# US 2023/0407069 A1 · Low-smoke self-extinguishing electrical cable and flame-retardant composition used therein

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0407069 A1
- Document ID: US20230407069A1
- Status: Published application
- Kind: A1
- Application number: 18/253,972
- Filed: 2021-11-16
- Published: 2023-12-21
- Earliest claimed: 2020-11-26
- Assignees: Basell Polyolefine GmbH
- Applicants: Basell Polyolefine GmbH
- Inventors: Christof Justus; Alexander Rodionov; Alexander Kulichenko; Cristinel Degeratu
- Web page: https://patentgrep.com/patent/US20230407069A1

## CPC

- C08L 23/0869: with unsaturated acids, e.g. [meth]acrylic acid; with unsaturated esters, e.g. [meth]acrylic acid esters
- C08K 3/22: of metals
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 33/08: Homopolymers or copolymers of acrylic acid esters
- C08L 51/003: {grafted on to macromolecular compounds obtained by reactions only involving unsaturated carbon-to-carbon bonds (C08L51/04, C08L51/06 take precedence)}
- H01B 3/441: {from alkenes}
- H01B 3/447: {from acrylic compounds}
- H01B 7/295: using material resistant to flame
- C08K 2003/2224: {Magnesium hydroxide}
- C08L 2203/202: use in electrical wires or wirecoating
- H01B 3/28: natural or synthetic rubbers
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

A thermoplastic composition made from or containing (i) a polyolefin portion made from or containing (a) an ethylene/alkyl acrylate, (b) a polyolefin elastomer selected from copolymers of ethylene with a C3-C15 alpha-olefin, and optionally with a diene, having a density of from 0.860 to g/cm3, (c) an ethylene polymer grafted with carboxyl groups or organic silane groups, and optionally (d) a copolymer of ethylene with a C4-C10 alpha-olefin, having a density of from 0.910 to g/cm3, and (ii) a mineral portion made from or containing (e) magnesium hydroxide, wherein the components (a)-(e) being present in amount such that the weight ratio (e)/polyolefin portion ranges from 0.8:1 to 1.75:1, the weight ratio (a)/(b) ranges from 0.75:1 to 1.25:1, and the weight ratio (a)/(e) ranges from 0.15:1 to 0.4:1; and wherein the thermoplastic composition has a melt flow rate of at least 2 g/10 min.

## Claims

### Claim 1

A thermoplastic composition for electrical cable coating comprising:
(i) a polyolefin portion comprising
(a) an ethylene copolymer being an ethylene/alkyl acrylate,
(b) a polyolefin elastomer (POE) being selected from copolymers of ethylene with a C3-C15 alpha-olefin, and optionally with a diene, having a density (ASTM D505) of from 0.860 to 0.904 g/cm3,
(c) a polymeric coupling agent selected from ethylene polymers grafted with carboxyl groups or organic silane groups, and optionally
(d) a copolymer of ethylene with a C4-C10 alpha-olefin, having a density of from 0.910 to 0.924 g/cm3, and
(ii) a mineral portion comprising
(e) magnesium hydroxide, said
wherein the components (a)-(e) being present in amount such that the weight ratio (e)/polyolefin portion ranges from 0.8:1 to 1.75:1, the weight ratio (a)/(b) ranges from 0.75:1 to 1.25:1, and the weight ratio (a)/(e) ranges from 0.15:1 to 0.4:1; and
wherein the thermoplastic composition having a melt flow rate (MFR) at 190° C. with a load of 21.6 kg, according to ISO 1133-2:2011, of at least 2 g/10 min.

### Claim 2 (depends on 1)

The thermoplastic composition of claim 1, wherein the ethylene copolymer (a) is selected from the group consisting of ethylene/butyl acrylate (EBA), ethylene/ethyl acrylate (EEA), and ethylene/methyl acrylate (EMA).

### Claim 3 (depends on 2)

The thermoplastic composition according to claim 2, wherein the ethylene copolymer (a) has the alkyl acrylate content ranging from 10 to 20 wt %, a MFR ranging from 0.5 to 25 g/10 min, and a density ranging from 0.920 to g/cm3.

### Claim 4 (depends on 1)

The thermoplastic composition according to claim 1, wherein the C3-C15 alpha-olefin of the polyolefin elastomer (b) is a C4-C12 alpha-olefin in an amount ranging from 3-25% by mole.

### Claim 5 (depends on 4)

The thermoplastic composition according to claim 4, wherein the polyolefin elastomer (b) has a density ranging from 0.870 and 0.90 g/cm3 and a MFR at 190° C. with a load of 2.16 kg, according to ISO 1133-2:2011, ranging from 0.1 to 30 g/10 min.

### Claim 6 (depends on 1)

The thermoplastic composition according to claim 1, wherein the polymer coupling agent (c) is a maleic anhydride grafted polyethylene (MAHg-PE), having the content of grafted organo-functional group in the range of −0.05 to 10 weight percent based on the weight of the resin.

### Claim 7 (depends on 1)

The thermoplastic composition according to claim 1 further comprising component the ethylene copolymer (d), having a density of from 0.912 to 0.922 g/cm3.

### Claim 8 (depends on 7)

The thermoplastic composition according to claim 7, wherein the alpha-olefin of the ethylene copolymer (d) is selected from the group consisting of 1-butene, 1-hexene, and 1-octene, and present in the copolymer in an amount of from 1 to 12% by moles, and wherein the ethylene copolymer (d) having a melt flow rate (MFR) at 190° C. with a load of 2.16 kg, according to ISO 1133-2:2011, ranging from 0.5 to 20 g/10 min.

### Claim 9 (depends on 1)

The thermoplastic composition according to claim 1 wherein the magnesium hydroxide (e) is selected from the group consisting of natural magnesium hydroxide and surface treated magnesium hydroxide, having a specific surface area of the ground product ranging from 5 and 20 m2/g and an average particle diameter of between 1 and 15 um.

### Claim 10 (depends on 9)

The thermoplastic composition according to claim 9, wherein the surface treated magnesium hydroxide is obtained by treating natural magnesium hydroxide with organic silanes.

### Claim 11 (depends on 1)

The thermoplastic composition according to claim 1 wherein the components (a) to (e) are present in amount such that the weight ratio (e)/polyolefin portion ranges from 1:1 to 1.65:1, the weight ratio (a)/(b) ranges from 0.85:1 to 1.15:1, and the weight ratio (a)/(e) ranges from 0.25:1 to 0.35:1.

### Claim 12 (depends on 11)

The thermoplastic composition according to claim 11, having the following composition (phr):
Ethylene copolymer (a) from 25 to 60;
Polyolefin elastomer (b) from 25 to 60;
Polymeric coupling agent (c) from 5 to 20;
Ethylene copolymer (d) from 5 to 20; and
Magnesium hydroxide (e) from 120 to 180.

### Claim 13 (depends on 12)

The composition of claim 12 further comprising 1 to 10 phr of an additive package comprising one or more of components selected from antioxidants, processing coadjuvants, lubricants, pigments, and other fillers.

### Claim 14 (depends on 1)

The thermoplastic composition according to claim 1, having a melt flow rate (MFR) at 190° C. with a load of 21.6 kg, according to ISO 1133-2:2011, of at least 2.5 g/10 min.

### Claim 15 (depends on 1)

An electrical cable coated with the thermoplastic composition according to claim 1.

### Claim 16 (depends on 2)

The thermoplastic composition of claim 2, wherein the content of alkyl acrylate ranges from 5 to 25 wt %, based upon the total weight of the ethylene copolymer (a).