# US 2023/0398571 A1 · Corrosion-resistant magnesium alloy with a multi-level protective coating and preparation process thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0398571 A1
- Document ID: US20230398571A1
- Status: Published application
- Kind: A1
- Application number: 18/250,597
- Filed: 2022-01-03
- Published: 2023-12-14
- Earliest claimed: 2021-01-04
- Assignees: The Boeing Company
- Applicants: The Boeing Company
- Inventors: Dingfei Zhang; Yuping Liu; Chao Miao; Hanxi Zhao; Libin Zhao
- Web page: https://patentgrep.com/patent/US20230398571A1

## CPC

- B05D 7/5483: {No curing step for any layer}
- C25D 11/026: {Anodisation with spark discharge}
- B05D 3/002: {Pretreatement}
- B05D 3/142: {Pretreatment}
- B05D 7/14: to metal, e.g. car bodies (involving a chemical reaction between the metal and the coating C23)
- B05D 7/51: {One specific pretreatment, e.g. phosphatation, chromatation, in combination with one specific coating (pretreatment of metallic substrates C23C; pretreatment before coating in general B05D3/00)}
- B05D 7/546: {each layer being cured, at least partially, separately}
- C22C 23/00: Alloys based on magnesium
- C23G 1/12: Light metals
- C25D 11/30: of magnesium or alloys based thereon
- B05D 1/02: performed by spraying
- B05D 3/0254: {After-treatment}
- B05D 3/12: by mechanical means
- B05D 2202/20: based on light metals
- B05D 2350/60: Adding a layer before coating
- B05D 2503/00: Polyurethanes
- B05D 2504/00: Epoxy polymers
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS

## Abstract

A corrosion-resistant magnesium alloy with a multi-level protective coating, and to a preparation process thereof. The magnesium alloy with a multi-level protective coating comprises a magnesium alloy substrate and a multi-level protective coating. The multi-level protective coating comprises a micro-arc oxidation layer of magnesium alloy provided on the surface of the magnesium alloy substrate, an epoxy primer layer provided on the surface of the micro-arc oxidation layer of magnesium alloy, and a polyurethane topcoat layer provided on the surface of the epoxy primer layer. The magnesium alloy with a multi-level protective coating effectively integrates the excellent adhesion of the micro-arc oxidation layer and the excellent anti-corrosion effect of the organic coating. The process for the preparation of the magnesium alloy with a multi-level protective coating is cost-effective, simple, suitable for large-area and large-scale magnesium alloy treatment, and suitable for the development for large-area scale industrialization. The magnesium alloy with a multi-level protective coating is characterized by a good adhesion and an excellent salt spray resistance, exhibits a period of neutral salt spray resistance test of greater than 1,000 hours, and can be applied in the automotive industry and the aviation industry.

## Claims

### Claim 1

A magnesium alloy comprising a magnesium alloy substrate and a multi-level protective coating on the magnesium alloy substrate, the multi-level protective coating comprising:
a micro-arc oxidation layer of magnesium alloy provided on a surface of the magnesium alloy substrate;
an epoxy primer layer provided on a surface of the micro-arc oxidation layer of magnesium alloy; and
a polyurethane topcoat layer provided on a surface of the epoxy primer layer.

### Claim 2 (depends on 1)

The magnesium alloy according to claim 1, wherein the micro-arc oxidation layer of magnesium alloy has a thickness of 5-20 μm.

### Claim 3 (depends on 1)

The magnesium alloy according to claim 1, wherein the epoxy primer layer has a thickness of 10-30 μm.

### Claim 4 (depends on 1)

The magnesium alloy according to claim 1, wherein the polyurethane topcoat layer has a thickness of 10-50 μm.

### Claim 5 (depends on 1)

The magnesium alloy according to claim 1, wherein the micro-arc oxidation layer of magnesium alloy has a thickness of 5-20 μm, the epoxy primer layer has a thickness of 10-30 μm, and the polyurethane topcoat layer has a thickness of 10-50 μm.

### Claim 6 (depends on 1)

The magnesium alloy according to claim 1, wherein the magnesium alloy substrate is selected from a group consisting of AZ21 series magnesium alloy, AZ31 series magnesium alloy, AZ91 series magnesium alloy, and ZE41 series magnesium alloy.

### Claim 7 (depends on 1)

The magnesium alloy according to claim 1 having a period of neutral salt spray test according to ASTM B117-16 of more than 1,000 hours.

### Claim 8 (depends on 7)

The magnesium alloy according to claim 7 having a degree of blistering according to ASTM D1654-08(2016) of up to 10, a degree of rusting according to ASTM D1654-08(2016) of up to 10, a degree of cracking according to ISO 4628-4 (2016) of up to 0, and a degree of flaking according to ISO 4628-5 (2016) of up to 0.

### Claim 9 (depends on 1)

The magnesium alloy according to claim 1 having a period of neutral salt spray test according to ASTM B117-16 of more than 1,100 hours.

### Claim 10 (depends on 9)

The magnesium alloy according to claim 9 having a degree of blistering according to ASTM D1654-08(2016) of up to 10, a degree of rusting according to ASTM D1654-08(2016) of up to 10, a degree of cracking according to ISO 4628-4 (2016) of up to 0, and a degree of flaking according to ISO 4628-5 (2016) of up to 0.

### Claim 11 (depends on 1)

The magnesium alloy according to claim 1 having a period of neutral salt spray test according to ASTM B117-16 of more than 1,200 hours.

### Claim 12 (depends on 11)

The magnesium alloy according to claim 11 having a degree of blistering according to ASTM D1654-08(2016) of up to 10, a degree of rusting according to ASTM D1654-08(2016) of up to 10, a degree of cracking according to ISO 4628-4 (2016) of up to 0, and a degree of flaking according to ISO 4628-5 (2016) of up to 0.

### Claim 13

A process for preparing a magnesium alloy with a multi-level protective coating, comprising:
pretreatment of a magnesium alloy substrate;
micro-arc oxidation of the pretreated magnesium alloy substrate to obtain a micro-arc oxidation layer of magnesium alloy;
formation of an epoxy primer layer on the surface of the micro-arc oxidation layer of magnesium alloy; and
formation of a polyurethane topcoat layer on the surface of the epoxy primer layer.

### Claim 14 (depends on 13)

The process according to claim 13 wherein the pretreatment of the magnesium alloy substrate comprises polishing the magnesium alloy substrate to yield a polished magnesium alloy substrate.

### Claim 15 (depends on 14)

The process according to claim 14 wherein the pretreatment of the magnesium alloy substrate further comprises acid pickling and water washing of the polished magnesium alloy substrate sequentially.

### Claim 16 (depends on 15)

The process according to claim 15, wherein the pretreatment of the magnesium alloy substrate comprises:
polishing the magnesium alloy substrate with water sandpaper from coarse to fine of 200 #, 400 #, 600 #, 800 #, 1000 #, 1200 # to remove burrs at margins and corners to obtain a preliminary-polished magnesium alloy substrate;
polishing the preliminary-polished magnesium alloy substrate with sandpaper or abrasive wheel from coarse to fine until a surface of the preliminary-polished magnesium alloy substrate is smooth to obtain the polished magnesium alloy substrate; and
pickling the polished magnesium alloy substrate with an acid of pH=0.5 to 2 and washing with pure water to obtain the pretreated magnesium alloy substrate.

### Claim 17 (depends on 13)

The process according to claim 13 further comprising coarsen treatment of the epoxy primer layer before formation of the polyurethane topcoat layer on the surface of the epoxy primer layer.

### Claim 18 (depends on 13)

The process according to claim 13, wherein the magnesium alloy substrate is selected from a group consisting of AZ21 series magnesium alloy, AZ31 series magnesium alloy, AZ91 series magnesium alloy, and ZE41 series magnesium alloy.

### Claim 19 (depends on 13)

A magnesium alloy with a multi-level protective coating produced by the process for preparing a magnesium alloy with a multi-level protective coating according to claim 13.

### Claim 20 (depends on 19)

The magnesium alloy of claim 19 having:
a period of neutral salt spray test according to ASTM B117-16 of more than 1,000 hours,
a degree of blistering according to ASTM D1654-08(2016) of up to 10,
a degree of rusting according to ASTM D1654-08(2016) of up to 10,
a degree of cracking according to ISO 4628-4 (2016) of up to 0, and
a degree of flaking according to ISO 4628-5 (2016) of up to 0.