# US 2023/0393055 A1 · Water film evaluation method, and antifogging agent evaluation method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0393055 A1
- Document ID: US20230393055A1
- Status: Published application
- Kind: A1
- Application number: 18/037,441
- Filed: 2021-11-17
- Published: 2023-12-07
- Earliest claimed: 2020-11-20
- Assignees: Resonac Corporation
- Applicants: Resonac Corporation
- Inventors: Ryuichiro FUKUTA; Tomohiko KOTAKE; Mari SHIMIZU; Chisato KIKKAWA; Takahiro YAMANAKA; Yuri NAKANE
- Web page: https://patentgrep.com/patent/US20230393055A1

## CPC

- G01N 21/17: Systems in which incident light is modified in accordance with the properties of the material investigated (where the material investigated is optically excited causing a change in wavelength of the incident light G01N21/63)
- G01N 21/8422: {Investigating thin films, e.g. matrix isolation method}
- C08J 5/18: Manufacture of films or sheets
- C08K 3/36: Silica
- G01N 1/28: Preparing specimens for investigation {including physical details of (bio-)chemical methods covered elsewhere, e.g. G01N33/50, C12Q}(mounting specimens on microscopic slides G02B21/34; means for supporting the objects or the materials to be analysed in electron microscopes H01J37/20 {; laboratory gas handling apparatus B01L5/00})
- G01N 13/02: Investigating surface tension of liquids
- G01N 2013/0208: {by measuring contact angle}
- G01N 2013/0275: {involving surface-active agents}
- G02B 1/18: Coatings for keeping optical surfaces clean, e.g. hydrophobic or photo-catalytic films (G02B1/16 takes precedence)
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A method for evaluating water film is a method for evaluating water film uniformity, and the method includes: a first step of preparing a base material for water film formation having a principal surface for forming a water film thereon; a second step of capturing an image of an object having a pattern in which a plurality of regions having predetermined brightness are disposed in a predetermined area, through the base material for water film formation having a water film formed on the principal surface, to obtain an image for evaluation; and a third step of deriving a water film uniformity index indicating uniformity of the water film based on the area distribution of the regions having predetermined brightness in the image for evaluation.

## Claims

### Claim 1

A method for evaluating water film for uniformity, the method comprising:
a first step of preparing a base material for water film formation having a principal surface for forming a water film thereon;
a second step of capturing an image of an object having a pattern in which a plurality of regions having predetermined brightness are disposed in a predetermined area, through the base material for water film formation having a water film formed on the principal surface, to obtain an image for evaluation; and
a third step of deriving a water film uniformity index indicating uniformity of the water film based on an area distribution of the regions having predetermined brightness in the image for evaluation.

### Claim 2

A method for evaluating antifogging agent, the method comprising:
a first step of preparing a sample by treating a principal surface of a base material with an antifogging agent;
a second step of capturing an image of an object having a pattern in which a plurality of regions having predetermined brightness are disposed in a predetermined area, through the sample having a water film formed on the principal surface treated with the antifogging agent, to obtain an image for evaluation; and
a third step of deriving a water film uniformity index indicating uniformity of the water film based on an area distribution of the regions having predetermined brightness in the image for evaluation,
wherein when the water film uniformity index is equal to or higher than a predetermined threshold value, the water film uniformity of the antifogging agent is considered high.

### Claim 3 (depends on 2)

The method for evaluating antifogging agent according to claim 2, wherein the method for evaluating antifogging agent is used for evaluating water film uniformity of an antifogging agent capable of forming a film having a contact angle against water of 10° or less.

### Claim 4 (depends on 2)

The method for evaluating antifogging agent according to claim 2, wherein the method for evaluating antifogging agent is used for evaluating water film uniformity of an antifogging agent including silica.

### Claim 5 (depends on 2)

The method for evaluating antifogging agent according to claim 2, further comprising:
a fourth step of applying a fog generating means capable of generating fog on the untreated base material, to the principal surface of the sample prepared in the first step, and then capturing an image of a predetermined object through the sample to obtain an image for antifogging properties evaluation; and
a fifth step of deriving an antifogging index indicating the antifogging properties of the antifogging agent on the basis of a file capacity at the time of compressing the image for antifogging properties evaluation by a predetermined compression method,
wherein the second step and the third step are carried out when the antifogging index is equal to or higher than a predetermined threshold value.

### Claim 6 (depends on 3)

The method for evaluating antifogging agent according to claim 3, wherein the method for evaluating antifogging agent is used for evaluating water film uniformity of an antifogging agent including silica.

### Claim 7 (depends on 3)

The method for evaluating antifogging agent according to claim 3, further comprising:
a fourth step of applying a fog generating means capable of generating fog on the untreated base material, to the principal surface of the sample prepared in the first step, and then capturing an image of a predetermined object through the sample to obtain an image for antifogging properties evaluation; and
a fifth step of deriving an antifogging index indicating the antifogging properties of the antifogging agent on the basis of a file capacity at the time of compressing the image for antifogging properties evaluation by a predetermined compression method,
wherein the second step and the third step are carried out when the antifogging index is equal to or higher than a predetermined threshold value.

### Claim 8 (depends on 4)

The method for evaluating antifogging agent according to claim 4, further comprising:
a fourth step of applying a fog generating means capable of generating fog on the untreated base material, to the principal surface of the sample prepared in the first step, and then capturing an image of a predetermined object through the sample to obtain an image for antifogging properties evaluation; and
a fifth step of deriving an antifogging index indicating the antifogging properties of the antifogging agent on the basis of a file capacity at the time of compressing the image for antifogging properties evaluation by a predetermined compression method,
wherein the second step and the third step are carried out when the antifogging index is equal to or higher than a predetermined threshold value.