# US 2023/0382785 A1 · Semiconductor element coating glass and semiconductor element coating material using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0382785 A1
- Document ID: US20230382785A1
- Status: Published application
- Kind: A1
- Application number: 18/027,743
- Filed: 2021-09-21
- Published: 2023-11-30
- Earliest claimed: 2020-10-13
- Assignees: Nippon Electric Glass Co., Ltd.
- Applicants: Nippon Electric Glass Co., Ltd.
- Inventors: Masayuki HIROSE
- Web page: https://patentgrep.com/patent/US20230382785A1

## CPC

- C03C 3/105: containing aluminium
- C03C 3/108: containing boron
- C03C 8/10: containing lead
- C03C 8/14: Glass frit mixtures having non-frit additions, e.g. opacifiers, colorants, mill-additions
- C03C 8/24: Fusion seal compositions being frit compositions having non-frit additions, i.e. for use as seals between dissimilar materials, e.g. glass and metal; Glass solders
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The present invention provides a glass for semiconductor element coating including as a glass composition, in terms of mol %, 55% to 85% of SiO2, 12% to 40% of PbO, 0.1% to 10% of Al2O3, and 0.1% to 6% of GeO2+Ta2O5+Nb2O5+Bi2O3.

## Claims

### Claim 1

A glass for semiconductor element coating, comprising, as a glass composition, in terms of mol %, 55% to 85% of SiO2, 12% to 40% of PbO, 0.1% to 10% of Al2O3, and 0.1% to 6% of GeO2+Ta2O5+Nb2O5+Bi2O3.

### Claim 2 (depends on 1)

The glass for semiconductor element coating according to claim 1, wherein the glass has a content of GeO2 of from 0.1% to 6%.

### Claim 3 (depends on 1)

A material for semiconductor element coating, comprising:
75 mass % to 100 mass % of glass powder formed of the glass for semiconductor element coating of claim 1; and
0 mass % to 25 mass % of ceramic powder.

### Claim 4 (depends on 3)

The material for semiconductor element coating according to claim 3, wherein the material for semiconductor element coating has a thermal expansion coefficient within a temperature range of from 30° C. to 300° C. of from 20×10−7° C. to 55×10−7° C.