# US 2023/0411183 A1 · Dopant diffusion with short high temperature anneal pulses

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411183 A1
- Document ID: US20230411183A1
- Status: Published application
- Kind: A1
- Application number: 17/842,381
- Filed: 2022-06-16
- Published: 2023-12-21
- Earliest claimed: 2022-06-16
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Wolfgang R. ADERHOLD
- Web page: https://patentgrep.com/patent/US20230411183A1

## CPC

- H10P 72/0436: {mainly by radiation}
- H10D 62/834: further characterised by the dopants
- H10P 32/1408: {from or through or into an external applied layer, e.g. photoresist or nitride layers}
- H10P 32/171: {being group IV material}
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10D 30/0193: {by modifying properties of the stacked channels}
- H10D 30/501: {FETs having stacked nanowire, nanosheet or nanoribbon channels}
- H10D 62/121: {oriented parallel to substrates}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A method and apparatus for diffusing a dopant within a semiconductor device is described. The method includes performing a dynamic surface anneal in which a substrate is placed inside of a process volume with a mixture of an inert gas and a small amount of oxygen gas. The surface of the substrate is then exposed to one or more rapid laser pulses. The rapid laser bursts diffuse dopant from a doped layer into the substrate. The doped layer is formed during a previous process operation. The temperature and number of laser pulses control the amount of diffusion of the dopant into the substrate. Other dynamic surface anneal operations may be optionally performed before or after the oxygenated dynamic surface anneal operation.

## Claims

### Claim 1

A method of diffusing a dopant, suitable for use during semiconductor processing, comprising:
flowing an inert gas into a process volume of a process chamber;
flowing an oxygen containing gas into the process volume such that an oxygen partial pressure of the oxygen containing gas is about 0.1% to about 10% within the process volume; and
exposing a portion of a substrate within the process volume to one or more laser pulses to heat the portion of the substrate to a temperature of greater than about 850° C.

### Claim 2 (depends on 1)

The method of claim 1, wherein each laser pulse of the one or more laser pulses has a duration of less than about 1 second.

### Claim 3 (depends on 2)

The method of claim 2, wherein each of the laser pulses of the one or more laser pulses has a wavelength of about 200 nm to about 20000 nm.

### Claim 4 (depends on 3)

The method of claim 3, wherein each of the laser pulses of the one or more laser pulses has an energy density of about 0.1 W/cm2 to about 10 W/cm2.

### Claim 5 (depends on 1)

The method of claim 1, wherein the inert gas is one or a combination of argon, nitrogen, helium, neon, krypton, and xenon.

### Claim 6 (depends on 1)

The method of claim 1, wherein there are 1 to 50 individual laser pulses in the one or more laser pulses.

### Claim 7 (depends on 1)

The method of claim 1, wherein the temperature of the portion of the substrate during exposure is about 800° C. to about 1410° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein exposing the portion of the substrate to the one or more laser pulses diffuses the dopant into the substrate.

### Claim 9 (depends on 8)

The method of claim 8, wherein a layer with a dopant concentration of greater than about 1·1020 atoms/cm3 is on a top surface of the substrate during exposing of the portion of the substrate to the one or more laser pulses.

### Claim 10 (depends on 9)

The method of claim 9, wherein the dopant is one or a combination of phosphorous, boron, arsenic, gallium, indium, aluminum, and lithium.

### Claim 11

A method of diffusing a dopant, suitable for use during semiconductor processing, comprising:
depositing a doped layer with a dopant, the doped layer having a dopant concentration of greater than about 1·1020 atoms/cm3 on a top surface of a substrate in a first process chamber; and
performing an oxygenated dynamic surface anneal comprising:
flowing an inert gas into a process volume of a second process chamber;
flowing an oxygen gas into the process volume of the second process chamber such that an oxygen partial pressure of the oxygen gas is about 0.1% to about 10% within the process volume; and
exposing a portion of a substrate within the process volume to a one or more laser pulses to heat the portion of the substrate to a temperature of greater than about 800° C.

### Claim 12 (depends on 11)

The method of claim 11, further comprising performing a first dynamic surface anneal within the second process chamber before performing the oxygenated dynamic surface anneal, the first dynamic surface anneal comprising:
flowing an inert gas into the process volume of the second process chamber, such that an inert gas partial pressure of the inert gas is greater than 99.9% within the process volume; and
exposing the portion of a substrate within the process volume to a plurality of first laser pulses.

### Claim 13 (depends on 11)

The method of claim 11, wherein the doped layer has a concentration of greater than about 1·1021 atoms/cm3 and a thickness of about 0.1 nm to about 2 nm.

### Claim 14 (depends on 11)

The method of claim 11, wherein each laser pulse of the one or more laser pulses has a duration of less than about 0.1 second.

### Claim 15 (depends on 11)

The method of claim 11, wherein the inert gas is one or a combination of argon gas, nitrogen gas, helium, neon, krypton, and xenon.

### Claim 16 (depends on 11)

The method of claim 11, wherein there are 1 to 15 individual laser pulses in the one or more laser pulses.

### Claim 17 (depends on 11)

The method of claim 11, wherein the dopant is one or a combination of phosphorous, boron, arsenic, gallium, indium, aluminum, and lithium.

### Claim 18

A method of diffusing a dopant, suitable for use during semiconductor processing, comprising:
selectively depositing a doped layer with a dopant on a top surface of a substrate within a first process chamber, the doped layer having a dopant concentration of greater than about 1·1021 atoms/cm3; and
performing an oxygenated dynamic surface anneal to diffuse the dopant into the substrate comprising:
flowing an inert gas into a process volume of a second process chamber;
flowing an oxygen gas into the process volume of the second process chamber such that an oxygen partial pressure of the oxygen gas is about 0.1% to about 10% within the process volume; and
exposing a portion of a substrate within the process volume to a plurality of laser pulses to heat the portion of the substrate to a temperature of greater than about 800° C. and diffuse the dopant into the substrate; and
removing an oxide formed on the substrate after the diffusing the dopant.

### Claim 19 (depends on 18)

The method of claim 18, wherein after diffusing the dopant, the substrate has a second dopant concentration of greater than about 1·1012 atoms/cm3 at a depth of about nm from the top surface.

### Claim 20 (depends on 18)

The method of claim 18, wherein the temperature of the portion of the substrate during exposure to the plurality of laser pulses is less than about 1200° C.