# US 2023/0407433 A1 · Wire rod and steel wire for springs having excellent corrosion fatigue resistance properties, and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0407433 A1
- Document ID: US20230407433A1
- Status: Published application
- Kind: A1
- Application number: 18/240,081
- Filed: 2023-08-30
- Published: 2023-12-21
- Earliest claimed: 2017-09-29
- Assignees: Posco
- Applicants: Posco Co., Ltd
- Inventors: Kwan-Ho Kim
- Web page: https://patentgrep.com/patent/US20230407433A1

## CPC

- C21D 9/525: {for wire, for rods (C21D9/54 takes precedence)}
- C21D 3/04: Decarburising
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/06: during manufacturing of rods or wires
- C21D 9/52: for wires; for strips {; for rods of unlimited length}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C21D 2211/001: Austenite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/18: containing chromium
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

An embodiment of the present invention provides a wire rod and a steel wire which are for springs and have excellent corrosion fatigue resistance properties, and a method for producing same, the wire rod and steel wire containing, in wt %, 0.40-0.70% of C, 1.20-2.30% of Si, 0.20-0.80% of Mn, 0.20-0.80% of Cr, 0.015% or less of P, 0.015% or less of S, and 0.010% or less of N, with the remainder comprising Fe and other unavoidable impurities, along with at least one among 0.01-0.20% of V and 0.01-0.10% of Nb, wherein the V and Nb satisfy relational expression 1 below, the average grain size of prior austenite is no greater than 20 μm, and the surface decarburization depth is no greater than 0.1 mm. [Relational expression 1] [V]+[Nb]≥0.08 (where the V and Nb contents are in wt %)

## Claims

### Claim 1

A method for producing a wire rod for a spring having an excellent corrosion fatigue resistance property, the method comprising:
heating, at 900 to 1050° C., a billet containing, by wt %, C: 0.40 to 0.70%, Si: 1.20 to 2.30%, Mn: 0.20 to 0.80%, Cr: 0.20 to 0.80%, P: 0.015% or less, S: 0.015% or less, N: 0.010% or less, and a balance of Fe and other unavoidable impurities, and further containing one or two of V: 0.01 to 0.20% and Nb: 0.01 to 0.10%, V and Nb satisfying the following Relational Expression 1;
finishing rolling and winding the heated billet at 800 to 1000° C. to obtain a wound coil; and
performing primary cooling on the wound coil at a cooling rate of 2.0 to 10° C./s up to Ar1-40° C. and performing secondary cooling on the wound coil at a cooling rate of 0.3 to 1.8° C./s in a temperature range of (Ar1-40° C.) to (Ar1-140° C.),
[V]+[Nb]≥0.08 (where, a content of each of V and Nb refers to wt %). [Relational Expression 1]

### Claim 2 (depends on 1)

The method of claim 1, wherein the billet further contains one or two of Ti: 0.01 to 0.15% and Mo: 0.01 to 0.40%.

### Claim 3 (depends on 1)

The method of claim 1, wherein the billet further contains one or two of Cu: 0.01 to 0.40% and Ni: 0.10 to 0.60%.

### Claim 4

A method for producing a steel wire for a spring having an excellent corrosion fatigue resistance property, the method comprising:
heating, at 900 to 1050° C., a billet containing, by wt %, C: 0.40 to 0.70%, Si: 1.20 to 2.30%, Mn: 0.20 to 0.80%, Cr: 0.20 to 0.80%, P: 0.015% or less, S: 0.015% or less, N: 0.010% or less, and a balance of Fe and other unavoidable impurities, and further containing one or two of V: 0.01 to 0.20% and Nb: 0.01 to 0.10%, V and Nb satisfying the following Relational Expression 1;
finishing rolling and winding the heated billet at 800 to 1000° C. to obtain a wound coil;
performing primary cooling on the wound coil at a cooling rate of 2.0 to 10° C./s up to Ar1-40° C. and performing secondary cooling on the wound coil at a cooling rate of 0.3 to 1.8° C./s in a temperature range of (Ar1-40° C.) to (Ar1-140° C.);
drawing the steel wire subjected to the primary and secondary cooling to obtain a steel wire;
heating the steel wire at 850 to 1000° C. and holding the steel wire for 1 to 300 seconds;
oil-cooling the heated and held steel wire up to 25 to 80° C.; and
tempering the oil-cooled steel wire at 350 to 500° C.,
[V]+[Nb]≥0.08 (where, a content of each of V and Nb refers to wt %). [Relational Expression 1]

### Claim 5 (depends on 4)

The method of claim 4, wherein the billet further contains one or two of Ti: 0.01 to 0.15% and Mo: 0.01 to 0.40%.

### Claim 6 (depends on 4)

The method of claim 4, wherein the billet further contains one or two of Cu: 0.01 to 0.40% and Ni: 0.10 to 0.60%.