# US 2023/0411104 A1 · Method of forming field emission cathodes by co-electrodeposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411104 A1
- Document ID: US20230411104A1
- Status: Published application
- Kind: A1
- Application number: 18/247,298
- Filed: 2021-09-29
- Published: 2023-12-21
- Earliest claimed: 2020-09-30
- Assignees: NCX Corporation
- Applicants: NCX Corporation
- Inventors: Cheng QIAN
- Web page: https://patentgrep.com/patent/US20230411104A1

## CPC

- H01J 9/025: {of field emission cathodes}
- C09D 5/4457: {containing special additives, e.g. pigments, polymeric particles}
- C09D 5/4473: {Mixture of polymers}
- C25D 13/12: characterised by the article coated
- C25D 13/22: Servicing or operating {apparatus or multistep processes}
- H01J 1/3048: {Distributed particle emitters}
- C01B 32/174: Derivatisation; Solubilisation; Dispersion in solvents
- C01B 2202/36: Diameter
- C25D 13/02: with inorganic material
- H01J 2201/30469: Carbon nanotubes (CNTs)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

A method for fabricating an electron field emission cathode, the field emission cathode including a substrate having a field emission layer engaged therewith, where the field emission layer incorporates modified carbon nanotubes and a matrix material to improve field emission characteristics of the cathode and field emission cathode devices implementing such cathodes.

## Claims

### Claim 1

A method of forming a field emission cathode, comprising:
forming a field emission material, comprising:
mixing a plurality of carbon nanotubes and a poly(3,4-ethylendioxythiophene)-poly(styrene sulfonic acid) (PEDOT:PSS) solution in water at a particular ratio to form a base mixture;
exposing the base mixture to an ultrasonic dispersion process at a power of greater than 1 W/cm2 and at a frequency of about 20-50 kHz;
introducing at least one matrix particle, at least one metal salt, at least one charger, or a combination thereof to the base mixture to form a field emission material precursor; and
exposing the field emission material precursor to an ultrasonic dispersion process at a power of less than 1 W/cm2 and at a frequency of greater than 50 kHz to form a stable suspension of the field emission material precursor;
depositing a layer of the field emission material precursor on to at least a portion of a substrate via a co-electrodeposition process;
drying the layer and the substrate at a temperature of about 20° C. to about 150° C. at atmosphere or under a vacuum;
annealing the layer and the substrate at a temperature of about 300° C. to about 1000° C. under a vacuum; and
activating the layer of the field emission material to obtain the field emission cathode.

### Claim 2 (depends on 1)

The method of claim 1, wherein mixing the plurality of carbon nanotubes and the PEDOT:PSS solution comprises mixing the plurality of carbon nanotubes and the PEDOT:PSS solution such that the particular ratio of carbon nanotubes to PEDOT:PSS solution ranges from 10:1 to 1:10.

### Claim 3 (depends on 1)

The method of claim 1, wherein introducing at least one matrix particle comprises introducing at least one glass particle.

### Claim 4 (depends on 3)

The method of claim 3, wherein introducing at least one glass particle comprises introducing at least one glass particle having a diameter of between about 100 nm to about 3 micrometers.

### Claim 5 (depends on 3)

The method of claim 3, wherein introducing at least one matrix particle comprises introducing at least one matrix particle such that the at least one matrix particle is dispersed in the base mixture at up to 10 wt % of total liquid medium of the field emission material precursor.

### Claim 6 (depends on 1)

The method of claim 1, wherein introducing at least one matrix particle comprises introducing at least one metal salt selected from the group consisting of a silver salt, a copper salt, a platinum salt, a bismuth salt, a tungsten salt, a stibium salt, a gold salt, or combinations thereof.

### Claim 7 (depends on 6)

The method of claim 6, wherein introducing at least one matrix particle comprises introducing at least one metal salt such that the at least one metal salt is dispersed in the base mixture at up to 10 wt % of total liquid medium of the field emission material precursor.

### Claim 8 (depends on 1)

The method of claim 1, wherein introducing at least one matrix particle comprises introducing at least one charger selected from the group consisting of a lithium salt, a sodium salt, a calcium salt, a magnesium salt, an aluminum salt, a zinc salt, an iron salt, a cobalt salt, a nickel salt, an ammonium salt, or combinations thereof.

### Claim 9 (depends on 8)

The method of claim 8, wherein introducing at least one matrix particle comprises introducing at least one charger such that the at least one charger is dispersed in the base mixture at up to 1 wt % of total liquid medium of the field emission material precursor.

### Claim 10 (depends on 1)

The method of claim 1, wherein depositing the layer of the field emission material precursor depositing the layer of the field emission material precursor on to the at least a portion of the substrate comprising a metal, an alloy, a glass, or a ceramic.

### Claim 11 (depends on 1)

The method of claim 1, wherein activating the layer of the field emission material comprises:
applying an adhesive tape on to a surface of the layer of the field emission material; and
removing the adhesive tape from the layer of the field emission material.

### Claim 12 (depends on 1)

The method of claim 1, wherein activating the layer of the field emission material comprises:
applying a curable adhesive on to a surface of the layer of the field emission material;
exposing the adhesive to a heat source or an ultraviolet light to cure the adhesive and form a layer of an adhesive film; and
removing the layer of adhesive film from the layer of the field emission material.

### Claim 13

A method of forming a field emission material precursor, comprising:
introducing a plurality of carbon nanotubes into a liquid medium;
introducing a PEDOT:PSS solution into the liquid medium at a particular ratio to the plurality of carbon nanotubes;
mixing the plurality of carbon nanotubes and the PEDOT:PSS solution via an ultrasonic dispersion process at a power of greater than 1 W/cm2 and at a frequency of about 20-50 kHz to form a base mixture;
introducing at least one matrix particle, at least one metal salt, at least one charger, or a combination thereof in the base mixture; and
exposing the base mixture comprising the at least one matrix particle, the at least one metal salt, and the at least one charger to an ultrasonic dispersion process at a power of less than 1 W/cm2 and at a frequency of greater than 50 kHz to form a stable suspension of a field emission material precursor.

### Claim 14 (depends on 13)

The method of claim 13, wherein introducing the PEDOT:PSS solution into the liquid medium comprises introducing a PEDOT:PSS solution into the water with the particular ratio of carbon nanotubes to PEDOT:PSS solution ranging from 10:1 to 1:10.

### Claim 15 (depends on 13)

The method of claim 13, comprising depositing the field emission material precursor on to a substrate via a co-electrodeposition process.

### Claim 16 (depends on 13)

The method of claim 13, wherein introducing at least one matrix particle comprises introducing at least one glass particle.

### Claim 17 (depends on 13)

The method of claim 13, wherein introducing at least one matrix particle comprises introducing at least one matrix particle such that the at least one matrix particle is dispersed in the base mixture up to 10 wt % of total liquid medium of the field emission material precursor.

### Claim 18 (depends on 13)

The method of claim 13, wherein introducing at least one matrix particle comprises introducing at least one metal salt selected from the group consisting of a silver salt, a copper salt, a platinum salt, a bismuth salt, a tungsten salt, a stibium salt, a gold salt, or combinations thereof.

### Claim 19 (depends on 13)

The method of claim 13, wherein introducing at least one matrix particle comprises introducing at least one metal salt such that the at least one metal salt is dispersed in the base mixture at up to 10 wt % of total liquid medium of the field emission precursor material.

### Claim 20 (depends on 13)

The method of claim 13, wherein introducing at least one matrix particle comprises introducing at least one charger selected from the group consisting of a lithium salt, a sodium salt, a calcium salt, a magnesium salt, an aluminum salt, a zinc salt, an iron salt, a cobalt salt, a nickel salt, an ammonium salt, or combinations thereof.

### Claim 21 (depends on 13)

The method of claim 13, wherein introducing at least one matrix particle comprises introducing at least one charger such that the at least one charger is dispersed in the base mixture at up to 1 wt % of total liquid medium of the field emission precursor material.

### Claim 22 (depends on 13)

A method of forming a field emission cathode, comprising:
depositing a layer of the field emission material of claim 13 on to at least a portion of a substrate via a co-electrodeposition process;
drying the layer and the substrate at a temperature of about 20° C. to about 150° C. at atmosphere or under a vacuum;
annealing the layer and the substrate at a temperature of about 300° C. to about 1000° C. under a vacuum; and
activating the layer of the field emission material to obtain the field emission cathode.

### Claim 23

(canceled)