# US 2023/0407002 A1 · Molded articles for use with terpene containing oils

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0407002 A1
- Document ID: US20230407002A1
- Status: Published application
- Kind: A1
- Application number: 18/251,549
- Filed: 2021-11-09
- Published: 2023-12-21
- Earliest claimed: 2020-11-17
- Assignees: Eastman Chemical Company
- Applicants: Eastman Chemical Campany
- Inventors: Steven Lee Stafford; Bryan Steven Bishop; Kathleen Jean White; Mason Scott Myers
- Web page: https://patentgrep.com/patent/US20230407002A1

## CPC

- C08G 63/199: Acids or hydroxy compounds containing cycloaliphatic rings
- C08G 2250/00: Compositions for preparing crystalline polymers
- C08G 2390/00: Containers
- Y02P 20/582: Recycling of unreacted starting or intermediate materials
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A shaped article comprising a molded component configured to receive a terpene containing oil composition, said molded component formed of a copolyester composition having high chemical resistance to terpene oil and having a Tg of at least 95° C.

## Claims

### Claim 1

An article comprising a molded component configured to receive a terpene containing oil composition, said molded component formed of a copolyester composition comprising at least one copolyester that comprises:
(a) a dicarboxylic acid component comprising:
i) 70 to 100 mole % of terephthalic acid residues;
(b) a glycol component comprising:
i) 5 to 15 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; and
ii) 85 to 95 mole % of 1,4-cyclohexanedimethanol residues,
wherein the total mole % of the dicarboxylic acid component is 100 mole %, and the total mole % of the glycol component is 100 mole %; and wherein the inherent viscosity is 0.60 to 1.2 dL/g as determined in 60/40 (wt/wt) phenol/tetrachloroethane at a concentration of 0.5 g/100 ml at 25° C.; and wherein the polyester has a Tg of 95° C. to 115° C.

### Claim 2 (depends on 1)

The article according to claim 1, wherein the copolyester composition has a Tg in the range from 100° C. to 115° C.

### Claim 3 (depends on 2)

The article according to claim 2, wherein the copolyester composition has an inherent viscosity is 0.70 to 1.0 dL/g, 0.75 to 0.95 dL/g.

### Claim 4 (depends on 1)

The article according to claim 1, wherein the glycol component comprises:
i) 9 to 13 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; and
ii) 87 to 91 mole % of 1,4-cyclohexanedimethanol residues.

### Claim 5 (depends on 1)

The article according to claim 1, wherein the dicarboxylic acid component comprises 100 mole % terephthalic acid residues.

### Claim 6 (depends on 1)

The article according to claim 1, wherein the dicarboxylic acid component comprises:
i) 95 to 100 mole % of terephthalic acid residues; and
0 to 5 mole % of isophthalic acid residues.

### Claim 7 (depends on 1)

The article according to claim 1, wherein the copolyester composition has a crystallization half time from 30 seconds to 5 minutes.

### Claim 8 (depends on 1)

The article according to claim 1, comprising a terpene containing oil composition in contact with a surface of said molded component, wherein the terpene containing oil composition is in the form of a pre-vapor formulation and/or a vapor.

### Claim 9 (depends on 1)

The article according to claim 1, wherein the terpene containing oil composition comprises at least 1 wt % of a terpene containing oil.

### Claim 10 (depends on 1)

The article according to claim 1, wherein the molded component comprises a container configured to contain a terpene containing oil composition and selectively release the terpene containing oil composition.

### Claim 11 (depends on 10)

The article according to claim 10, wherein the molded component comprises a container configured to contain a terpene containing oil composition that is in a pre-vapor formulation form.

### Claim 12 (depends on 1)

The article according to claim 1, wherein the molded component comprises a conduit configured to convey a terpene containing oil composition.

### Claim 13 (depends on 12)

The article according to claim 12, wherein the molded component comprises a conduit configured to convey a terpene containing oil composition that is in a vapor form.

### Claim 14 (depends on 10)

The article according to claim 10, wherein the article comprises one or more molded components that comprise a container configured to contain a terpene containing oil composition and a conduit configured to convey a terpene containing oil composition, wherein the container and conduit are in fluid communication.

### Claim 15 (depends on 1)

The article according to claim 1, wherein the article is a vapor delivery device configured to deliver a vapor comprising a terpene containing oil composition.

### Claim 16 (depends on 15)

The article according to claim 15, wherein the vapor delivery device is chosen from a vaporizer, nebulizer, humidifier, air freshener, or hand-held vapor delivery device.

### Claim 17 (depends on 1)

The article according to claim 1, wherein the molded component can be chosen from injection molded articles, extrusion molded articles, rotational molded articles, compression molded articles, blow molded articles, injection blow molded articles, injection stretch blow molded articles, extrusion blow molded articles, sheet or film extrusion articles, profile extrusion articles, gas assist molding articles, structural foam molded articles, or thermoformed articles.

### Claim 18 (depends on 1)

The article according to claim 1, wherein the plastic composition has a reverse-side impact strength retention of at least 80% after exposure to a terpene oil, when tested according to the methods disclosed in Example 2.

### Claim 19 (depends on 18)

The article according to claim 18, wherein the plastic composition has a reverse-side impact strength retention of at least 95% after exposure to d-limonene, when tested according to the methods disclosed in Example 2.

### Claim 20 (depends on 1)

The article according to claim 1, wherein the dicarboxylic acid component of the polyester comprises monomer residues having at least 50 mole % recycle content, or at least 75 mole % recycle content.