# US 2023/0411150 A1 · Cyclic Spin-On Coating Process for Forming Dielectric Material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411150 A1
- Document ID: US20230411150A1
- Status: Published application
- Kind: A1
- Application number: 18/362,136
- Filed: 2023-07-31
- Published: 2023-12-21
- Earliest claimed: 2018-05-30
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Je-Ming Kuo; Yen-Chun Huang; Chih-Tang Peng; Tien-I Bao
- Web page: https://patentgrep.com/patent/US20230411150A1

## CPC

- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P 14/6689: {the compound being a silazane}
- B05D 3/067: {Curing or cross-linking the coating}
- B05D 7/546: {each layer being cured, at least partially, separately}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10D 84/0151: {Manufacturing their isolation regions}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/6304: {Formation by oxidation, e.g. oxidation of the substrate}
- H10P 14/6519: {the substance being oxygen}
- H10P 14/6522: {introduced into a nitride material, e.g. changing SiN to SiON}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6538: {by exposure to UV light}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P 50/283: {by chemical means}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W 20/098: {by filling between adjacent conductive parts}
- B05D 1/005: {Spin coating}
- B05D 1/38: with intermediate treatment (intermediate treatment per se B05D3/00)
- G03F 7/162: {Coating on a rotating support, e.g. using a whirler or a spinner}
- H10P 14/6322: {Formation by thermal treatments (formation by plasma treatment H10P14/6319)}
- H10W 20/075: {of multilayered thin functional dielectric layers}
- H10W 20/095: {by irradiating with electromagnetic or particle radiation (plasma treatment H10W20/096)}
- H10W 20/096: {by contacting with gases, liquids or plasmas}
- H10W 20/097: {by thermally treating}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

The present disclosure is generally related to semiconductor devices, and more particularly to a dielectric material formed in semiconductor devices. The present disclosure provides methods for forming a dielectric material layer by a cyclic spin-on coating process. In an embodiment, a method of forming a dielectric material on a substrate includes spin-coating a first portion of a dielectric material on a substrate, curing the first portion of the dielectric material on the substrate, spin-coating a second portion of the dielectric material on the substrate, and thermal annealing the dielectric material to form an annealed dielectric material on the substrate.

## Claims

### Claim 1

A method of semiconductor processing, the method comprising:
spin-coating a first portion of a dielectric material on to a non-planar substrate;
curing the first portion of the dielectric material to decompose Si—N and Si—H bonds in the first portion of the dielectric material to form a first silicon nitride;
spin-coating a second portion of the dielectric material on the first portion of the dielectric material, wherein the second portion comprises a second silicon nitride; and
thermal annealing the dielectric material to form an annealed dielectric material on the substrate, wherein the thermal annealing the dielectric material converts the first silicon nitride and the second silicon nitride into a silicon oxide material and increases a thickness of the dielectric material.

### Claim 2 (depends on 1)

The method of claim 1, wherein the spin-coating the first portion of the dielectric material onto the non-planar substrate fills surface discontinuities in the non-planar substrate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the curing the first portion of the dielectric material comprises providing a UV energy to the first portion of the dielectric material.

### Claim 4 (depends on 3)

The method of claim 3, wherein the providing the UV energy further comprises controlling a substrate temperature of the non-planar substrate in a range of 50° C. to 400° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the thermal annealing the dielectric material further comprises supplying an oxygen containing gas to the dielectric material during the thermal annealing of the dielectric material.

### Claim 6 (depends on 5)

The method of claim 5, wherein the thermal annealing the dielectric material further comprises controlling a substrate temperature of the non-planar substrate in a range of 400° C. to 1200° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the spin-coating the first portion of the dielectric material further comprises:
spin-coating a first solution onto the non-planar substrate, wherein the first solution comprises a perhydro-polysilazane compound and a solvent and wherein the curing the first portion of the dielectric material drives out the solvent from the first solution.

### Claim 8

A method of semiconductor processing, the method comprising curing a first solution to form a cured first portion in a curing apparatus, wherein the cured first portion is silicon nitride;
spin-coating a second solution on to the cured first portion in a coating apparatus;
curing the second solution to form a cured second portion in the curing apparatus, wherein the cured second portion is silicon nitride; and
annealing the cured first portion and the cured second portion to form an annealed dielectric material in an annealing apparatus, wherein the annealed dielectric material is silicon oxide, wherein a first thickness of the cured first portion and the cured second portion before the annealing the cured first portion and the cured second portion is less than a second thickness of the annealed dielectric material.

### Claim 9 (depends on 8)

The method of claim 8, wherein the annealed dielectric material is a shallow trench isolation.

### Claim 10 (depends on 8)

The method of claim 8, wherein the first solution comprises a perhydro-polysilazane compound having an average molecular weight in a range of 5000 g/mol to about 8000 g/mol.

### Claim 11 (depends on 10)

The method of claim 10, wherein the first solution comprises 5 to 30 percent by weight of the perhydro-polysilazane compound.

### Claim 12 (depends on 8)

The method of claim 8, wherein the curing the second solution comprises exposing the second solution to a UV energy.

### Claim 13 (depends on 8)

The method of claim 8, wherein the annealing the cured first portion comprises supplying an oxygen-containing gas in the annealing apparatus.

### Claim 14 (depends on 8)

The method of claim 8, wherein the annealing the cured first portion comprises controlling a substrate temperature of a non-planar substrate in a range of 400° C. to 1200° C.

### Claim 15 (depends on 8)

The method of claim 8, wherein a nitrogen concentration of the annealed dielectric material is less than 5 atomic percent.

### Claim 16

A method of semiconductor processing, the method comprising:
curing a first portion of a first solution to form a first moisture-free portion of a dielectric material;
spin-coating a second portion of the first solution on the first moisture-free portion of the dielectric material; and
annealing the second portion of the first solution and the first moisture-free portion of the dielectric material to form a dielectric layer, wherein the annealing converts both the second portion of the first solution and the first moisture-free portion of the dielectric material from a non-oxide into an oxide, wherein the first moisture-free portion of the dielectric material and the second portion of the first solution have a first thickness before the annealing and the dielectric layer has a second thickness after the annealing, wherein the second thickness is greater than the first thickness.

### Claim 17 (depends on 16)

The method of claim 16, wherein the curing the first portion of the first solution comprises exposing the first portion of the first solution to a UV light having a wavelength in a range of 100 nm to 300 nm.

### Claim 18 (depends on 16)

The method of claim 16, wherein the curing the first portion of the first solution comprises exposing the first portion of the first solution to a UV light having a UV power in a range of 500 mJ/cm2 to about 6000 mJ/cm2.

### Claim 19 (depends on 16)

The method of claim 16, further comprising curing the second portion of the first solution by providing a UV energy to the second portion, wherein the UV energy decomposes Si—N and Si—H bonds in the second portion to form silicon nitride before the annealing.

### Claim 20 (depends on 16)

The method of claim 16, wherein the dielectric layer comprises a silicon oxide material having a nitrogen content in a range from about 0.005 atomic percent to about 0.5 atomic percent.