# US 2023/0411157 A1 · Methods of manufacturing semiconductor devices including a repeating pattern of lines and spaces

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411157 A1
- Document ID: US20230411157A1
- Status: Published application
- Kind: A1
- Application number: 18/136,407
- Filed: 2023-04-19
- Published: 2023-12-21
- Earliest claimed: 2022-06-15
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Seungkyo Lee; Jongin Kang; Gyeyoung Kim; Youngwoo Kim; Yonghan Park; Woojin Jung; Seunguk Han; Juyoung Huh
- Web page: https://patentgrep.com/patent/US20230411157A1

## CPC

- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 50/283: {by chemical means}
- H10P 50/693: {characterised by their size, orientation, disposition, behaviour or shape, in horizontal or vertical plane}
- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- H10P 50/73: {using masks for insulating materials}
- H10P 76/20: of masks comprising organic materials
- H10P 76/408: {characterised by their sizes, orientations, dispositions, behaviours or shapes}
- H10W 46/00: Marks applied to devices, e.g. for alignment or identification
- H10W 76/40: Fillings or auxiliary members in containers, e.g. centering rings (fillings or auxiliary members for thermal protection or control in containers or encapsulations H10W40/70)
- H10W 46/301: {for alignment}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a semiconductor device includes: forming a mask layer, a first separation layer, a first mandrel layer, a second separation layer and a second mandrel layer on a substrate; patterning the second mandrel layer to form second mandrel patterns; forming first spacers on the second mandrel patterns; removing the second mandrel patterns; patterning the second separation layer and the first mandrel layer to form first structures; forming a second spacer layer on the first structures and the first separation layer; anisotropically etching the second spacer layer to form second spacers on the first structures, and to form first dummy patterns and align key patterns on the first structures; and spin-coating a spin-on hard mask layer on the first separation layer, wherein the spin-on hard mask layer covers the first structures, the first dummy patterns and the align key patterns.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, the method comprising:
forming a mask layer, a first separation layer, a first mandrel layer, a second separation layer and a second mandrel layer on a substrate including a main chip region and a scribe lane region;
patterning the second mandrel layer to form second mandrel patterns that extend in a first direction and separated from each other on the main chip region and the scribe lane region;
forming first spacers on the second mandrel patterns in the main chip region and the scribe lane region;
removing the second mandrel patterns;
patterning the second separation layer and the first mandrel layer by using the first spacers to form first structures that include a first mandrel pattern and a second separation layer pattern stacked on the first mandrel pattern;
forming a second spacer layer on the first structures and on the first separation layer in the main chip region and the scribe lane region;
anisotropically etching the second spacer layer to form second spacers on side walls of the first structures of the main chip region, and to form first dummy patterns and align key patterns on the side walls of the first structures of the scribe lane region; and
spin-coating a spin-on hard mask layer on the first separation layer, wherein the spin-on hard mask layer covers the first structures, the first dummy patterns and the align key patterns.

### Claim 2 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein the second mandrel patterns have the same shape and the same arrangement as each other in the main chip region and in the scribe lane region.

### Claim 3 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein a line width of each of the second mandrel patterns is about three times a first target line width of each of the second spacers, and a gap between the second mandrel patterns is about five times the first target line width.

### Claim 4 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein each of the second spacers, first dummy patterns and align key patterns extends in the first direction, and has a repeating arrangement of lines and spaces.

### Claim 5 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein a line width of each of the second spacers, a line width of each of the first dummy patterns and a line width of each of the align key patterns are the same as each other.

### Claim 6 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein a first pitch, which is the sum of one line width of a second spacer of the second spacers and one gap between the second spacers, a second pitch, which is the sum of one line width of a first dummy pattern of the first dummy patterns and one gap between the first dummy patterns, and a third pitch, which is the sum of one line width of an align key pattern of the align key patterns and one gap between the align key patterns, are the same as each other.

### Claim 7 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, further comprising:
forming a photoresist pattern on the spin-on hard mask layer, wherein the photoresist pattern exposes the main chip region;
removing the first structures and the spin-on hard mask layer in the main chip region by using the photoresist pattern as an etching mask; and
etching the mask layer using the second spacers in the main chip region as an etching mask to form mask patterns.

### Claim 8 (depends on 7)

The method of manufacturing a semiconductor device of claim 7, further comprising:
etching the substrate using the mask patterns to form a recess; and
forming a gate structure in the recess.

### Claim 9 (depends on 1)

The method of manufacturing a semiconductor device of claim 1, wherein
a cell block region and a cell block division region are in the main chip region; and
second dummy patterns are formed on the side walls of the first structure in the cell block division region.

### Claim 10 (depends on 9)

The method of manufacturing a semiconductor device of claim 9, wherein the second dummy patterns extend in the first direction.

### Claim 11

A method of manufacturing a semiconductor device, the method comprising:
forming a mask layer, a first separation layer, a first mandrel layer, a second separation layer and a second mandrel layer on a substrate including a main chip region and a scribe lane region;
patterning the second mandrel layer to form second mandrel patterns that extend in a first direction and separated from each other on the main chip region and the scribe lane region;
forming first spacers on the side walls of the second mandrel patterns in the main chip region and the scribe lane region, wherein the first spacers have a first target line width;
removing the second mandrel patterns;
patterning the second separation layer and the first mandrel layer using the first spacers to form first structures that include a first mandrel pattern and a second separation layer pattern stacked on the first mandrel pattern and that extend in the first direction;
forming a second spacer layer on the first structures and on the first separation layer in the main chip region and the scribe lane region;
anisotropically etching the second spacer layer to form second spacers, which have the first target line width, on side walls of the first structures of the main chip region, and to form first dummy patterns, which have the first target line width, and align key patterns, which have the first target line width, on the side walls of the first structures of the scribe lane region;
spin-coating a spin-on hard mask layer on the first separation layer, wherein the spin-on hard mask layer covers the first structures, the first dummy patterns and the align key patterns;
forming a photoresist pattern on the spin-on hard mask layer, wherein the photoresist pattern exposes the main chip region;
removing the first structures and the spin-on hard mask layer in the main chip region by using the photoresist pattern as an etching mask; and
etching the mask layer using the second spacers in the main chip region as an etching mask to form mask patterns.

### Claim 12 (depends on 11)

The method of manufacturing a semiconductor device of claim 11, wherein each of the second spacers, first dummy patterns and align key patterns extends in the first direction, and has a repeating arrangement of lines and spaces.

### Claim 13 (depends on 11)

The method of manufacturing a semiconductor device of claim 11, wherein a first pitch, which is the sum of one line width of a second spacer of the second spacers and one gap between the second spacers, a second pitch, which is the sum of one line width of a first dummy pattern of the first dummy patterns and one gap between the first dummy patterns, and a third pitch, which is the sum of one line width of an align key pattern of the align key patterns and one gap between the align key patterns, are the same as each other.

### Claim 14 (depends on 11)

The method of manufacturing a semiconductor device of claim 11, wherein
a cell block region and a cell block division region in the main chip region; and
second dummy patterns are formed on the side walls of the first structures in the cell block division region.

### Claim 15 (depends on 14)

The method of manufacturing a semiconductor device of claim 14, wherein the second dummy patterns extend in the first direction.

### Claim 16 (depends on 14)

The method of manufacturing a semiconductor device of claim 14, wherein the second spacer layer is formed by an atomic layer deposition method.

### Claim 17

A semiconductor device, comprising:
a substrate comprising a main chip region and a scribe lane region;
a cell pattern structure formed on the main chip region of the substrate, and spacers that extend in a first direction are separated from each other and repeatedly arranged;
a dummy pattern structure formed the scribe lane region of the substrate, wherein first dummy patterns that extend in the first direction are separated from each other and repeatedly arranged; and
an align key pattern structure formed on the scribe lane region of the substrate, wherein align key patterns that extend in the first direction are separated from each other and repeatedly arranged.

### Claim 18 (depends on 17)

The semiconductor device of claim 17, wherein a line width of each of the spacers, a line width of each of the first dummy patterns and a line width of each of the align key patterns, are the same as each other.

### Claim 19 (depends on 17)

The semiconductor device of claim 17, wherein a first pitch, which is the sum of one line width of a spacer of the spacers and one gap between the spacers, a second pitch, which is the sum of one line width of a first dummy pattern of the first dummy patterns and one gap between the first dummy patterns, and a third pitch, which is the sum of one line width of an align key pattern of the align patterns and one gap between the align key patterns, are the same as each other.

### Claim 20 (depends on 17)

The semiconductor device of claim 17, wherein a cell block region and a cell block division region are in the main chip region, and second dummy patterns that extend in the first direction are provided in the cell block division region.