# US 2023/0352727 A1 · Preparation method of lithium thiophosphate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0352727 A1
- Document ID: US20230352727A1
- Status: Published application
- Kind: A1
- Application number: 17/778,804
- Filed: 2020-11-20
- Published: 2023-11-02
- Earliest claimed: 2019-11-20
- Assignees: Solvay SA
- Applicants: Solvay SA
- Inventors: Marc-David Braida; Lauriane D'Alencon; Jean-Daniel Compain; Thierry Le Mercier
- Web page: https://patentgrep.com/patent/US20230352727A1

## CPC

- C01B 25/30: Alkali metal phosphates
- H01M 10/0562: Solid materials
- H01M 6/18: with solid electrolyte
- H01M 6/188: {Processes of manufacture}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present disclosure concerns a method for the preparation of lithium thiophosphate, as well as the products obtainable by said methods, and uses thereof especially as solid electrolytes. The method includes preparing a lithium thiophosphate including at least one step for the preparation of a solution S1 at a temperature T1 from −200° C. to 10° C. followed by a step for removing at least a portion of the solvent from solution S1 to obtain lithium thiophosphate. The solution S1 includes a solvent and at least P species under the form of (PS4)3−, Li species under the form of Li+, and remaining sulfur under the form of polysulfide. followed by a step for removing at least a portion of the solvent from said solution S1 to obtain lithium thiophosphate.

## Claims

### Claim 1

A method of preparing a lithium thiophosphate comprising at least one step for the preparation of a solution S1 at a temperature T1 from −200° C. to 10° C., the solution S1 comprising a solvent and at least P species in the form of (PS4)3−, Li species in the form of Li+, and remaining sulfur in the form of polysulfide, followed by a step for removing at least a portion of the solvent from the solution S1 to obtain lithium thiophosphate.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the solution S1 is obtained by admixing lithium sulfide and phosphorus sulfide in the solvent, at a temperature from −200° C. to 10° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the solution S1 is obtained from the following steps:
obtaining a precursor solution by admixing lithium sulfide in the solvent;
adding phosphorus sulfide into the precursor solution at a temperature from −200° C. to 10° C.; in order to obtain the solution S1.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the step for removing at least a portion of the solvent from the solution S1 is carried out at a temperature from 30° C. to 200° C.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the preparation of the solution S1 occurs in an inert atmosphere, under vacuum or under H2S flow.

### Claim 6 (depends on 1)

The method according to claim 1, wherein lithium thiophosphate is then thermally treated at a temperature from 150° C. to 700° C.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the solvent is able to dissolve lithium thiophosphate, lithium sulfide and phosphorus sulfide.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the solvent is an aliphatic alcohol.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the solvent is selected from the group consisting of: ethanol, methanol, and mixtures thereof.

### Claim 10

The method according to, wherein the temperature T1 is from −110° C. to 0° C.

### Claim 11 (depends on 1)

The method according claim 1, wherein the lithium thiophosphate is selected from the group consisting of: Li3PS4, Li7PS6, Li7P3S11, and Li9.6P3S12.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the solution S1 comprises at least 50% mol. of Li species under the form of Li+, with respect to the total amount in moles of lithium sulfide added in the solvent.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the solution S1 comprises at least 50% mol. of P species in the form of (PS4)3−, with respect to the total amount in moles of phosphorus sulfide added in the solvent.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the temperature T1 is from −100° C. to −50° C. and the step for removing at least a portion of the solvent from the solution S1 is carried out at a temperature comprised from 35° C. to 65° C.

### Claim 15 (depends on 1)

A lithium thiophosphate obtained from the method according to claim 1.

### Claim 16 (depends on 1)

The method of claim 1, further comprising, using the obtained lithium thiophosphate as a solid electrolyte.

### Claim 17 (depends on 15)

A solid electrolyte comprising the lithium thiophosphate of claim 15.

### Claim 18 (depends on 17)

An electrochemical device comprising the solid electrolyte of claim 17.

### Claim 19 (depends on 18)

A solid state battery comprising the solid electrolyte of claim 18.

### Claim 20 (depends on 19)

A vehicle comprising the solid state battery of claim 19.