# US 2023/0407248 A1 · Methods of increasing growth of corals using a bioceramic

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0407248 A1
- Document ID: US20230407248A1
- Status: Published application
- Kind: A1
- Application number: 18/332,823
- Filed: 2023-06-12
- Published: 2023-12-21
- Earliest claimed: 2022-06-10
- Assignees: Novum Coral, Inc.
- Applicants: Novum Coral, Inc.
- Inventors: Michael A. DAVITZ; William SHEEHAN; Lawrence A. SHIMP; Onno VISSER
- Web page: https://patentgrep.com/patent/US20230407248A1

## CPC

- C12N 5/0601: {Invertebrate cells or tissues, e.g. insect cells; Culture media therefor}
- C12N 2500/05: Inorganic components
- C12N 2500/14: Calcium; Ca chelators; Calcitonin
- C12N 2533/14: Ceramic
- C12N: MICROORGANISMS OR ENZYMES; COMPOSITIONS THEREOF; PROPAGATING, PRESERVING, OR MAINTAINING MICROORGANISMS; MUTATION OR GENETIC ENGINEERING; CULTURE MEDIA (microbiological testing media C12Q1/00)

## Abstract

The present disclosure is directed to a method of increasing growth of coral by growing the coral on a bioceramic hydroxyapatite material. An increased growth rate in the coral species is observed with respect to perimeter, surface area and volume as compared with the growth rate on a control material. In some embodiments, the bioceramic hydroxyapatite material contains a carbonatable calcium component with a Ca/P ratio greater than about 1.67.

## Claims

### Claim 1

A method of increasing growth rate of a coral species, comprising growing the coral species on a bioceramic hydroxyapatite material for a period of time, t.

### Claim 2 (depends on 1)

The method of claim 1, wherein growth rate is measured by an increase in the perimeter of the coral species.

### Claim 3 (depends on 1)

The method of claim 1, wherein growth rate is measured by an increase in surface area of the coral species.

### Claim 4 (depends on 1)

The method of claim 1, wherein growth rate is measured by an increase in volume of the coral species.

### Claim 5 (depends on 1)

The method of claim 1, wherein the period of time, t, ranges from about 1 month to 1 about year.

### Claim 6 (depends on 1)

The method of claim 1, wherein the growth rate of the coral species on the bioceramic hydroxyapatite material increases from about 10% to about 100% when compared to growth on a control material.

### Claim 7 (depends on 6)

The method of claim 6, wherein the control material is fired clay.

### Claim 8 (depends on 2)

The method of claim 2, wherein increase of the perimeter of the coral species ranges from about 0.1 cm/month to 10 cm/month.

### Claim 9 (depends on 8)

The method of claim 8, wherein increase of the surface area of the coral species is in the range of from 0.5 cm2/month to 50 cm2/month.

### Claim 10 (depends on 4)

The method of claim 4, wherein the increase of the volume of the coral species ranges from about 0.25 cm3/month to 20 cm3/month.

### Claim 11 (depends on 1)

The method of claim 1, wherein the increase in growth rate is measured by an increase in amount (% W) of aragonite in the bioceramic hydroxyapatite material attached to the coral species.

### Claim 12 (depends on 1)

The method of claim 1, wherein the coral species comprises stoney corals, Hexacorallia, and soft corals, Octocorallia.

### Claim 13 (depends on 12)

The method of claim 12, wherein the coral species comprises stoney corals, Hexacorallia

### Claim 14 (depends on 1)

The method of claim 1, wherein the bioceramic hydroxyapatite comprises Ca10(PO4)6OH2.

### Claim 15 (depends on 1)

The method of claim 1, wherein the bioceramic hydroxyapatite comprises a hydroxyapatite material comprising a carbonatable calcium component, said carbonatable calcium component providing said hydroxyapatite material a Ca/P ratio greater than about 1.67.