# US 2023/0403852 A1 · Memory device and method for forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0403852 A1
- Document ID: US20230403852A1
- Status: Published application
- Kind: A1
- Application number: 17/837,227
- Filed: 2022-06-10
- Published: 2023-12-14
- Earliest claimed: 2022-06-10
- Assignees: Macronix International Co., Ltd.
- Applicants: Macronix International Co., Ltd.
- Inventors: Chi-Pin LU; Pei-Ci JHANG; Masaru NAKAMICHI; Ling-Wuu YANG; Kuang-Chao CHEN
- Web page: https://patentgrep.com/patent/US20230403852A1

## CPC

- H10B 43/27: the channels comprising vertical portions, e.g. U-shaped channels
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

An integrated circuit structure includes a plurality of gate layers, a laterally stacked multi-layered memory structure, and a vertical channel layer. The gate layers laterally extend above the substrate and spaced apart from each other. The laterally stacked multi-layered memory structure extends upwardly above the substrate and through the gate layers and including a blocking layer, a charge storage stack, and a tunneling layer. The charge storage stack is on the blocking layer and including a first silicon nitride layer, a second silicon nitride layer, and a silicon oxynitride layer sandwiched between the first and second silicon nitride layers. The tunneling layer is on the charge storage stack. The vertical channel layer is on the laterally stacked multi-layered memory structure.

## Claims

### Claim 1

An integrated circuit (IC) structure, comprising:
a plurality of gate layers laterally extending above a substrate and spaced apart from each other;
a laterally stacked multi-layered memory structure extending upwardly above the substrate and through the gate layers and comprising:
a blocking layer;
a charge storage stack on the blocking layer and comprising a first silicon nitride layer, a second silicon nitride layer, and a silicon oxynitride layer sandwiched between the first and second silicon nitride layers; and
a tunneling layer on the charge storage stack; and
a vertical channel layer on the laterally stacked multi-layered memory structure.

### Claim 2 (depends on 1)

The IC structure of claim 1, wherein the first silicon nitride layer has a greater nitrogen atomic concentration than the second silicon nitride layer.

### Claim 3 (depends on 2)

The IC structure of claim 2, wherein the first silicon nitride layer is in contact with the blocking layer.

### Claim 4 (depends on 1)

The IC structure of claim 1, wherein the first silicon nitride layer has a less refractive index than the second silicon nitride layer.

### Claim 5 (depends on 1)

The IC structure of claim 1, wherein the first silicon nitride layer has a refractive index in a range from about 2.00 to about 2.03, and the second silicon nitride layer has a refractive index in a range from about 2.07 to about 2.10.

### Claim 6 (depends on 1)

The IC structure of claim 1, wherein the silicon oxynitride layer has a less refractive index than the first and second silicon nitride layers.

### Claim 7 (depends on 1)

The IC structure of claim 1, wherein the silicon oxynitride layer has a refractive index in a range from about 1.52 to about 1.65.

### Claim 8 (depends on 1)

The IC structure of claim 1, wherein the silicon oxynitride layer has a thinner thickness than the first and second silicon nitride layers.

### Claim 9 (depends on 1)

The IC structure of claim 1, wherein the silicon oxynitride layer has a greater oxygen atomic concentration than the first and second silicon nitride layers.

### Claim 10 (depends on 1)

The IC structure of claim 1, wherein the first and second silicon nitride layers are free of oxygen.

### Claim 11

A method for forming a memory device, comprising:
forming a multi-layered stack including insulating layers and gate layers alternately stacked in a vertical direction over a substrate;
etching the multi-layered stack to form a through opening;
forming a blocking layer lining a sidewall of the through opening;
forming a first silicon nitride layer on the blocking layer;
forming a silicon oxynitride layer on the first silicon nitride layer;
forming a second silicon nitride layer on the silicon oxynitride layer;
forming a tunneling layer on the second silicon nitride layer; and
forming a channel layer on the tunneling layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein forming the first silicon nitride layer is performed by introducing a first nitrogen-containing gas over the substrate having a first flow rate, and forming the second silicon nitride layer is performed by introducing a second nitrogen-containing gas over the substrate having a second flow rate less than the first flow rate.

### Claim 13 (depends on 12)

The method of claim 12, wherein the first flow rate of forming the first silicon nitride layer is in a range from about 5 to about 20 slm, and the second flow rate of forming the second silicon nitride layer is in a range from about 1 to about 5 slm.

### Claim 14 (depends on 11)

The method of claim 11, wherein forming the first silicon nitride layer is performed at a first temperature, and forming the second silicon nitride layer is performed at a second temperature substantially the same as the first temperature.

### Claim 15 (depends on 11)

The method of claim 11, wherein the first silicon nitride layer has a greater nitrogen atomic concentration than the second silicon nitride layer.

### Claim 16 (depends on 11)

The method of claim 11, wherein forming the first silicon nitride layer is performed under a first pressure, and forming the second silicon nitride layer is performed under a second pressure substantially the same as the first pressure.

### Claim 17 (depends on 11)

The method of claim 11, wherein the first silicon nitride layer has a less refractive index than the second silicon nitride layer.

### Claim 18 (depends on 11)

The method of claim 11, wherein forming the second silicon nitride layer is performing by introducing a mixture gas comprising Si2Cl6 and NH3.

### Claim 19 (depends on 11)

The method of claim 11, wherein forming the silicon oxynitride layer is performing by introducing a mixture gas comprising Si2Cl6, NH3, and O2.

### Claim 20 (depends on 11)

The method of claim 11, wherein forming the silicon oxynitride layer and the first and second silicon nitride layers are in-situ performed.