# US 2023/0408733 A1 · Optical body, manufacturing method of optical body, laminate, and image sensor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0408733 A1
- Document ID: US20230408733A1
- Status: Published application
- Kind: A1
- Application number: 18/255,454
- Filed: 2021-12-10
- Published: 2023-12-21
- Earliest claimed: 2020-12-11
- Assignees: Dexerials Corporation
- Applicants: Dexerials Corporation
- Inventors: Shunichi KAJIYA
- Web page: https://patentgrep.com/patent/US20230408733A1

## CPC

- G02B 1/118: having sub-optical wavelength surface structures designed to provide an enhanced transmittance, e.g. moth-eye structures
- B32B 7/023: Optical properties
- B32B 27/18: characterised by the use of special additives
- G02B 1/111: using layers comprising organic materials
- G02B 1/12: by surface treatment, e.g. by irradiation
- G02B 5/208: {for use with infrared or ultraviolet radiation, e.g. for separating visible light from infrared and/or ultraviolet radiation}
- G02B 5/22: Absorbing filters {(G02B5/201 - G02B5/208 take precedence)}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

An optical body that has excellent anti-reflection performance and transmittance for light having wavelengths in the visible light band and good absorption performance for light having wavelengths in the near-infrared band is provided. To solve the above problem, the present disclosure provides an optical body 100 including a base material 20, a dye-containing resin layer 30 formed on the base material 20, and an anti-reflection layer 40 formed on the resin layer 30 and having a micro uneven structure in at least one surface. The average spectral transmittance of the optical body 100 for light in a wavelength range of 420 to 680 nm is 60% or greater, and the minimum spectral transmittance of the optical body 100 for light in a wavelength range of 750 to 1400 nm is less than 60%.

## Claims

### Claim 1

An optical body comprising:
a base material;
a dye-containing resin layer formed on the base material; and
an anti-reflection layer formed on the resin layer, the anti-reflection layer having a micro uneven structure in at least one surface,
wherein average spectral transmittance of the optical body for light in a wavelength range of 420 to 680 nm is 60% or greater, and minimum spectral transmittance of the optical body for light in a wavelength range of 750 to 1400 nm is less than 60%.

### Claim 2 (depends on 1)

The optical body according to claim 1, wherein the anti-reflection layer has the micro uneven structure in both surfaces.

### Claim 3 (depends on 1)

The polarization element according to claim 1, wherein storage elastic modulus of the resin layer is less than storage elastic modulus of the anti-reflection layer.

### Claim 4 (depends on 1)

The optical body according to claim 1, wherein thickness of the resin layer is greater than or equal to 1 μm.

### Claim 5 (depends on 1)

The optical body according to claim 1, wherein thickness of the anti-reflection layer is 0.2 to 1.0 μm.

### Claim 6 (depends on 1)

The optical body according to claim 1, wherein a retention film is further formed on the anti-reflection layer.

### Claim 7

A manufacturing method of an optical body, comprising the steps of:
making an anti-reflection layer having a micro uneven structure in a surface by curing a retention film while the retention film is pressed against a curable resin, the retention film having a micro uneven structure with an uneven period less than or equal to a wavelength of visible light; and
making an optical body with the retention film by, after a dye-containing curable resin is applied to a base material, curing the obtained anti-reflection layer while the anti-reflection layer is pressed against the dye-containing curable resin.

### Claim 8

A laminate comprising:
a retention film having a micro uneven structure with an unevenness period less than or equal to a wavelength of visible light;
an anti-reflection layer having a micro uneven structure in at least one surface, the micro uneven structure being formed after shape of the micro uneven structure of the retention film; and
a dye-containing resin layer formed on the anti-reflection layer.

### Claim 9 (depends on 1)