# US 2023/0407434 A1 · Methods and Systems for the Reduction of Rare Earth Metal Oxides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0407434 A1
- Document ID: US20230407434A1
- Status: Published application
- Kind: A1
- Application number: 18/210,366
- Filed: 2023-06-15
- Published: 2023-12-21
- Earliest claimed: 2022-06-15
- Assignees: SHINE Technologies, LLC
- Applicants: SHINE Technologies, LLC
- Inventors: Matthew Szymski; Marci Shelton; Eric Van Abel
- Web page: https://patentgrep.com/patent/US20230407434A1

## CPC

- C22B 5/16: with volatilisation or condensation of the metal being produced
- C22B 1/24: Binding; Briquetting {; Granulating}
- C22B 59/00: Obtaining rare earth metals
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

A method includes forming a powder mixture from a rare earth oxide powder and a lanthanum powder, heating the powder mixture in a crucible assembly positioned in a reduced pressure environment, wherein heating the powder mixture comprises applying heat using a heating element and heating the powder mixture reduces the rare earth oxide powder into a rare earth metal that collects on a collection region of the crucible assembly. The method also includes monitoring a pressure in the reduced pressure environment using a pressure sensor and reducing the heat applied by the heating element to the powder mixture when the pressure in the reduced pressure environment is above a threshold pressure.

## Claims

### Claim 1

A method comprising:
mixing a rare earth oxide powder and a lanthanum powder to form a powder mixture;
heating the powder mixture in a crucible assembly positioned in a reduced pressure environment, wherein:
heating the powder mixture comprises applying heat using a heating element; and
heating the powder mixture reduces the rare earth oxide powder into a rare earth metal that collects on a collection region of the crucible assembly;
monitoring a pressure in the reduced pressure environment using a pressure sensor; and
reducing the heat applied by the heating element to the powder mixture when the pressure in the reduced pressure environment is above a threshold pressure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the rare earth oxide powder comprises an ytterbium oxide powder or a gadolinium oxide powder and the rare earth metal comprises an ytterbium metal or a gadolinium metal.

### Claim 3 (depends on 1)

The method of claim 1, further comprising halting application of heat by the heating element to the powder mixture when the pressure in the reduced pressure environment is above the threshold pressure.

### Claim 4 (depends on 1)

The method of claim 1, further comprising resuming application of heat from the heating element to the powder mixture when the pressure of the reduced pressure environment is at or below the threshold pressure.

### Claim 5 (depends on 1)

The method of claim 1, wherein the powder mixture is a homogeneous mixture of rare earth oxide powder and lanthanum powder.

### Claim 6 (depends on 1)

The method of claim 1, wherein heating the powder mixture retains lanthanum in a reaction region of the crucible assembly.

### Claim 7 (depends on 1)

The method of claim 1, further comprising cooling the collection region of the crucible assembly while heating powder mixture to promote collection of the rare earth metal on the collection region.

### Claim 8 (depends on 1)

The method of claim 1, wherein the threshold pressure is in a range of from 1×10−6 torr to 1×10−2 torr.

### Claim 9 (depends on 1)

The method of claim 1, wherein when heating the powder mixture, the powder mixture is positioned in a reaction crucible of the crucible assembly, the crucible assembly further comprising:
a collection crucible, wherein the collection crucible is in the collection region of the crucible assembly;
a support sleeve; and
an insulative holder, wherein the collection crucible extends into a first end of the support sleeve and the reaction crucible extends into a first end of the insulative holder; and
the method further comprises, when heating the powder mixture, cooling the collection crucible.

### Claim 10 (depends on 1)

The method of claim 1, further comprising:
orienting a collection substrate to face the collection region of the crucible assembly holding the rare earth metal; and
sublimating the rare earth metal in an environment at a temperature in a range of from 400° C. to 3000° C. to transfer the rare earth metal from the collection region of the crucible assembly to a collection surface of the collection substrate, wherein the rare earth metal comprises an ytterbium metal.

### Claim 11 (depends on 1)

The method of claim 1, wherein the rare earth oxide powder comprises rare earth oxide particles comprising an average maximum cross-sectional dimension of 5 μm or less and a particle size distribution in which 90% or more of the rare earth oxide particles comprise a maximum cross-sectional dimension of 10 μm or less.

### Claim 12

A method comprising:
forming a powder mixture from a rare earth oxide powder and a lanthanum powder; wherein the rare earth oxide powder comprises rare earth oxide particles comprising an average maximum cross-sectional dimension of 5 μm or less and a particle size distribution in which 90% or more of the rare earth oxide particles comprise a maximum cross-sectional dimension of 10 μm or less;
agitating the powder mixture to increase a distribution uniformity of the rare earth oxide powder and the lanthanum powder in the powder mixture; and
heating the powder mixture in a crucible assembly positioned in a reduced pressure environment, wherein heating the powder mixture reduces the rare earth oxide powder into a rare earth metal that collects on a collection region of the crucible assembly.

### Claim 13 (depends on 12)

The method of claim 12, wherein, subsequent to agitating the powder mixture, the powder mixture comprises a homogeneous mixture of the rare earth oxide powder and the lanthanum powder.

### Claim 14 (depends on 12)

The method of claim 12, wherein the rare earth oxide particles comprise an average maximum cross-sectional dimension in a range of 1 μm to 3 μm.

### Claim 15 (depends on 12)

The method of claim 12, wherein the lanthanum powder comprises lanthanum particles comprising an average maximum cross-sectional dimension of 90 μm or less

### Claim 16 (depends on 12)

The method of claim 12, further comprising, prior to agitating the powder mixture, positioning the powder mixture in a reaction crucible of the crucible assembly such that the powder mixture is agitated in the reaction crucible, and subsequent to agitating the powder mixture, packing the powder mixture to increase a density of the powder mixture in the reaction crucible.

### Claim 17 (depends on 12)

The method of claim 12, further comprising, prior to forming the powder mixture, milling the rare earth oxide powder to increase a sphericity the rare earth oxide particles of the rare earth oxide powder.

### Claim 18 (depends on 17)

The method of claim 17, wherein, subsequent to milling the rare earth oxide powder, the ratio of the maximum cross-sectional dimension to the minimum cross-sectional dimension of 90% of more of the rare earth oxide particles of the rare earth oxide powder is 2:1 or less

### Claim 19 (depends on 12)

The method of claim 12, wherein the ratio of the maximum cross-sectional dimension to the minimum cross-sectional dimension of 90% of more of the rare earth oxide particles of the rare earth oxide powder is 2:1 or less.

### Claim 20 (depends on 12)

The method of claim 12, wherein the rare earth oxide powder comprises an ytterbium oxide powder or a gadolinium oxide powder and the rare earth metal comprises an ytterbium metal or a gadolinium metal.