# US 2023/0390868 A1 · Method for the manufacture of a welded joint by Laser Arc Hybrid Welding

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0390868 A1
- Document ID: US20230390868A1
- Status: Published application
- Kind: A1
- Application number: 18/031,388
- Filed: 2020-10-21
- Published: 2023-12-07
- Earliest claimed: 2020-10-21
- Assignees: Verdicio Solutions A.I.E.
- Applicants: Verdicio Solutions A.I.E.
- Inventors: Alvaro MANJON FERNANDEZ; Sivasambu BOHM; Marcos PEREZ RODRIGUEZ
- Web page: https://patentgrep.com/patent/US20230390868A1

## CPC

- B23K 26/322: involving coated metal parts (using absorbing layers on the workpiece B23K26/18)
- B23K 26/0006: {taking account of the properties of the material involved (B23K26/32, B23K26/40 take precedence)}
- B23K 26/348: in combination with arc heating, e.g. tungsten inert gas [TIG], metal inert gas [MIG] or plasma welding
- B23K 35/3608: {Titania or titanates}
- B23K 2103/04: Steel {or steel} alloys
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method for the manufacture of a welded joint having the following successive steps: I. the provision of at least two metallic substrates wherein at least one metallic substrate is a steel substrate having a thickness of at least 8 mm and being delimited by at least one beveled edge, wherein said beveled edge is at least partially coated with a pre-coating having a titanate and a nanoparticulate oxide selected from the group consisting of TiO2, SiO2, ZrO2, Y2O3, Al2O3, MoO3, CrO3, CeO2, La2O3 and mixtures thereof, and II. the welding of the at least two metallic substrates along the at least partially coated beveled edge by laser arc hybrid welding in leading arc configuration.

## Claims

### Claim at position 1

1-19. (canceled)

### Claim 20

A method for the manufacture of a welded joint comprising the following successive steps:
providing at least two metallic substrates wherein a first of the least two metallic substrates is a steel substrate having a thickness of at least 8 mm and being delimited by at least one beveled edge, the beveled edge being at least partially coated with a pre-coating including a titanate and a nanoparticulate oxide selected from the group consisting of TiO2, SiO2, ZrO2, Y2O3, Al2O3, MoO3, CrO3, CeO2, La2O3 and mixtures thereof; and
welding the at least two metallic substrates along the at least partially coated beveled edge by laser arc hybrid welding in leading arc configuration.

### Claim 21 (depends on 20)

The method as recited in claim 20 wherein the titanate is chosen from the group consisting of: Na2Ti3O7, NaTiO3, K2TiO3, K2Ti2O5, MgTiO3, SrTiO3, BaTiO3, CaTiO3, FeTiO3 and ZnTiO4 and mixtures thereof.

### Claim 22 (depends on 20)

The method as recited in claim 20 wherein a thickness of the pre-coating is between 10 to 140 μm.

### Claim 23 (depends on 20)

The method as recited in claim 20 wherein a percentage of the nanoparticulate oxide in the pre-coating is below or equal to 80 wt. %.

### Claim 24 (depends on 20)

The method as recited in claim 20 wherein a percentage of the nanoparticulate oxide in the pre-coating is above or equal to 10 wt. %.

### Claim 25 (depends on 20)

The method as recited in claim 20 wherein the nanoparticles have a size between 5 and 60 nm.

### Claim 26 (depends on 20)

The method as recited in claim 20 wherein a percentage of titanate in the pre-coating is above or equal to 45 wt. %.

### Claim 27 (depends on 20)

The method as recited in claim 20 wherein a diameter of the titanate is between 1 and 40 μm.

### Claim 28 (depends on 20)

The method as recited in claim 20 wherein the pre-coating further includes a binder.

### Claim 29 (depends on 28)

The method as recited in claim 28 wherein a percentage of binder in the pre-coating is between 1 and 20 wt. %.

### Claim 30 (depends on 20)

The method as recited in claim 20 wherein the arc of the laser arc hybrid welding is selected among submerged arc, gas metal arc, gas tungsten arc and plasma arc.

### Claim 31

A method for the manufacture of a pre-coated steel substrate comprising the successive following steps:
providing a steel substrate having a thickness of at least 8 mm and being delimited by at least one beveled edge with a bevel angle between 1 and 10°; and
depositing, at least partially on the beveled edge, a pre-coating solution including a titanate and a nanoparticulate oxide selected from the group consisting of TiO2, SiO2, ZrO2, Y2O3, Al2O3, MoO3, CrO3, CeO2, La2O3 and mixtures thereof.

### Claim 32 (depends on 31)

The method as recited in claim 31 wherein the depositing of the pre-coating solution is performed by spin coating, spray coating, dip coating or brush coating.

### Claim 33 (depends on 31)

The method as recited in claim 31 wherein the pre-coating solution further includes a solvent.

### Claim 34 (depends on 31)

The method as recited in claim 31 wherein the pre-coating solution includes from 1 to 200 g/L of nanoparticulate oxide.

### Claim 35 (depends on 31)

The method as recited in claim 31 wherein the pre-coating solution includes from 100 to 500 g/L of titanate.

### Claim 36 (depends on 31)

The method as recited in claim 31 wherein the pre-coating solution further includes a binder precursor.

### Claim 37 (depends on 31)

The method as recited in claim 31 further comprising drying the pre-coated steel substrate obtained by the depositing step.

### Claim 38

A coated steel substrate comprising: a steel substrate having a thickness of at least 8 mm and being delimited by at least one beveled edge with a bevel angle between 1 and 10°, the beveled edge being at least partially coated with a pre-coating comprising a titanate and a nanoparticulate oxide selected from the group consisting of TiO2, SiO2, ZrO2, Y2O3, Al2O3, MoO3, CrO3, CeO2, La2O3 and mixtures thereof.