# US 2023/0407061 A1 · Method for manufacturing asphalt comprising rubber from end-of-life tires

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0407061 A1
- Document ID: US20230407061A1
- Status: Published application
- Kind: A1
- Application number: 18/035,677
- Filed: 2021-11-05
- Published: 2023-12-21
- Earliest claimed: 2020-11-06
- Assignees: Bridgestone Europe NV/SA
- Applicants: Bridgestone Europe NV/SA [BE/BE]
- Inventors: Luca Lelio; Massimo Losa; Pietro Leandri
- Web page: https://patentgrep.com/patent/US20230407061A1

## CPC

- C08L 17/00: Compositions of reclaimed rubber
- B09B 3/40: involving thermal treatment, e.g. evaporation (processes using mineral binders involving a melting or softening step B09B3/29; involving radiation B09B3/50)
- C04B 18/22: Rubber {, e.g. ground waste tires}
- C04B 26/26: Bituminous materials, e.g. tar, pitch {(C08L95/00 takes precedence)}
- C08K 7/26: Silicon- containing compounds
- C10B 53/07: {of solid raw materials consisting} of synthetic polymeric materials, e.g. tyres (recovery or working-up of waste materials of organic macromolecular compounds or compositions based thereon by dry-heat treatment for obtaining partially depolymerised materials C08J11/10; production of liquid hydrocarbon mixtures from rubber or rubber waste C10G1/10)
- C10C 3/002: {by thermal means}
- C10C 3/005: {by mixing several fractions (also coaltar fractions with petroleum fractions)}
- B09B 2101/80: Rubber waste, e.g. scrap tyres
- C08L 2207/24: recycling of old tyres and caoutchouc and addition of caoutchouc particles
- Y02P 20/143: the feedstock being recycled material, e.g. plastics
- Y02W 30/62: Plastics recycling; Rubber recycling
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B09B: DISPOSAL OF SOLID WASTE NOT OTHERWISE PROVIDED FOR
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C10B: DESTRUCTIVE DISTILLATION OF CARBONACEOUS MATERIALS FOR PRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS (cracking oils C10G; underground gasification of minerals E21B43/295)
- C10C: WORKING-UP PITCH, ASPHALT, BITUMEN, TAR; PYROLIGNEOUS ACID (compositions of bituminous materials C08L95/00; carbon filaments by decomposition of organic filaments D01F9/14)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method for producing asphalt comprising a heat treatment step, wherein the rubber granules deriving from an end-of-life tyre granulation process are subjected to a temperature of between 80 and 300° C., for a period of time necessary in order to obtain rubber granules with a density of between 1.0 and 1.5 g/cm3; and a mixing step wherein the rubber granules from the heat treatment step are mixed with stone aggregate and bitumen in order to obtain asphalt.

## Claims

### Claim at position 1

1-16. (canceled)

### Claim 17

A method for producing asphalt comprising:
a heat treatment step, wherein first rubber granules deriving from an end-of-life tire granulation process are subjected to a temperature of between 80 and 300° C., for a period of time such that second rubber granules are obtained with a density of between 1.0 and 1.5 g/cm3; and
a mixing step wherein the second rubber granules are mixed with stone aggregate and bitumen to obtain asphalt.

### Claim 18 (depends on 17)

The method of claim 17, wherein during the heat treatment step the first rubber granules are subjected to a temperature of between 100 and 200° C., for a period of time such that the second rubber granules are obtained with a density of between 1.2 and 1.3 g/cm3.

### Claim 19 (depends on 17)

The method of claim 17, wherein the mixing step comprises a first mixing operation wherein the stone aggregate and the bitumen are mixed together at a temperature of between 150 and 200° C., and a second mixing operation wherein the second rubber granules are added to the mixture from the first mixing operation.

### Claim 20 (depends on 17)

The method of claim 17, wherein the second rubber granules constitute from 1 to 30% by volume of a quantity of inert material comprised within the asphalt.

### Claim 21 (depends on 17)

The method of claim 17, wherein the first rubber granules have a substantially polyhedral conformation, wherein a ratio between a maximum size and a minimum size thereof is less than 2.

### Claim 22 (depends on 17)

The method of claim 17, wherein the first rubber granules have dimensions to pass through a sieve having meshes with dimensions of between 10 mm and 1.5 mm.

### Claim 23 (depends on 17)

The method of claim 17, wherein the first rubber granules have dimensions to pass through a sieve having meshes with dimensions of between 2.0 mm and 6.0 mm.

### Claim 24 (depends on 17)

The method of claim 17, comprising a preliminary thermal step preceding the heat treatment step, wherein rubber granules are subjected to a temperature of between 120 and 200° C. for a period of time of between 15 and 30 h.

### Claim 25 (depends on 17)

The method of claim 17, comprising a surface treatment step, subsequent to the heat treatment step and wherein the second rubber granules from the heat treatment step are subjected to a surface abrasion operation.

### Claim 26 (depends on 25)

The method of claim 25, comprising a final heat treatment step subsequent to the surface treatment step and preceding the mixing step, wherein during the final heat treatment step the rubber granules deriving from the surface treatment step are subjected to a temperature of between 80 and 300° C. for a period of time to obtain rubber granules with a density of between 1.0 and 1.5 g/cm3.

### Claim 27 (depends on 26)

The method of claim 26, wherein during the final heat treatment step the rubber granules deriving from the surface treatment step are subjected to a temperature of between 100 and 200° C. for a period of time to obtain rubber granules with a density of between 1.2 and 1.3 g/cm3.

### Claim 28 (depends on 16)

Asphalt manufactured using the method of claim 16.

### Claim 29

Rubber granules and/or powder deriving from an end-of-life tire granulation process, which have dimensions to pass through a sieve having meshes with dimensions up to 10 mm and that are subjected during a heat treatment step to a temperature of between and 300° C. for a period of time to obtain rubber granules and/or powder with a density of between 1.0 and 1.5 g/cm3.

### Claim 30 (depends on 29)

The rubber granules and/or powder of claim 29, further subjected to a preliminary thermal step, preceding the heat treatment step, and wherein the rubber granules and/or powder deriving from the granulation process are subjected to a temperature of between 120 and 200° C. for a period of time of between 15 and 30 h.

### Claim 31 (depends on 29)

The rubber granules and/or powder of claim 29, further subjected to a surface treatment step, subsequent to the heat treatment step, and wherein the rubber granules and/or powder from the heat treatment step are subjected to a surface abrasion operation.

### Claim 32 (depends on 31)

The rubber granules and/or powder of claim 31, further subjected to a final heat treatment step subsequent to the surface treatment step, wherein during the final heat treatment step the rubber granules and/or powder deriving from the surface treatment step are subjected to a temperature of between 80 and 300° C. for a period of time to obtain rubber granules and/or powder with a density of between 1.0 and 1.5 g/cm3.