# US 2023/0391669 A1 · Method for preparing grouting reinforcement filler for mining

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0391669 A1
- Document ID: US20230391669A1
- Status: Published application
- Kind: A1
- Application number: 18/182,836
- Filed: 2023-03-13
- Published: 2023-12-07
- Earliest claimed: 2022-06-01
- Assignees: CCTEG China Coal Research Institute
- Applicants: Ccteg China Coal Research Institute
- Inventors: Xiaofeng YU; Yuchao WANG; Dong SHEN; Lizong LIU; Guangfeng BAI; Yifang LIU; Mingkun ZHANG; Mengyuan JIA; Enqing XIE
- Web page: https://patentgrep.com/patent/US20230391669A1

## CPC

- C04B 16/0675: {from polymers obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds}
- C04B 26/16: Polyurethanes
- C04B 20/026: {Comminuting, e.g. by grinding or breaking; Defibrillating fibres other than asbestos}
- C04B 2103/30: Water reducers, plasticisers, air-entrainers, flow improvers
- C04B 2103/40: Surface-active agents, dispersants
- C04B 2103/48: Foam stabilisers
- C04B 2103/63: Flame-proofing agents
- C04B 2111/00724: {in mining operations, e.g. for backfilling; in making tunnels or galleries}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

The present disclosure provides a grouting reinforcement filler for mining and a preparation method thereof The grouting reinforcement filler for mining includes a first component and a second component. The first component includes 100 to 130 parts by weight of a polyol polymer, 0.8 to 1.2 parts by weight of a catalyst, 0.1 to 0.3 parts by weight of a foaming agent, and 0.5 to 1.5 parts by weight of a surfactant, and the second component includes 65 to 85 parts by weight of polyisocyanate, 5 to 15 parts by weight of a modifier, 10 to 20 parts by weight of a plasticizer, and 10 to 15 parts by weight of a reactive flame retardant.

## Claims

### Claim 1

A grouting reinforcement filler for mining, comprising a first component and a second component;
wherein a weight ratio of the first component to the second component is in a range of 0.85:1 to 1.15:1;
the first component comprises 100 to 130 parts by weight of a polyol polymer, 0.8 to 1.2 parts by weight of a catalyst, 0.1 to 0.3 parts by weight of a foaming agent, and 0.5 to 1.5 parts by weight of a surfactant; and
the second component comprises 65 to 85 parts by weight of polyisocyanate, 5 to 15 parts by weight of a modifier, 10 to 20 parts by weight of a plasticizer, and 10 to 15 parts by weight of a reactive flame retardant.

### Claim 2 (depends on 1)

The grouting reinforcement filler according to claim 1, wherein the polyol polymer is composed of a high ethylene oxide polyether polyol, a cross-linked polyether polyol and a phthalic anhydride polyester polyol, and a weight ratio of the high ethylene oxide polyether polyol, the cross-linked polyether polyol and the phthalic anhydride polyester polyol is in a range of 20:50:30 to 30:60:40.

### Claim 3 (depends on 2)

The grouting reinforcement filler according to claim 2, wherein the high ethylene oxide polyether polyol is NRC2000, the cross-linked polyether polyol is DL400, and the phthalic anhydride polyester polyol is RAYNOL-3152.

### Claim 4 (depends on 1)

The grouting reinforcement filler according to claim 1, wherein the catalyst is composed of a foaming catalyst and a gel catalyst, and a weight ratio of the foaming catalyst and the gel catalyst is in a range of 0.8:1 to 2.5:1.

### Claim 5 (depends on 4)

The grouting reinforcement filler according to claim 4, wherein the foaming catalyst is pentamethyldiethylenetriamine, and the gel catalyst is 1,8-diazabicyclo[5.4.0]undec-7-ene.

### Claim 6 (depends on 1)

The grouting reinforcement filler according to claim 1, wherein the foaming agent is water, and the surfactant is an organosilicon surfactant.

### Claim 7 (depends on 6)

The grouting reinforcement filler according to claim 6, wherein the organosilicon surfactant is SZ-1959.

### Claim 8 (depends on 1)

The grouting reinforcement filler according to claim 1, wherein the polyisocyanate is polyphenyl polymethylene polyisocyanate.

### Claim 9 (depends on 1)

The grouting reinforcement filler according to claim 1, wherein the modifier is AL-MIL101-NH2.

### Claim 10 (depends on 1)

The grouting reinforcement filler according to claim 1, wherein the plasticizer is dimethoxyethylene phthalate, coumarone-indene resin or a combination thereof.

### Claim 11 (depends on 1)

The grouting reinforcement filler according to claim 1, wherein the reactive flame retardant is composed of diethyl bis(2-hydroxyethyl)aminomethyl phosphonate and dibromoneopentyl glycol, and a weight ratio of diethyl bis(2-hydroxyethyl)aminomethyl phosphonate and dibromoneopentyl glycol is in a range of 4:1 to 2:1.

### Claim 12

A method for preparing a grouting reinforcement filler for mining, comprising:
adding a catalyst, a surfactant and a foaming agent into a polyol polymer in sequence for stirring at room temperature to obtain a first component;
modifying polyisocyanate with a modifier to obtain a modified polyisocyanate solution;
adding a plasticizer and a reactive flame retardant into the modified polyisocyanate solution in a closed environment in sequence for stirring at room temperature to obtain a second component; and
mixing the first component and the second component in a weight ratio of 0.85:1 to 1.15:1 to obtain the grouting reinforcement filler for injecting into a fracture of a coal-rock mass through a grouting pump.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the polyol polymer is composed of a high ethylene oxide polyether polyol, a cross-linked polyether polyol and a phthalic anhydride polyester polyol, and a weight ratio of the high ethylene oxide polyether polyol, the cross-linked polyether polyol and the phthalic anhydride polyester polyol is in a range of 20:50:30 to 30:60:40.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the high ethylene oxide polyether polyol is NRC2000, the cross-linked polyether polyol is DL400, and the phthalic anhydride polyester polyol is RAYNOL-3152.

### Claim 15 (depends on 12)

The method according to claim 12, wherein the catalyst is composed of a foaming catalyst and a gel catalyst, and a weight ratio of the foaming catalyst and the gel catalyst is in a range of 0.8:1 to 2.5:1.

### Claim 16 (depends on 12)

The method according to claim 12, wherein the reactive flame retardant is composed of diethyl bis(2-hydroxyethyl)aminomethyl phosphonate and dibromoneopentyl glycol, and a weight ratio of diethyl bis(2-hydroxyethyl)aminomethyl phosphonate and dibromoneopentyl glycol is in a range of 4:1 to 2:1.

### Claim 17 (depends on 15)

The method according to claim 15, wherein the foaming catalyst is pentamethyldiethylenetriamine, and the gel catalyst is 1,8-diazabicyclo[5.4.0]undec-7-ene.

### Claim 18 (depends on 12)

The method according to claim 12, wherein modifying polyisocyanate with the modifier comprises:
grinding the modifier in a glove box without contact with water vapor;
adding the modifier into the polyisocyanate with a quantitative sampler to obtain a mixture;
stirring the mixture at a temperature of 80° C. for 6 h; and
cooling the mixture to room temperature.

### Claim 19 (depends on 12)

The method according to claim 12, wherein the modifier is AL-MIL101-NH2, and the AL-MIL101-NH2 is prepared by:
dissolving 2-aminoterephthalic acid (H2BDC-NH2) in N,N-dimethylformamide (DMF) by heating and stirring at 110° C. to obtain a solution heated;
dividing aluminum chloride hydrated metal salt (AlCl3 6H2O) into 5 equal parts to be added into the solution heated in batches with a 10 min interval between each batch, while stirring;
stirring the solution at 110° C. for 4 h, pouring the solution into a 250 mL high-pressure reactor lined with Teflon, and standing at 110° C. for 20 h;
cooling the solution to room temperature, and filtering the solution to obtain a yellow solid;
dipping the yellow solid 5 times with 30 mL of N,N-dimethylformamide (DMF) for each time and 5 times with 30 mL of formaldehyde for each time;
performing soxhlet extraction on the yellow solid with ethanol for 24 hours for activating; and
drying the yellow solid activated at 120° C. for 24 h in a vacuum to obtained AL-MIL101-NH2.

### Claim 20 (depends on 19)

The method according to claim 19, wherein a weight ratio of the 2-aminoterephthalic acid and the aluminum chloride hydrated metal salt in preparing AL-MIL101-NH2 is 2.1:2.