# US 2023/0407143 A1 · Method for producing composite resin particle dispersion, method for producing pressure-sensitive adhesive, method for producing pressure-responsive resin, method for producing toner for electrostatic charge image development, and composite resin particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0407143 A1
- Document ID: US20230407143A1
- Status: Published application
- Kind: A1
- Application number: 18/240,989
- Filed: 2023-08-31
- Published: 2023-12-21
- Earliest claimed: 2021-03-24
- Assignees: FUJIFILM Business Innovation Corp.
- Applicants: FUJIFILM Business Innovation Corp.
- Inventors: Sumiaki YAMASAKI; Takahiro ISHIZUKA; Kiyohiro YAMANAKA; Yasunobu KASHIMA; Satoshi INOUE
- Web page: https://patentgrep.com/patent/US20230407143A1

## CPC

- C09D 11/106: containing macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds
- C09J 7/38: Pressure-sensitive adhesives [PSA]
- C08F 2/22: Emulsion polymerisation
- C08F 212/08: Styrene
- C08F 220/1804: {C4-(meth)acrylate, e.g. butyl (meth)acrylate, isobutyl (meth)acrylate or tert-butyl (meth)acrylate}
- C08F 220/1808: {C8-(meth)acrylate, e.g. isooctyl (meth)acrylate or 2-ethylhexyl (meth)acrylate}
- C08F 257/02: on to polymers of styrene or alkyl-substituted styrenes
- C08F 285/00: Macromolecular compounds obtained by polymerising monomers on to preformed graft polymers
- C09D 11/02: Printing inks (C09D11/30 takes precedence)
- C09D 11/107: from unsaturated acids or derivatives thereof
- C09D 151/003: {grafted on to macromolecular compounds obtained by reactions only involving unsaturated carbon-to-carbon bonds (C09D151/04, C09D151/06 take precedence)}
- C09J 151/003: {grafted on to macromolecular compounds obtained by reactions only involving unsaturated carbon-to-carbon bonds (C09J151/04, C09J151/06 take precedence)}
- G03G 9/0804: {whereby the components are brought together in a liquid dispersing medium}
- G03G 9/0823: {Electric parameters}
- G03G 9/08711: {with esters of acrylic or methacrylic acid}
- G03G 9/08795: {characterised by their chemical properties, e.g. acidity, molecular weight, sensitivity to reactants}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- C08L 25/14: with unsaturated esters
- C09J 2301/302: the adhesive being pressure-sensitive, i.e. tacky at temperatures inferior to 30°C
- C09J 2301/312: parameters being the characterizing feature
- C09J 2425/00: Presence of styrenic polymer
- C09J 2433/00: Presence of (meth)acrylic polymer
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A method for producing a composite resin particle dispersion includes: performing polymerization A by polymerizing a styrene compound and a vinyl monomer other than the styrene compound to form a styrene-based resin; performing polymerization B by polymerizing a (meth)acrylic acid ester compound in the presence of the styrene-based resin to form intermediate resin particles containing the styrene-based resin and a (meth)acrylic acid ester-based resin; and performing polymerization C by polymerizing a styrene compound and a vinyl monomer other than the styrene compound in the presence of the intermediate resin particles to form composite resin particles. The mass ratio of the styrene-based resin to the (meth)acrylic acid ester-based resin in the composite resin particles is from 80:20 to 20:80. A difference between the lowest glass transition temperature and the highest glass transition temperature in the composite resin particles is 30° C. or more.

## Claims

### Claim 1

A method for producing a toner for electrostatic charge image development containing a resin formed by aggregation and coalescence of composite resin particles contained in a composite resin particle dispersion,
wherein the composite resin particle dispersion is produced by the method comprising:
performing polymerization A by polymerizing a styrene compound and a vinyl monomer other than the styrene compound to form a styrene-based resin;
performing polymerization B by polymerizing a (meth)acrylic acid ester compound in the presence of the styrene-based resin to form intermediate resin particles containing the styrene-based resin and a (meth)acrylic acid ester-based resin; and
performing polymerization C by polymerizing a styrene compound and a vinyl monomer other than the styrene compound in the presence of the intermediate resin particles to form composite resin particles,
wherein a mass ratio of the styrene-based resin to the (meth)acrylic acid ester-based resin in the composite resin particles is from 80:20 to 20:80, and
a difference between the lowest glass transition temperature of the (meth)acrylic acid ester-based resin contained in the composite resin particles and the highest glass transition temperature of the styrene-based resin contained in the composite resin particles in the composite resin particles is 30° C. or more.

### Claim 2 (depends on 1)

The method for producing a toner for electrostatic charge image development according to claim 1, wherein a mass ratio of a total amount of the styrene compound and the vinyl monomer other than the styrene compound added in the polymerization C to an amount of the (meth)acrylic acid ester-based resin contained in the intermediate resin particles is from 5:95 to 40:60.

### Claim 3 (depends on 1)

The method for producing a toner for electrostatic charge image development according to claim 1, wherein the styrene compounds used in the polymerization A and the polymerization C are styrene.

### Claim 4 (depends on 3)

The method for producing a toner for electrostatic charge image development according to claim 3, wherein a mass percentage of the styrene relative to a total mass of polymer components of the styrene-based resin in the composite resin particles is 60 mass % or more and 95 mass % or less

### Claim 5 (depends on 1)

The method for producing a toner for electrostatic charge image development according to claim 1, wherein the vinyl monomer used in the polymerization A and the vinyl monomer used in the polymerization C include a (meth)acrylic acid ester compound.

### Claim 6 (depends on 1)

The method for producing a toner for electrostatic charge image development according to claim 1, wherein the (meth)acrylic acid ester compound used in the polymerization B includes at least two (meth)acrylic acid ester compounds.

### Claim 7 (depends on 6)

The method for producing a toner for electrostatic charge image development according to claim 6, wherein the (meth)acrylic acid ester compound used in the polymerization B includes 2-ethylhexyl acrylate and n-butyl acrylate.

### Claim 8 (depends on 1)

The method for producing a toner for electrostatic charge image development according to claim 1, wherein a mass percentage of the (meth)acrylic acid ester compound relative to a total mass of polymer components of the (meth)acrylic acid ester-based resin contained in the composite resin particles is 90 mass % or more.

### Claim 9 (depends on 1)

The method for producing a toner for electrostatic charge image development according to claim 1, wherein the (meth)acrylic acid ester-based resin contained in the composite resin particles has a glass transition temperature of −30° C. or lower.

### Claim 10 (depends on 1)

The method for producing a toner for electrostatic charge image development according to claim 1, wherein the styrene-based resin contained in the composite resin particles has a glass transition temperature of 30° C. or higher.

### Claim 11 (depends on 1)

The method for producing a toner for electrostatic charge image development according to claim 1, wherein the styrene-based resin synthesized in the polymerization step C and the (meth)acrylic acid ester-based resin synthesized in the polymerization step B each have a structural unit derived from the same (meth)acrylic acid ester compound.

### Claim 12 (depends on 1)

The method for producing a toner for electrostatic charge image development according to claim 1, wherein the styrene-based resin synthesized in the polymerization step A contain at least one of n-butyl acrylate or 2-ethylhexyl acrylate as a polymer component.

### Claim 13 (depends on 12)

The method for producing a toner for electrostatic charge image development according to claim 12, wherein the total amount of the n-butyl acrylate and the 2-ethylhexyl acrylate relative to a total amount of the polymer components of the styrene-based resin synthesized in the polymerization step A is 30 mass % to 10 mass %.

### Claim 14 (depends on 11)

The method for producing a toner for electrostatic charge image development according to claim 11, wherein the styrene-based resin synthesized in the polymerization step A, the (meth)acrylic acid ester-based resin synthesized in the polymerization step B, and the styrene-based resin synthesized in the polymerization step C have a structural unit derived from the same (meth)acrylic acid ester compound.

### Claim 15

A method for producing a toner for electrostatic charge image development containing a resin formed by aggregation and coalescence of composite resin particles contained in a composite resin particle dispersion,
wherein the composite resin particle dispersion produced by the method comprising:
performing polymerization A by polymerizing a styrene compound and a vinyl monomer other than the styrene compound to form a styrene-based resin;
performing polymerization B by polymerizing a (meth)acrylic acid ester compound in the presence of the styrene-based resin to form intermediate resin particles containing the styrene-based resin and a (meth)acrylic acid ester-based resin; and
performing polymerization C by polymerizing a styrene compound and a vinyl monomer other than the styrene compound in the presence of the intermediate resin particles to form composite resin particles,
wherein a mass ratio of the styrene-based resin to the (meth)acrylic acid ester-based resin in the composite resin particles is from 80:20 to 20:80, and
a difference between the lowest glass transition temperature of the (meth)acrylic acid ester-based resin contained in the composite resin particles and the highest glass transition temperature of the styrene-based resin contained in the composite resin particles in the composite resin particles is 30° C. or more,
the styrene-based resin synthesized in the polymerization step A contain at least one of n-butyl acrylate or 2-ethylhexyl acrylate as a polymer component, and a total amount of the n-butyl acrylate and the 2-ethylhexyl acrylate relative to a total amount of the polymer components of the styrene-based resin synthesized in the polymerization step A is 30 mass % to 10 mass %, and the styrene-based resin synthesized in the polymerization step A, the (meth)acrylic acid ester-based resin synthesized in the polymerization step B, and the styrene-based resin synthesized in the polymerization step C have a structural unit derived from the same (meth)acrylic acid ester compound.