# US 2023/0357884 A1 · Low temperature direct reduction of metal oxides via the in situ production of reducing gas

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0357884 A1
- Document ID: US20230357884A1
- Status: Published application
- Kind: A1
- Application number: 18/352,745
- Filed: 2023-07-14
- Published: 2023-11-09
- Earliest claimed: 2016-11-23
- Assignees: Environmental Clean Technologies Limited
- Applicants: Environmental Clean Technologies Limited
- Inventors: Keith Michael HENLEY-SMITH; Adam David GILES; Lachlan Phillip Clive BARTSCH; Ashley Charles MOORE
- Web page: https://patentgrep.com/patent/US20230357884A1

## CPC

- C22B 1/245: with carbonaceous material for the production of coked agglomerates
- C21B 13/0066: {Preliminary conditioning of the solid carbonaceous reductant}
- C21B 13/0073: {Selection or treatment of the reducing gases}
- C21B 13/04: in retorts
- C22B 5/12: by gases
- Y02P 10/134: by avoiding CO2, e.g. using hydrogen
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A continuous process for low temperature reduction of metal oxides from carbonaceous material, using in situ produced reducing gas. In particular, a method of reducing metal oxide to metal in a continuous process comprising: (a) continuously introducing composite bodies comprising low rank carbonaceous material and metal oxide containing material that are in intimate contact and in a dry mix ratio of from about 1:2 to about 1:10 to an upper region of an upright retort; (b) conveying said bodies from said upper region to a heated lower region of said retort wherein said composite bodies are exposed to increasing temperature of up to about 950° C. and wherein said composite bodies are exposed to reducing gas generated in situ for a period of from about 15 minutes to about 3 hours to thereby produce a reduced metal containing product; and (c) continuously removing the reduced metal containing product from a lower

## Claims

### Claim 1

A method of reducing metal oxide to metal in a continuous process comprising:
a. continuously introducing composite bodies comprising low rank carbonaceous material having moisture content of from about 30% to about 70% and metal oxide containing material that are in intimate contact and in a dry mix ratio of from about 1:2 to about 1:10 by weight to an upper region of an upright retort;
b. conveying said bodies from said upper region to a heated lower region of said retort wherein said composite bodies are exposed to increasing temperature of up to about 950° C. and wherein said composite bodies are exposed to reducing gas generated in situ for a period of from about 15 minutes to about 3 hours to thereby produce a reduced metal containing product; and
c. continuously removing the reduced metal containing product from a lower region of the retort.

### Claim 2 (depends on 1)

The method according to claim 1 wherein the composite bodies comprising low rank carbonaceous material and metal oxide are produced by mixing/attritioning particulate low rank carbonaceous material and metal oxide containing material with optional addition of water to produce a plastic mass, forming moist composite bodies and drying to produce dried composite bodies.

### Claim 3 (depends on 2)

The method according to claim 2 wherein the metal oxide containing material is a metal oxide containing mineral ore or a metal oxide containing material produced as a product or by-product of an industrial process.

### Claim 4 (depends on 2)

The method of claim 2 wherein the moisture content of said dried composite bodies is up to about 15% w/w.

### Claim 5 (depends on 2)

The method according to claim 2 wherein the forming of moist composite bodies is by extrusion and the composite bodies are pellets.

### Claim 6 (depends on 1)

The method according to claim 1 wherein the dry mix ratio of low rank carbonaceous material to metal oxide containing material is from about 1:3 to about 1:9 by weight.

### Claim 7 (depends on 1)

The method according to claim 1 wherein the dry mix ratio of low rank carbonaceous material to metal oxide containing material is about 1:5 by weight.

### Claim 8 (depends on 1)

The method according to claim 1 wherein the low rank carbonaceous material is lignite or sub-bituminous coal.

### Claim 9 (depends on 1)

The method according to claim 1 wherein the low rank carbonaceous material is peat.

### Claim 10 (depends on 1)

The method according to claim 1 wherein the metal oxide containing material comprises one or more of ferrous oxide (FeO), hematite (Fe2O3), magnetite (Fe3O4), chromite (FeCr2O4), magnesiochromite (MgCr2O4), ilmenite (FeO·TiO2), manganese ore (Mn2O3) and limonite (Fe·Ni)O(OH)·H2O.

### Claim 11 (depends on 1)

The method according to claim 1 wherein said composite bodies are exposed to reducing gas generated in situ for a period of from about 20 minutes to about 2 hours.

### Claim 12 (depends on 1)

The method according to claim 1 wherein the reducing gas comprises gases selected from one or more of C1-C10 hydrocarbon, H2, CO, CO2 and H2O.

### Claim 13 (depends on 12)

The method according to claim 12 wherein the hydrocarbon comprises C1-C6 hydrocarbon.

### Claim 14 (depends on 1)

The method according to claim 1 wherein metal oxide reduction is primarily H2 gas reduction.

### Claim 15 (depends on 1)

The method according to claim 1 wherein metal oxide reduction occurs within the composite bodies due to reducing gas evolved within the composite bodies.