# US 2023/0402600 A1 · Positive electrode active material particle, lithium ion secondary battery and method for producing positive electrode active material particle

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0402600 A1
- Document ID: US20230402600A1
- Status: Published application
- Kind: A1
- Application number: 18/326,483
- Filed: 2023-05-31
- Published: 2023-12-14
- Earliest claimed: 2022-06-14
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: So YUBUCHI; Jun Yoshida
- Web page: https://patentgrep.com/patent/US20230402600A1

## CPC

- C01G 53/51: containing sodium
- C01G 53/502: containing lithium and cobalt
- C01G 53/82: Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/366: {as layered products}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/60: Compounds characterised by their crystallite size
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/76: by a space-group or by other symmetry indications
- C01P 2004/03: obtained by SEM
- C01P 2004/32: Spheres
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2004/80: Particles consisting of a mixture of two or more inorganic phases
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The rate characteristic of O2-type positive electrode active material particle is improved. The positive electrode active material particle of the first mode have an O2-type structure, comprise at least one transition metal elements from among Mn, Ni and Co, with Li and O, as constituent elements, and are spherical. The positive electrode active material particle of the second mode have at least one shell and at least one void in the cross-sectional structure, wherein the shell has an O2-type structure, the shell comprises at least one transition metal element from among Mn, Ni and Co, with Li and O, as constituent elements, the surface of the shell comprises crystallites, and the void is present along the inner wall of the shell.

## Claims

### Claim 1

A positive electrode active material particle,
having an O2-type structure,
comprising at least one transition metal element from among Mn, Ni and Co, with Li and O, as constituent elements, and
being spherical.

### Claim 2

A positive electrode active material particle having at least one shell and at least one void in the cross-sectional structure, wherein
the shell has an O2-type structure,
the shell comprises at least one transition metal element from among Mn, Ni and Co, with Li and O, as constituent elements,
the surface of the shell comprises crystallites, and
the void is present along an inner wall of the shells.

### Claim 3 (depends on 2)

The positive electrode active material particle according to claim 2, wherein
the positive electrode active material has layered shells, and
the void is present at least between one shell and another shell.

### Claim 4 (depends on 2)

The positive electrode active material particle according to claim 2, wherein
an outer shape of the shell is spherical.

### Claim 5 (depends on 1)

The positive electrode active material particle according to claim 1, wherein
the surface of the particle comprises crystallites.

### Claim 6 (depends on 2)

The positive electrode active material particle according to claim 2, wherein
the diameters of the crystallites are less than 1 μm.

### Claim 7 (depends on 2)

The positive electrode active material particle according to claim 2, wherein
the crystallites have first surfaces exposed on the surface of the particle, and
the first surfaces are flat.

### Claim 8 (depends on 1)

The positive electrode active material particle according to claim 1, wherein
the positive electrode active material particle comprises Li, Mn, Ni, Co and O as constituent elements.

### Claim 9 (depends on 1)

The positive electrode active material particles according to claim 1, wherein
the positive electrode active material particle has a chemical composition represented by LiaNabMnx-pNiy-qCoz-rMp+q+rO2 (where 0<a≤1.00, 0≤b≤0.20, x+y+z=1, and 0<p+q+r≤0.15, and M is at least one element selected from among B, Mg, Al, K, Ca, Ti, V, Cr, Fe, Cu, Zn, Ga, Ge, Sr, Y, Zr, Nb, Mo and W).

### Claim 10 (depends on 1)

A lithium ion secondary battery having a positive electrode, an electrolyte layer and a negative electrode, wherein
the positive electrode comprises the positive electrode active material particle according to claim 1.

### Claim 11 (depends on 10)

The lithium ion secondary battery according to claim 10, wherein
the positive electrode comprises an electrolyte solution.

### Claim 12

A method for producing a positive electrode active material particle, the method including:
obtaining a precursor particle,
covering the surface of the precursor particle with a Na salt to obtain a covered particle,
firing the covered particle to obtain Na-containing transition metal oxide particle having a P2-type structure, and
replacing at least a portion of the Na in the Na-containing transition metal oxide particle with Li by ion-exchange to obtain the positive electrode active material particle,
wherein:
the precursor particle is composed of a salt containing one or more transition metal elements from among Mn, Ni and Co,
the precursor particle is spherical,
the covered particle is obtained by covering 40 area % or more of the surface of the precursor particle with the Na salt, and
the Na-containing transition metal oxide particle is spherical.