
performing a nitridation treatment on the 2D material layer to form a nitrided 2D material layer;
forming a metal layer on the nitrided 2D material layer and filling in the opening; and
performing a planarization process on the metal layer and the nitrided 2D material layer to expose a top surface of the dielectric layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the 2D material layer comprises a transition metal dichalcogenide (TMD) material having a formula MX2, wherein M is a transition metal element, and X is a chalcogen.

### Claim 3 (depends on 2)

The method of claim 2, wherein the transition metal element comprises titanium, vanadium, cobalt, nickel, zirconium, molybdenum, technetium, rhodium, palladium, hafnium, tantalum, tungsten, rhenium, iridium, platinum, or a combination thereof, and the chalcogen comprises sulfur, selenium, tellurium, or a combination thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the nitrided 2D material layer comprises a transition metal nitride (TMN) material having a formula MNy, wherein M is a transition metal element, N is a nitrogen element, and y is 0.5 to 2.

### Claim 5 (depends on 1)

The method of claim 1, wherein after performing the nitridation treatment, transition metal elements in the nitrided 2D material layer are bonded together by nitrogen elements, so that a thickness of the nitrided 2D material layer is less than a thickness of the 2D material layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein a ratio of a thickness of the nitrided 2D material layer to a thickness of the 2D material layer is 0.3 to 0.4.

### Claim 7 (depends on 1)

The method of claim 1, wherein the nitridation treatment comprises a plasma-enhanced nitridation process, and a process temperature of the plasma-enhanced nitridation process is lower than 500° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein after performing the planarization process, the method further comprises forming a cap layer to cover the metal layer, the nitrified 2D material layer, and the dielectric layer.

### Claim 9

A method of forming an interconnect structure, comprising:
forming an opening in a dielectric layer;
forming a first material layer to conformally cover a surface of the opening;
performing a nitridation treatment on the first material layer with a semiconductor property to form a second material layer with a metal conductive property; and
forming a metal plug in the opening, so that the second material layer extends between the dielectric layer and a bottom surface and a sidewall of the metal plug.

### Claim 10 (depends on 9)

The method of claim 9, wherein the first material layer comprises a transition metal dichalcogenide (TMD) material having a formula MX2, wherein M is a transition metal element, and X is a chalcogen.

### Claim 11 (depends on 9)

The method of claim 9, wherein the second material layer comprises a transition metal nitride (TMN) material having a formula MNy, wherein M is a transition metal element, N is a nitrogen element, and y is 0.5 to 2.

### Claim 12 (depends on 9)

The method of claim 9, wherein after performing the nitridation treatment, transition metal elements in the second material layer are bonded together by nitrogen elements, so that a thickness of the second material layer is less than a thickness of the first material layer.

### Claim 13 (depends on 9)

The method of claim 9, wherein the nitridation treatment comprises a plasma-enhanced nitridation process, and a process temperature of the plasma-enhanced nitridation process is lower than 500° C.

### Claim 14 (depends on 9)

The method of claim 9, wherein a sidewall of the opening comprises a straight sidewall, an inclined sidewall, a stepped sidewall, or a combination thereof.

### Claim 15

An interconnect structure, comprising:
a conductive feature embedded in a dielectric layer; and
a barrier layer extending between the dielectric layer and a bottom surface and a sidewall of the conductive feature, wherein the barrier layer comprises a nitrided 2D material layer which is in direct contact with the conductive feature.

### Claim 16 (depends on 15)

The interconnect structure of claim 15, wherein the nitrided 2D material layer comprises a transition metal nitride (TMN) material having a formula MNy, wherein M is a transition metal element, N is a nitrogen element, and y is 0.5 to 2.

### Claim 17 (depends on 15)

The interconnect structure of claim 15, wherein transition metal elements in the nitrided 2D material layer are bonded together by nitrogen elements, so that the nitrided 2D material layer is configured as a three-dimensional (3D) crystal structure.

### Claim 18 (depends on 15)

The interconnect structure of claim 15, wherein a shortest distance between the transition metal elements in two adjacent layers is 2Å to 3 Å.

### Claim 19 (depends on 15)

The interconnect structure of claim 15, wherein the conductive feature comprises a metal plug, a metal layer, a metal routing, or a combination thereof.

### Claim 20 (depends on 15)

The interconnect structure of claim 15, wherein a thickness of the nitrided 2D material layer is 1 nm to 2 nm.