# US 2023/0357071 A1 · Water-containing glass-based articles with high indentation cracking threshold

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0357071 A1
- Document ID: US20230357071A1
- Status: Published application
- Kind: A1
- Application number: 18/218,748
- Filed: 2023-07-06
- Published: 2023-11-09
- Earliest claimed: 2017-11-17
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Timothy Michael Gross; Georgiy M. Guryanov
- Web page: https://patentgrep.com/patent/US20230357071A1

## CPC

- C03C 3/105: containing aluminium
- C03C 3/083: containing aluminium oxide or an iron compound
- C03B 2201/21: doped with molecular hydrogen
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 21/007: {in gaseous phase}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

Glass-based articles that include a hydrogen-containing layer extending from the surface of the article to a depth of layer. The hydrogen-containing layer includes a hydrogen concentration that decreases from a maximum hydrogen concentration to the depth of layer. The glass-based articles exhibit a high Vickers indentation cracking threshold. Glass compositions that are selected to promote the formation of the hydrogen-containing layer and methods of forming the glass-based article are also provided.

## Claims

### Claim 1

A glass article strengthened by steam treatment, comprising:
a surface of the glass article;
a hydrogen-containing layer extending from the surface into the glass article to a depth of layer, wherein the depth of layer refers to a first depth below the surface where hydrogen concentration matches a hydrogen concentration at a center of the glass article; and
a compressive stress layer from hydrogen species, the compressive stress layer extending from the surface of the glass article into the glass article to a depth of compression, wherein the depth of compression refers to the depth at which stress in the glass article changes from compressive to tensile;
wherein the depth of layer is greater than 5 μm from the surface; and
wherein the compressive stress layer comprises compressive stress of at least 100 MPa.

### Claim 2 (depends on 1)

The glass article of claim 1, wherein at least a portion of the compressive stress layer is free of larger alkali ions exchanged for smaller alkali ions, corresponding to traditional ion-exchange strengthening.

### Claim 3 (depends on 1)

The glass article of claim 1, further comprising a tensile stress region comprising a maximum central tension greater than or equal to 10 MPa.

### Claim 4 (depends on 1)

The glass article of claim 1, wherein a maximum hydrogen concentration is located at the surface of the glass-based article, and wherein hydrogen concentration of the hydrogen-containing layer decreases from the maximum hydrogen concentration to the depth of layer.

### Claim 5 (depends on 1)

The glass article of claim 1, wherein the hydrogen species comprise one or more of molecular water, hydroxyl, hydrogen ions, and hydronium.

### Claim 6 (depends on 1)

The glass article of claim 1, wherein the surface is a first surface of the glass article, and the glass article further comprises a second surface and a thickness that extends therebetween.

### Claim 7 (depends on 6)

The glass article of claim 6, wherein the depth of layer is greater than 0.005 times the thickness of the glass article.

### Claim 8 (depends on 7)

The glass article of claim 7, wherein the thickness is less than or equal to 2 mm.

### Claim 9 (depends on 6)

The glass article of claim 6, wherein the hydrogen-containing layer is a first hydrogen-containing layer, the depth of layer is a first depth of layer, and the glass article further comprises a second hydrogen containing layer extending from the second surface into the article to a second depth of layer; and wherein the glass article still further comprises a region between the first depth of layer and the second depth of layer, wherein the region is free of hydrogen species added by the steam treatment such that hydrogen concentration is substantially constant between the first depth of layer and the second depth of layer.

### Claim 10 (depends on 6)

The glass article of claim 6, wherein the article is shaped as a sheet such that the first and second surfaces are opposing major surfaces thereof.

### Claim 11 (depends on 10)

The glass article of claim 10, wherein the article has a 3D shape such that the first and second surfaces are at least partially nonplanar.

### Claim 12 (depends on 10)

The glass article of claim 10, comprising at least some transparency.

### Claim 13 (depends on 1)

A transportation article, comprising the glass article strengthened by steam treatment of claim 1 incorporated therein, wherein the transportation article is automotive.

### Claim 14 (depends on 1)

A device, comprising:
electrical components comprising a display; and
a cover overlaying the display, wherein at least a portion of the cover comprises the glass article strengthened by steam treatment of claim 1.

### Claim 15

A glass article, comprising:
a first surface, a second surface, and a thickness that extends therebetween, wherein the article is shaped as a sheet such that the first and second surfaces are opposing major surfaces thereof;
a hydrogen-containing layer extending from the first surface into the glass article to a depth of layer, wherein the depth of layer refers to a first depth below the first surface where hydrogen concentration matches a hydrogen concentration at a center of the glass article; and
a compressive stress layer from hydrogen species, the compressive stress layer extending from the first surface of the glass article into the glass article to a depth of compression, wherein the depth of compression refers to the depth at which stress in the glass article changes from compressive to tensile;
wherein the depth of layer is greater than or equal to 20 μm; and
wherein the compressive stress layer comprises compressive stress of at least 100 MPa.

### Claim 16 (depends on 15)

The glass article of claim 15, wherein the depth of layer is less than or equal to 195 μm.

### Claim 17 (depends on 16)

The glass article of claim 16, wherein the depth of compression is greater than 0.05 times the thickness.

### Claim 18 (depends on 17)

The glass article of claim 17, wherein the compressive stress layer is free of larger alkali ions exchanged for smaller alkali ions, corresponding to traditional ion-exchange strengthening.

### Claim 19 (depends on 18)

The glass article of claim 18, wherein the thickness is less than or equal to 2 mm.

### Claim 20

A glass article, comprising:
a first surface, a second surface, and a thickness that extends therebetween;
a first hydrogen-containing layer extending from the first surface into the glass article to a first depth of layer, wherein the first depth of layer refers to a first depth below the first surface where hydrogen concentration matches a hydrogen concentration at a center of the glass article;
a second hydrogen containing layer extending from the second surface into the article to a second depth of layer, wherein the second depth of layer refers to a first depth below the second surface where hydrogen concentration matches a hydrogen concentration at a center of the glass article;
a region between the first depth of layer and the second depth of layer, wherein hydrogen concentration is substantially constant between the first depth of layer and the second depth of layer;
a compressive stress layer from hydrogen species, the compressive stress layer extending from the first surface of the glass article into the glass article to a depth of compression, wherein the depth of compression refers to the depth at which stress in the glass article changes from compressive to tensile; and
a tensile stress region, whereby forces within the glass article are balanced;
wherein the first depth of layer is greater than 0.005 times the thickness and less than or equal to 0.205 times the thickness, wherein the thickness is less than or equal to 2 mm;
wherein the compressive stress layer comprises compressive stress of at least 100 MPa;
wherein at least a portion of the compressive stress layer is free of larger alkali ions exchanged into the glass for smaller alkali ions, corresponding to traditional ion-exchange strengthening; and
where the tensile stress region comprises a maximum central tension greater than or equal to 10 MPa.