# US 2023/0405967 A1 · Fiber-reinforced resin substrate, preform, integrated product, and method for producing fiber-reinforced resin substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0405967 A1
- Document ID: US20230405967A1
- Status: Published application
- Kind: A1
- Application number: 18/035,366
- Filed: 2021-11-15
- Published: 2023-12-21
- Earliest claimed: 2020-11-20
- Assignees: Toray Industries, Inc.
- Applicants: Toray Industries, Inc.
- Inventors: Takashi Fujioka; Masato Honma; Yoshifumi Nakayama
- Web page: https://patentgrep.com/patent/US20230405967A1

## CPC

- B32B 5/02: characterised by structural features of a {fibrous or filamentary} layer {(layer formed of metallic wires B32B15/02; layer formed of natural mineral fibres B32B19/02; layer formed of wood fibres B32B21/02)}
- C08J 5/042: {with carbon fibres}
- B29C 37/0082: {Mechanical anchoring (B29C66/303 takes precedence)}
- B29C 70/0035: {comprising two or more matrix materials}
- B29C 70/506: {and impregnating by melting a solid material, e.g. sheet, powder, fibres (B29C70/508 takes precedence)}
- B32B 27/12: next to a fibrous or filamentary layer
- B32B 27/20: using fillers, pigments, thixotroping agents
- B32B 27/34: comprising polyamides
- C08J 5/06: using pretreated fibrous materials
- B32B 2250/02: 2 layers
- B32B 2260/021: Fibrous or filamentary layer
- B32B 2260/046: Synthetic resin
- B32B 2262/02: Synthetic macromolecular fibres
- B32B 2262/106: Carbon fibres, e.g. graphite fibres
- B32B 2307/538: Roughness
- B32B 2307/54: Yield strength; Tensile strength
- B32B 2307/704: Crystalline
- B32B 2307/748: Releasability
- C08J 2365/00: Characterised by the use of macromolecular compounds obtained by reactions forming a carbon-to-carbon link in the main chain (C08J2307/00 - C08J2357/00, C08J2361/00 take precedence); Derivatives of such polymers
- C08J 2371/00: Characterised by the use of polyethers obtained by reactions forming an ether link in the main chain; Derivatives of such polymers
- C08J 2377/02: Polyamides derived from omega-amino carboxylic acids or from lactams thereof (C08J2377/10 takes precedence)
- C08J 2381/04: Polysulfides
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

A fiber-reinforced resin substrate is described in which a plurality of resins having differing properties are strongly composited, wherein the fiber-reinforced resin substrate is obtained by impregnating a thermoplastic resin (A) and a thermoplastic resin (B) into continuous reinforcement fibers, wherein a thermoplastic resin (A) layer, which comprises the thermoplastic resin (A) and is exposed at one surface, and a thermoplastic resin (B) layer, which comprises the thermoplastic resin (B) and is exposed at the other surface, form a boundary region, where at least some of the continuous reinforcement fibers exist in a manner spanning across the boundary region and both the thermoplastic resin (A) and the thermoplastic resin (B) are crystalline resins having a melting point of not less than 200° C.

## Claims

### Claim 1

A fiber-reinforced resin substrate obtained by impregnating a thermoplastic resin (A) and a thermoplastic resin (B) into continuous reinforcing fibers,
wherein a thermoplastic resin (A) layer, which comprises the thermoplastic resin (A) and is exposed at one surface, and a thermoplastic resin (B) layer, which comprises the thermoplastic resin (B) and is exposed at the other surface, form a boundary region,
at least some of the continuous reinforcing fibers exist across the boundary region, and
both the thermoplastic resin (A) and the thermoplastic resin (B) are a crystalline resin having a melting point of 200° C. or higher.

### Claim 2 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein a difference in melting point between the thermoplastic resin (A) and the thermoplastic resin (B) is 10 to 50° C.

### Claim 3 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein the thermoplastic resin (A) layer exposed at the one surface and the thermoplastic resin (B) layer exposed at the other surface are joined to each other by forming an interface.

### Claim 4 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein an interlaminar shear strength between the thermoplastic resin (A) layer and the thermoplastic resin (B) layer as measured according to JIS K7092 (2005) is 30 MPa or more.

### Claim 5 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein the thermoplastic resin (A) and the thermoplastic resin (B) are different resin types.

### Claim 6 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein the thermoplastic resin (A) is a resin selected from the group consisting of polyarylene ether ketone, polyphenylene sulfide, polyether ether ketone, and polyether ketone ketone.

### Claim 7 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein a thickness of the thermoplastic resin (A) layer is 20 to 80% of a thickness of the fiber-reinforced resin substrate.

### Claim 8 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein a volume content of reinforcing fibers of the thermoplastic resin (A) layer and the thermoplastic resin (B) layer is 30 vol % or more.

### Claim 9 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein melting points of the thermoplastic resin (A) and the thermoplastic resin (B) are both 250° C. or higher and/or glass transition temperatures of the thermoplastic resin (A) and the thermoplastic resin (B) are both 100° C. or higher.

### Claim 10 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein thermal decomposition start temperatures of the thermoplastic resin (A) and the thermoplastic resin (B) are 480° C. or higher.

### Claim 11 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein reinforcing fibers having a surface free energy as measured by a Wilhelmy plate method of 10 to 50 mJ/m2 are used as the reinforcing fibers.

### Claim 12 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein a tensile strength of the reinforcing fiber is 5.5 GPa or more.

### Claim 13 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein in a cross section in a thickness direction taken along a direction of 45 degrees with respect to a fiber direction of the reinforcing fiber, a profile curve formed by the interface has an average roughness length RSm, defined in JIS B0601 (2001), of 100 μm or less and an average roughness height Rc of 3.5 μm or more.

### Claim 14 (depends on 1)

The fiber-reinforced resin substrate according to claim 1, wherein a thickness of the fiber-reinforced resin substrate is 500 μm or less.

### Claim 15 (depends on 1)

A preform comprising the fiber-reinforced resin substrate according to claim 1, the fiber-reinforced resin substrate being disposed between a member A having a thermoplastic resin (A) on a surface thereof and a member B having a thermoplastic resin (B) on a surface thereof such that the thermoplastic resin (A) layer and the thermoplastic resin (B) layer of the fiber-reinforced resin substrate are in contact with the thermoplastic resin (A) of the member A and the thermoplastic resin (B) of the member B, respectively.

### Claim 16 (depends on 1)

An integrated product obtained by welding a member A having a thermoplastic resin (A) on a surface thereof and a member B having a thermoplastic resin (B) on a surface thereof with the fiber-reinforced resin substrate according to claim 1 interposed therebetween such that the thermoplastic resin (A) layer and the thermoplastic resin (B) layer of the fiber-reinforced resin substrate are welded to the thermoplastic resin (A) of the member A and the thermoplastic resin (B) of the member B, respectively.

### Claim 17 (depends on 16)

The integrated product according to claim 16, wherein the member A and/or the member B is a fiber-reinforced resin.

### Claim 18

A method for producing a fiber-reinforced resin substrate obtained by impregnating a thermoplastic resin (A) and a thermoplastic resin (B) into continuous reinforcing fibers, comprising:
impregnating a thermoplastic resin (A) from one surface of a continuous reinforcing fiber sheet to obtain a semi-preg having a thermoplastic resin (A) layer exposed at one surface and the continuous reinforcing fiber sheet exposed at the other surface; impregnating a thermoplastic resin (B) from the other surface of the semi-preg or impregnating a thermoplastic resin (B) from one surface of the continuous reinforcing fiber sheet to obtain a semi-preg having a thermoplastic resin (B) layer exposed at one surface and the continuous reinforcing fiber sheet exposed at the other surface; and impregnating the thermoplastic resin (A) from the other surface of the semi-preg.