# US 2023/0411061 A1 · Laminated sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0411061 A1
- Document ID: US20230411061A1
- Status: Published application
- Kind: A1
- Application number: 18/455,359
- Filed: 2023-08-24
- Published: 2023-12-21
- Earliest claimed: 2020-02-17
- Assignees: Nitto Denko Corporation
- Applicants: Nitto Denko Corporation
- Inventors: Yoshihiro FURUKAWA; Keisuke OKUMURA
- Web page: https://patentgrep.com/patent/US20230411061A1

## CPC

- H01F 17/04: with magnetic core
- B32B 3/08: characterised by added members at particular parts {(layer formed of separate pieces of material which are juxtaposed side-by-side B32B3/14, B32B3/18)}
- B32B 3/30: characterised by a layer formed with recesses or projections, e.g. {hollows, grooves, protuberances, ribs (apertured layer B32B3/266; layer with cavities or internal voids B32B3/26)}
- B32B 5/30: one layer {being formed of particles, e.g. chips,} granules, powder
- B32B 7/02: Physical, chemical or physicochemical properties
- B32B 7/025: Electric or magnetic properties
- B32B 27/14: next to a particulate layer
- B32B 27/20: using fillers, pigments, thixotroping agents
- B32B 27/26: using curing agents
- B32B 27/283: {comprising polysiloxanes}
- B32B 27/38: comprising epoxy resins
- B32B 27/42: comprising condensation resins of aldehydes, e.g. with phenols, ureas or melamines
- H01F 1/26: by macromolecular organic substances
- H01F 27/255: made from particles (H01F27/26 takes precedence)
- B32B 5/16: characterised by features of a layer formed of particles, e.g. chips, powder {or granules (layer formed of natural mineral particles B32B19/00; layer being formed of wood fibres, chips or particles B32B21/02)}
- B32B 2250/04: 4 layers
- B32B 2255/04: on a particulate layer
- B32B 2255/205: Metallic coating
- B32B 2260/025: Particulate layer
- B32B 2260/046: Synthetic resin
- B32B 2264/10: Inorganic particles
- B32B 2264/102: Oxide or hydroxide
- B32B 2264/105: Metal
- B32B 2264/107: Ceramic
- B32B 2264/12: Mixture of at least two particles made of different materials
- B32B 2270/00: Resin or rubber layer containing a blend of at least two different polymers
- B32B 2307/20: having particular electrical or magnetic properties, e.g. piezoelectric
- B32B 2307/202: Conductive
- B32B 2307/208: Magnetic, paramagnetic
- B32B 2307/538: Roughness
- B32B 2307/732: Dimensional properties
- B32B 2457/00: Electrical equipment
- H01F 2017/048: {with encapsulating core, e.g. made of resin and magnetic powder}
- Y10T 428/32: Composite [nonstructural laminate] of inorganic material having metal-compound-containing layer and having defined magnetic layer
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A laminated sheet includes a sheet-shaped inductor including a plurality of wirings and a magnetic layer embedding the plurality of wirings, and a processing stability layer disposed on at least one surface in a thickness direction of the inductor. The magnetic layer includes a binder and a magnetic particle having a generally flat shape and whose material is a metal. The processing stability layer includes a cured product of a thermosetting resin composition. The thermosetting resin composition includes a thermosetting resin as an essential component. The thermosetting resin composition includes at least one kind of particle, as an optical component, selected from the group consisting of a first particle having a generally spherical shape and a second particle having a generally flat shape and whose material is an inorganic compound.

## Claims

### Claim 1

A laminated sheet comprising:
a sheet-shaped inductor including a plurality of wirings and a magnetic layer embedding the plurality of wirings, and
a processing stability layer disposed on the inductor, wherein
the magnetic layer has a first surface and a second surface spaced from the first surface,
the magnetic layer includes a binder, and
a magnetic particle having a generally flat shape and whose material is a metal;
the processing stability layer includes a cured product of a thermosetting resin composition; and
the thermosetting resin composition includes:
a thermosetting resin, and
at least one particle selected from the group consisting of a first particle having a generally spherical shape and a second particle having a generally flat shape and whose material is an inorganic compound, and any combinations thereof; and
wherein the processing stability layer is in contact with the first surface of the magnetic layer.

### Claim 2 (depends on 1)

The laminated sheet according to claim 1, wherein
the processing stability layer is in contact with the entire first surface.

### Claim 3 (depends on 1)

The laminated sheet according to claim 1, further comprising a second processing stability layer being contact with the second surface of the magnetic layer.

### Claim 4 (depends on 3)

The laminated sheet according to claim 3, wherein
the second processing stability layer is in contact with the entire second surface.

### Claim 5 (depends on 1)

The laminated sheet according to claim 1, wherein
the particle included in the thermosetting resin composition consists of the first particle.

### Claim 6 (depends on 1)

The laminated sheet according to claim 1 satisfying at least one test of the following test (a) to test (e):
test (a): the laminated sheet is trimmed into a 3 cm square piece to fabricate a sample, and the relative permeability μ1 thereof at a frequency of 10 MHz is determined, thereafter, the sample is immersed in 200 mL of copper sulfate plating solution containing 66 g/L of copper sulfate pentahydrate, 180 g/L of sulfuric acid concentration, 50 ppm of chlorine, and Top Lutina alpha at 25° C. for 120 minutes, and thereafter, the relative permeability μ2 of the sample at a frequency of 10 MHz is determined, by the following formula, a rate of change of the magnetic permeability before and after the immersion is determined, and as a result, the rate of change of the magnetic permeability of the sample is 5% or less:
Rate of Change of Magnetic Permeability (%)=Iμ1−μ2I/μ1×100;
test (b): the laminated sheet is trimmed into a 3 cm square piece to fabricate a sample, and the relative permeability μ3 thereof at a frequency of 10 MHz is determined, thereafter, the sample is immersed in 200 mL of an acid active aqueous solution containing 55 g/L of sulfuric acid at 25° C. for 1 minute, and thereafter, the relative permeability μ4 of the sample at a frequency of 10 MHz is determined, by the following formula, a rate of change of the magnetic permeability before and after the immersion is determined, and as a result, the rate of change of the magnetic permeability of the sample is 5% or less:
Rate of Change of Magnetic Permeability (%)=Iμ3−μ4I/μ3×100;
test (c): the laminated sheet is trimmed into a 3 cm square piece to fabricate a sample, and the relative permeability μ5 thereof at a frequency of 10 MHz is determined, thereafter, the sample is immersed in 200 mL of Reduction Solution Securiganth P manufactured by Atotech Japan K.K. at 45° C. for 5 minutes, and thereafter, the relative permeability μ6 of the sample at a frequency of 10 MHz is determined, by the following formula, a rate of change of the magnetic permeability before and after the immersion is determined, and as a result, the rate of change of the magnetic permeability of the sample is 5% or less:
Rate of Change of Magnetic Permeability (%)=Iμ5−μ6I/μ5×100;
test (d): the laminated sheet is trimmed into a 3 cm square piece to fabricate a sample, and the relative permeability μ7 thereof at a frequency of 10 MHz is determined, thereafter, the sample is immersed in 200 mL of Concentrate Compact CP manufactured by Atotech Japan K.K. at 80° C. for 15 minutes, and thereafter, the relative permeability μ8 of the sample at a frequency of 10 MHz is determined, by the following formula, a rate of change of the magnetic permeability before and after the immersion is determined, and as a result, the rate of change of the magnetic permeability of the sample is 5% or less:
Rate of Change of Magnetic Permeability (%)=Iμ7−μ8I/μ7×100;
test (e): the laminated sheet is trimmed into a 3 cm square piece to fabricate a sample, and the relative permeability μ9 thereof at a frequency of 10 MHz is determined, thereafter, the sample is immersed in 200 mL of Swelling Dip Securiganth P manufactured by Atotech Japan K.K. at 60° C. for 5 minutes, and thereafter, the relative permeability μ10 of the sample at a frequency of 10 MHz is determined, by the following formula, a rate of change of the magnetic permeability before and after the immersion is determined, and as a result, the rate of change of the magnetic permeability of the sample is 5% or less:
Rate of Change of Magnetic Permeability (%)=Iμ9−μ101/μ9×100.

### Claim 7 (depends on 1)

The laminated sheet according to claim 1, wherein
the arithmetic average roughness Ra of a surface of the processing stability layer is 10 μm or less.