# US 2023/0390858 A1 · Method and device for pressure sintering connection

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0390858 A1
- Document ID: US20230390858A1
- Status: Published application
- Kind: A1
- Application number: 18/201,726
- Filed: 2023-05-24
- Published: 2023-12-07
- Earliest claimed: 2022-06-03
- Assignees: Semikron Elektronik GmbH & Co. KG
- Applicants: Semikron Elektronik GmbH & Co. KG
- Inventors: Dominic BIRKICHT; Matthias DÖRRICH; Silke KRAFT; Erik MICHAELSEN
- Web page: https://patentgrep.com/patent/US20230390858A1

## CPC

- B23K 20/023: {Thermo-compression bonding}
- H10W 72/0711: {Apparatus therefor}
- B22F 7/062: {involving the connection or repairing of preformed parts}
- H10W 72/071: {Connecting or disconnecting}
- H10W 99/00: Subject matter not provided for in other groups of this subclass
- H10W 72/07331: {Connecting techniques}
- H10W 90/00: Package configurations
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A method and a device for pressure sintering connection of a joining group composed of a first and a second joining partner by means of a device with a lower tool and an upper tool having the steps: providing the joining group at room temperature as an initial temperature, arranging the joining group between the supporting surface and the pressure surface, wherein the joining group has no direct thermal contact with the supporting surface and no direct thermal contact with the pressure surface, introducing pressure onto the joining group, wherein at the start of the introduction of pressure the starting temperature of the joining group is no more than 100K above an initial temperature; increasing the temperature of the sintering agent by at least 50K above the starting temperature; ending the introduction of pressure.

## Claims

### Claim 1

A method for pressure sintering connection of a joining group (2) composed of a first and a second joining partner (20, 26) by means of a device (1) with a lower tool (4) and an upper tool (3) which are formed to exert a pressure of more than 5 MPa on the joining group (2) which is arranged between a supporting surface (40) of the lower tool (4) and a pressure surface (34) of the upper tool (3), comprising the following method steps:
A) providing the joining group (2) at room temperature as an initial temperature;
B) arranging the joining group (2) between the supporting surface (40) and the pressure surface (34), wherein the joining group (2) has no direct thermal contact with the supporting surface (40) and no direct thermal contact with the pressure surface (34);
C) introducing a pressure onto the joining group (2) by moving the lower tool (4) and the upper tool (3) towards one another, wherein at the start of the introduction of the pressure the starting temperature of the joining group (2) and a sintering agent (28), which is arranged between the first and the second joining partner (20, 26) of the joining group (2), is no more than 100K above the initial temperature;
D) increasing the temperature of the sintering agent (28), with a heating apparatus (5) of the lower tool (4), by at least 50K above the starting temperature; and
E) ending the introduction of pressure.

### Claim 2 (depends on 1)

The method, according to claim 1, wherein:
in method step A) the joining group (2) is arranged on a workpiece carrier surface of a workpiece carrier (7).

### Claim 3 (depends on 2)

The method, according to claim 2, wherein:
at a start of method step D) at least 10% of a maximum pressure bears on the joining group (2).

### Claim 4 (depends on 3)

The method, according to claim 3, wherein:
between the method steps D) and E) the sintering agent (28) is transformed at least partially into a sintered metal and the materially bonded sintering connection is formed between the first and second joining partner (20, 26).

### Claim 5 (depends on 1)

The method, according to claim 1, wherein:
in the method step C) at the start of the introduction of pressure the starting temperature is no more than 50K above the initial temperature.

### Claim 6 (depends on 4)

The method, according to claim 4, wherein:
the sintering agent (28) has metal particles including non-precious metal particles; and
a proportion of the non-precious metal particles of a total mass of the metal particles of the sintering agent (28) is more than 50%.

### Claim 7 (depends on 6)

The method, according to claim 6, wherein:
the metal of the non-precious metal particles is selected from the group consisting of copper, tin, zinc, aluminum, nickel, titanium, magnesium, and chromium.

### Claim 8 (depends on 4)

The method, according to claim 4, wherein:
method steps B) to E) are performed at normal pressure.

### Claim 9 (depends on 8)

The method, according to claim 8, wherein:
method steps B) to E) are executed in the normal atmospheric air.

### Claim 10 (depends on 4)

The method, according to claim 4, wherein:
in a method step F) which follows on from method step E) the joining group (2) is purified with formic acid.

### Claim 11 (depends on 1)

A pressure sintering connection device, provided according to claim 1, further comprising:
the lower tool (4) with a heating apparatus (5) and the upper tool (3), wherein, as a result of the movement of the upper tool (3) towards the lower tool (4), a pressure of more than 5 MPa can be operably exerted on the joining group (2) between the supporting surface (40) of the lower tool (4) and the pressure surface (34) of the upper tool (3);
wherein a holding apparatus (6) is formed such that, as long as the supporting surface (40) is adequately spaced apart from the pressure surface (34), the joining group (2) can be arranged on the holding means (62) of the holding device (6) and in movement of the pressure surface (34) towards the supporting surface (40), the holding apparatus (6) arranges the joining group (2) on the supporting surface (40).

### Claim 12 (depends on 11)

The device, according to claim 11, wherein:
the holding device (6) has a plurality of the pins (60) which project out of the lower tool (4) on the supporting surface (40), in the direction of the upper tool (3); and
the plurality of pins (60) are formed to be actively or passively movable relative to the upper tool (3).

### Claim 13 (depends on 12)

The device, according to claim 12, wherein:
respective head ends of the pins (60) that face the upper tool (3) form the holding means (62).

### Claim 14 (depends on 13)

The device, according to claim 13, wherein:
the holding device (6) further comprises:
a plurality of hooks (64) that project out of the upper tool (3) in the direction of the lower tool (4); and
the plurality of hooks (64) are formed to be actively or passively movable in perpendicular to the direction of the lower tool (4).

### Claim 15 (depends on 14)

The device, according to claim 14, wherein:
the joining group (2) further comprises the workpiece carrier (7) arranged on the holding device (6).

### Claim 16 (depends on 15)

The device, according to claim 15, wherein:
the heating apparatus (5) is formed to increase the temperature of the sintering agent (28) by at least 150K.