# US 2023/0398519 A1 · Hydrotalcite-precursor based catalyst with improved performance for lts reaction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0398519 A1
- Document ID: US20230398519A1
- Status: Published application
- Kind: A1
- Application number: 18/121,637
- Filed: 2023-03-15
- Published: 2023-12-14
- Earliest claimed: 2022-06-09
- Assignees: Clariant International Ltd.
- Applicants: Clariant International Ltd
- Inventors: Tobias MUELLER; Stephan J. REITMEIER; Hongyi C. HOU; Claus G. LUGMAIR
- Web page: https://patentgrep.com/patent/US20230398519A1

## CPC

- B01J 23/80: with zinc, cadmium or mercury
- B01J 6/001: {Calcining}
- B01J 21/04: Alumina
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 35/37: Crush or impact strength
- B01J 35/613: {10-100 m2/g}
- B01J 35/615: {100-500 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/647: {2-50 nm}
- B01J 35/70: characterised by their crystalline properties, e.g. semi-crystalline (catalysts comprising carbon B01J21/18; molecular sieves B01J29/00)
- B01J 35/80: characterised by their amorphous structures
- B01J 37/0009: {Use of binding agents; Moulding; Pressing; Powdering; Granulating; Addition of materials ameliorating the mechanical properties of the product catalyst}
- B01J 37/031: {Precipitation}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C01B 3/16: using catalysts
- B01J 35/38: Abrasion or attrition resistance
- B01J 2235/15: X-ray diffraction
- C01B 2203/0283: containing a CO-shift step, i.e. a water gas shift step
- C01B 2203/1005: Arrangement or shape of catalyst
- C01B 2203/1076: Copper or zinc-based catalysts
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to a novel catalyst for LTS processes, the method of its preparation and LTS process by use of this catalyst.

## Claims

### Claim 1

Catalyst for an LTS reaction, comprising an amorphous Cu—Zn—Al mixed oxide.

### Claim 2 (depends on 1)

Catalyst according to claim 1, whereby it comprises domains of CuO, ZnO and a Zn spinel, preferably a Zn spinel of gahnite structure, as determined by Pair Distribution Function (PDF) analysis.

### Claim 3 (depends on 1)

Catalyst according to claim 1, wherein the catalyst is present as a shaped catalyst body, preferably as a tableted shaped body.

### Claim 4 (depends on 3)

Catalyst according to claim 3, wherein the catalyst is present as a tableted shaped body with a side crush strength of from 40 to 250 N, preferably of from 80 to 220 N, more preferably of from 100 to 220 N, most preferably of from 150 N to 210 N.

### Claim 5 (depends on 1)

Catalyst according to claim 1, wherein the amount of Cu is in the range of from 30 to 50 mol-%, preferably of from 30 to 45 mol-%, the amount of Zn is in the range of from 15 to 45 mol-%, preferably of from 20 to 40 mol-%, and the amount of Al is is in the range of from 15 to 50 mol-%, preferably in the range of from 20 to 40 mol-%, in relation to the overall amount of Cu, Zn and Al in the catalyst.

### Claim 6 (depends on 1)

Catalyst according to claim 1, wherein the phase content in weight percent, as determined by PDF analysis, of CuO is in the range of from 10 to 20, preferably in the range of from 15 to 20, of ZnO is in the range of from 1 to 10, preferably of from 2 to 7, and of the Zn spinel of gahnite structure is in the range of from 70 to 89, preferably in the range of from 75 to 85.

### Claim 7 (depends on 1)

Process for the preparation of the catalyst according to claim 1, comprising the following steps:
a) Providing an aqueous solution comprising solved Cu, Zn and Al compounds
b) Providing an aqueous solution comprising a carbonate
c) mixing the solution obtained in step a) and the carbonate solution obtained in step b) to obtain a mixture comprising a precipitate of mixed Cu—Zn—Al hydroxide-carbonate
d) Ageing the mixture obtained after step c)
e) Separating the precipitate from the solution and optionally washing and/or drying the precipitate
f) Calcining the precipitate at a temperature in the range of from 200° C. to 600° C., preferably in the range of from 200 to 500° C., more preferably in the range of from 300° C. to 500° C., most preferably in the range of from 350° C. to 500° C., for a duration in the range of from 15 minutes to 8 hours, preferably in the range of from 0.5 to 6 h, more preferably in the range of from 1 hour to 6 hours.

### Claim 8 (depends on 7)

Process according to claim 7, wherein the precipitate after step f) is formed to obtain a shaped catalyst body in a step g).

### Claim 9 (depends on 7)

Process according to claim 7, wherein the pH value after step c) is 8 or higher, preferably lies within a range of from 8 to 9, more preferably within 8.5 to 9.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6)

LTS reaction by use of a catalyst according to any of claims 1 to 6.

### Claim 11 (depends on 10)

LTS reaction according to claim 10, whereby the catalyst is reduced before usage.

### Claim 12 (depends on 10, 11)

LTS reaction according to claim 10 or 11, wherein a synthesis gas comprising CO, CO2 and H2 is used and wherein the CO content is 60% or less, preferably 20% or less, more preferably in the range of from 0.1 to 20%.