# US 2023/0406765 A1 · Synthetic silica glass in non-portland cements

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0406765 A1
- Document ID: US20230406765A1
- Status: Published application
- Kind: A1
- Application number: 17/807,106
- Filed: 2022-06-15
- Published: 2023-12-21
- Earliest claimed: 2022-06-15
- Assignees: Halliburton Energy Services, Inc.
- Applicants: Halliburton Energy Services, Inc.
- Inventors: Thomas Jason PISKLAK; Kyriacos AGAPIOU; Samuel J LEWIS
- Web page: https://patentgrep.com/patent/US20230406765A1

## CPC

- C04B 14/22: Glass {; Devitrified glass}
- C04B 28/04: Portland cements
- C04B 7/02: Portland cement
- C04B 7/32: Aluminous cements
- C04B 7/34: Hydraulic lime cements; Roman cements {; natural cements}
- C04B 28/06: Aluminous cements (monolithic refractories or refractory mortars C04B35/66)
- C04B 28/30: containing magnesium cements {or similar cements}(magnesium oxide cements C04B28/10)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A cement composition can include water and a blended cement. The cement composition can be free of Portland cement. The blended cement can include cement and a supplementary cementitious material. The cement can be calcium aluminate cement or calcium aluminophosphate cement. Fly ash is a common supplementary cementitious material containing silica. However, fly ash can have large variances depending on the source of the fly ash. Instead of fly ash, the supplementary cementitious material can be ground synthetic glass, such as soda-lime glass, which has consistent properties regardless of the source.

## Claims

### Claim 1

A cement composition comprising:
water; and
a blended cement, wherein the blended cement comprises:
(i) cement, wherein less than 30% weight by weight of the cement is Portland cement; and
(ii) a supplementary cementitious material, wherein the supplementary cementitious material is ground synthetic glass.

### Claim 2 (depends on 1)

The cement composition according to claim 1, wherein the water is selected from the group consisting of freshwater, brackish water, saltwater, and combinations thereof.

### Claim 3 (depends on 1)

The cement composition according to claim 1, wherein the cement is in a concentration in the range of 20% to 80% by weight of the blended cement.

### Claim 4 (depends on 1)

The cement composition according to claim 1, wherein the cement is a calcium aluminate cement.

### Claim 5 (depends on 1)

The cement composition according to claim 1, wherein the cement is a calcium aluminophosphate cement, and wherein a phosphate is in a concentration in the range of 1% to 10% by weight of the cement.

### Claim 6 (depends on 1)

The cement composition according to claim 1, wherein the ground synthetic glass is selected from the group consisting of soda-lime glass, borosilicate glass, lead glass, aluminosilicate glass, germanosilicate glass, phosphosilicate glass, silicate filter glasses, and combinations thereof.

### Claim 7 (depends on 1)

The cement composition according to claim 1, wherein the ground synthetic glass is in a concentration in the range of 20% to 80% by weight of the blended cement.

### Claim 8 (depends on 1)

The cement composition according to claim 1, wherein the ground synthetic glass is recycled glass.

### Claim 9 (depends on 1)

The cement composition according to claim 1, wherein the cement and the supplementary cementitious material have a particle size less than or equal to 0.8 millimeters.

### Claim 10 (depends on 1)

The cement composition according to claim 1, wherein the cement and the supplementary cementitious material have a particle size in the range of 0.025 to 0.8 millimeters.

### Claim 11 (depends on 1)

The cement composition according to claim 1, wherein the cement composition has a thickening time in the range of 4 to 15 hours at a temperature of 93.3° C. and a pressure of 65 millipascal.

### Claim 12 (depends on 1)

The cement composition according to claim 1, wherein the cement composition has a compressive strength in the range of 500 to 10,000 psi when tested at 24 hours, a temperature of 125° F., and a pressure of 3,000 psi.

### Claim 13 (depends on 1)

The cement composition according to claim 1, wherein the blended cement has a water requirement at least 20% greater than a blended cement containing fly ash as the supplementary cementitious material.

### Claim 14 (depends on 1)

The cement composition according to claim 1, wherein the cement composition further comprises a second supplementary cementitious material, and wherein the second supplementary cementitious material is selected from lime or kiln dust.

### Claim 15 (depends on 1)

The cement composition according to claim 1, wherein the cement composition has a thermal stability at a temperature less than or equal to 1,400° C.

### Claim 16

A method of cementing in a well comprising:
introducing a cement composition into the well, wherein the cement composition comprises:
water; and
a blended cement, wherein the blended cement comprises:
(i) cement, wherein less than 30% weight by weight of the cement is Portland cement; and
(ii) a supplementary cementitious material, wherein the supplementary cementitious material is ground synthetic glass; and
allowing the cement composition to set.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the cement is a calcium aluminate cement or a calcium aluminophosphate cement, and wherein a phosphate of the calcium aluminophosphate cement is in a concentration in the range of 1% to 10% by weight of the cement.

### Claim 18 (depends on 16)

The method according to claim 16, wherein the ground synthetic glass is selected from the group consisting of soda-lime glass, borosilicate glass, lead glass, aluminosilicate glass, germanosilicate glass, phosphosilicate glass, silicate filter glasses, and combinations thereof.

### Claim 19 (depends on 16)

The method according to claim 16, wherein the ground synthetic glass is in a concentration in the range of 20% to 80% by weight of the blended cement.

### Claim 20 (depends on 16)

The method according to claim 16, wherein the cement composition has a thermal stability at a temperature less than or equal to 1,400° C.