# US 2023/0411175 A1 · Method for manufacturing a semiconductor package assembly as well as such semiconductor package assembly

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411175 A1
- Document ID: US20230411175A1
- Status: Published application
- Kind: A1
- Application number: 18/333,854
- Filed: 2023-06-13
- Published: 2023-12-21
- Earliest claimed: 2022-06-15
- Assignees: Nexperia B.V.
- Applicants: Nexperia B.V.
- Inventors: Wai Wai Lee; Ting Wei Chang; Jia Yunn Ting; Wei Leong Tan
- Web page: https://patentgrep.com/patent/US20230411175A1

## CPC

- H10W 70/424: {Cross-sectional shapes (H10W70/481 takes precedence)}
- H10W 74/016: {using moulds}
- H10P 72/0404: {for general liquid treatment, e.g. etching followed by cleaning}
- H10P 72/0416: {with the semiconductor substrates being dipped in baths or vessels}
- H10W 70/045: {Cleaning}
- H10W 72/071: {Connecting or disconnecting}
- H10W 74/127: {characterised by arrangements for sealing or adhesion}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing a semiconductor package assembly is provided. The assembly includes a semiconductor package and a molding resin case encapsulating the semiconductor package. The complete semiconductor package undergoes a surface roughening treatment, thus improving the overall adhesion with the molding resin (EMC) and reducing the risks of delamination.

## Claims

### Claim 1

A method for manufacturing a semiconductor package assembly, the method comprising the steps of
i) forming at least one semiconductor package by:
i1) providing a lead frame having a first frame side and a second frame side opposite to the first frame side;
i2) adhering at least one semiconductor die structure having a first die side and a second die side opposite to the first die side with the second die side on the first frame side of the lead frame, resulting in a first conductive connection between the lead frame and the at least one semiconductor die structure;
i3) adhering at least one bond element on the first die side of the at least one semiconductor die structure and/or on the first frame side of the lead frame, resulting in at least one further conductive connection between the at least one bond element and the at least one semiconductor die structure and between at least a further bond element and the lead frame;
and
ii) encapsulating the at least one semiconductor package with a molding resin, thereby forming at least one encapsulated semiconductor package assembly;
wherein, prior to step ii but after step i3, the method further comprises the step of:
iii) subjecting the exposed surfaces of the first frame side of the lead frame, the adhering connections and the at least one bond element of the at least one semiconductor package to a surface roughening treatment using a chemical solution, wherein the chemical solution is an organic or inorganic cleaning agent.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the organic or inorganic cleaning agent is a photoresist layer stripping agent.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the surface roughening treatment of step iii) consists of submerging the at least one semiconductor package in the chemical solution for a period of at least 10 minutes.

### Claim 4 (depends on 1)

The method according to claim 1, wherein prior to the encapsulating of step ii) but after the surface roughening treatment of step iii) the method further comprises the steps of:
iv) rinsing the semiconductor package with deionized water; and
v) drying the semiconductor package.

### Claim 5 (depends on 1)

The method according to claim 1, further comprising, after the encapsulating of step ii), the steps of:
vi) plating the exposed lead frame; and
vii) singulating the at least one encapsulated semiconductor package assembly.

### Claim 6 (depends on 2)

The method according to claim 2, wherein the surface roughening treatment of step iii) consists of submerging the at least one semiconductor package in the chemical solution for a period of at least 10 minutes.

### Claim 7 (depends on 2)

The method according to claim 2, wherein, prior to the encapsulating of step ii) but after the surface roughening treatment of step iii) the method further comprises the steps of:
iv) rinsing the semiconductor package with deionized water; and
v) drying the semiconductor package.

### Claim 8 (depends on 2)

The method according to claim 2, further comprising, after the encapsulating of step ii), the steps of:
vi) plating the exposed lead frame; and
vii) singulating the at least one encapsulated semiconductor package assembly.

### Claim 9 (depends on 2)

The method according to claim 2, wherein the photoresist layer stripping agent can be an aqueous, a solvent or a semi-aqueous agent.

### Claim 10 (depends on 3)

The method according to claim 3, wherein the submerging period is 20-40 minutes.

### Claim 11 (depends on 3)

The method according to claim 3, wherein the submerging period is about minutes.

### Claim 12 (depends on 3)

The method according to claim 3, wherein the submerging of step iii) is performed at an elevated temperature of at least 10° C. below the flashpoint temperature of the chemical solution used.

### Claim 13 (depends on 10)

The method according to claim 10, wherein the submerging period is about minutes.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the submerging of step iii) is performed at an elevated temperature of at least 10° C. below the flashpoint temperature of the chemical solution used.

### Claim 15 (depends on 12)

The method according to claim 12, wherein, prior to the encapsulating of step ii) but after the surface roughening treatment of step iii) the method further comprises the steps of:
iv) rinsing the semiconductor package with deionized water; and
v) drying the semiconductor package.

### Claim 16 (depends on 1)

A semiconductor package assembly comprising:
semiconductor package composed of a lead frame having a first frame side and a second frame side opposite to the first frame side; at least one semiconductor die structure having a first die side and a second die side opposite to the first die side being adhered with the second die side on the first frame side of the lead frame, resulting in a first conductive connection between the lead frame and the at least one semiconductor die structure; at least one bond element adhered on the first die side of the at least one semiconductor die structure and/or on the first frame side of the lead frame, resulting in at least one further conductive connection between the at least one bond element and the at least one semiconductor die structure and between at least a further bond element and the lead frame; and
a molding resin encapsulating the at least one semiconductor package, wherein prior to encapsulating the at least one semiconductor package with the molding resin the exposed surfaces of the first frame side of the lead frame, the adhering connections and the at least one bond element of the at least one semiconductor package are surface roughened using a chemical solution using the method steps of claim 1.