# US 2023/0405874 A1 · Monocrystalline silicon micro-nano dual-scale anti-reflection texture and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0405874 A1
- Document ID: US20230405874A1
- Status: Published application
- Kind: A1
- Application number: 17/941,726
- Filed: 2022-09-09
- Published: 2023-12-21
- Earliest claimed: 2022-06-20
- Assignees: Shandong University; Yanshan University
- Applicants: Shandong University; Yanshan University
- Inventors: Chuanzhen HUANG; Xuefei LIU; Hanlian LIU; Peng YAO; Hongtao ZHU; Bin ZOU; Dun LIU; Jun WANG; Zhen WANG; Longhua XU; Shuiquan HUANG
- Web page: https://patentgrep.com/patent/US20230405874A1

## CPC

- B28D 5/04: by tools other than rotary type, e.g. reciprocating tools {(B28D5/0005 takes precedence)}
- B23K 26/0624: {using ultrashort pulses, i.e. pulses of 1 ns or less}
- G02B 1/113: using inorganic layer materials only
- G02B 1/118: having sub-optical wavelength surface structures designed to provide an enhanced transmittance, e.g. moth-eye structures
- B23K 26/0622: by shaping pulses
- B23K 26/0869: {Devices involving movement of the laser head in at least one axial direction}
- B23K 26/146: the fluid stream containing a liquid
- B23K 26/147: {Features outside the nozzle for feeding the fluid stream towards the workpiece}
- B23K 26/364: for making a groove or trench, e.g. for scribing a break initiation groove
- B23K 26/402: involving non-metallic material, e.g. isolators
- B23K 2101/36: Electric or electronic devices
- B23K 2103/56: {being semiconducting}
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- B28D: WORKING STONE OR STONE-LIKE MATERIALS
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A monocrystalline silicon micro-nano dual-scale anti-reflection texture and a preparation method therefor. The preparation method combines nanosecond-laser-assisted waterjet near-damage-free processing and femtosecond laser scanning, and subsurface damage caused by a re-cast layer phenomenon and a hot crack in a monocrystalline silicon laser texturing process can be effectively reduced by combining a nanosecond-laser-assisted waterjet near-damage-free processing technology and an ultra-short pulse femtosecond laser cold processing technology; and meanwhile, a micro-scale frame structure and a nano-scale structure can be flexibly modified respectively by adjusting nanosecond-laser-assisted waterjet technological parameters and femtosecond laser technological parameters, a geometry light trapping effect and an effective dielectric effect can be achieved in a micro-nano dual-scale hybrid structure at the same time, and surface reflection is reduced.

## Claims

### Claim 1

A method for preparing a monocrystalline silicon micro-nano dual-scale anti-reflection texture, comprising: a nanosecond-laser-assisted waterjet device is utilized for scanning in a longitudinal direction of a monocrystalline silicon wafer, and waterjet is arranged behind nanosecond lasers in a scanning speed direction to prepare a V-shaped groove array in the monocrystalline silicon wafer; and
nano structures different in size or density are processed in different positions of the V-shaped groove array by utilizing femtosecond lasers in different focus hight for sequential scanning in a transverse direction perpendicular to the V-shaped groove array or forming a set angle with the V-shaped groove array, thereby obtaining the micro-nano dual-scale anti-reflection texture.

### Claim 2 (depends on 1)

The method for preparing a monocrystalline silicon micro-nano dual-scale anti-reflection texture according to claim 1, comprising: a pulse width of the nanosecond lasers is 10-350 ns, pulse repetition frequency is 20-1000 kHz, a scanning speed is 1-5 mm/s, and pressure intensity of waterjet is 5-20 MPa.

### Claim 3 (depends on 2)

The method for preparing a monocrystalline silicon micro-nano dual-scale anti-reflection texture according to claim 2, comprising: a wavelength of the nanosecond lasers is 1064 nm.

### Claim 4 (depends on 1)

The method for preparing a monocrystalline silicon micro-nano dual-scale anti-reflection texture according to claim 1, comprising: laser pulse energy is 0-0.6 mJ, focus hight is -0.6-0.6 mm, a waterjet nozzle standoff distance is 0.2-1.2 mm, an offset distance of the waterjet is 0.1-0.8 mm, and a waterjet impact angle ranges from 30 degrees to 60 degrees.

### Claim 5 (depends on 4)

The method for preparing a monocrystalline silicon micro-nano dual-scale anti-reflection texture according to claim 4, comprising: laser pulse energy of the femtosecond lasers is 0-13 mJ, a scanning speed is 25-300 μm/s, and pulse repetition frequency is 1-1000 Hz.

### Claim 6 (depends on 5)

The method for preparing a monocrystalline silicon micro-nano dual-scale anti-reflection texture according to claim 5, comprising: a wavelength of the femtosecond lasers is 800 nm, and a laser pulse width is 35 fs.

### Claim 7 (depends on 6)

The method for preparing a monocrystalline silicon micro-nano dual-scale anti-reflection texture according to claim 6, comprising: the focal planes of the femtosecond lasers are positioned to middles of V-shaped grooves.

### Claim 8 (depends on 1)

The method for preparing a monocrystalline silicon micro-nano dual-scale anti-reflection texture according to claim 1, comprising: a depth of the V-shaped grooves is 20-40 μm, and a width is 20-40 μm.

### Claim 9 (depends on 1)

The method for preparing a monocrystalline silicon micro-nano dual-scale anti-reflection texture according to claim 1, comprising: the nano structure is a fine ripple periodic structure, a coarse ripple periodic structure or/and a nano particle.

### Claim 10 (depends on 1)

A monocrystalline silicon micro-nano dual-scale anti-reflection texture, prepared by the preparation method according to claim 1.