# US 2023/0332347 A1 · Polyamino acid-grafted modified water-repellent fabric and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0332347 A1
- Document ID: US20230332347A1
- Status: Published application
- Kind: A1
- Application number: 18/027,301
- Filed: 2021-01-27
- Published: 2023-10-19
- Earliest claimed: 2020-09-28
- Assignees: Soochow University
- Applicants: Soochow University
- Inventors: Zhanxiong LI
- Web page: https://patentgrep.com/patent/US20230332347A1

## CPC

- D06M 13/513: with at least one carbon-silicon bond
- D06M 13/5135: {Unsaturated compounds containing silicon atoms}
- D06M 13/342: Amino-carboxylic acids; Betaines; Aminosulfonic acids; Sulfo-betaines
- D06M 13/352: having five-membered heterocyclic rings
- D06M 14/04: of vegetal origin, e.g. cellulose or derivatives thereof
- D06M 14/06: of animal origin, e.g. wool or silk
- D06M 15/59: Polyamides; Polyimides
- D06M 2101/06: cellulosic
- D06M 2101/12: Keratin fibres or silk
- D06M 2200/12: Hydrophobic properties
- D06M 2400/01: Creating covalent bondings between the treating agent and the fibre
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS

## Abstract

An amino group is grafted to a fiber surface, the ring-opening polymerization of aniline acid anhydride is initiated by the amino group on the fiber surface to form a graft chain, and a water-repellent fabric the fiber surface of which is modified by polyamino acid is prepared. The fabric treatment uses an amino group pre-grafted on a fiber surface as an initiator in the liquid phase, and initiates (substitutes), by means of ring-opening polymerization (ROP), aniline acid anhydride to complete graft polymerization on the fiber surface. The production conditions are mild, the preparation process of the product is simple, and operation is safe. In the disclosed water-repellent fabric obtained by chemical grafting, a functional protective layer on the fiber surface is covalently bonded to the fiber, thereby having excellent fastness without affecting the wearability of the fabric, thus the problem of a water-repellent fabric having poor fastness is solved.

## Claims

### Claim 1

A polyamino acid-grafted modified water-repellent fabric, wherein: the polyamino acid-grafted modified water-repellent fabric comprises a fabric and a polyamino acid graft chain on the fabric surface; the chemical structure of the polyamino acid graft chain is as follows:
wherein: R1, R2, R3 are independently selected from H, —CH3, —CH2CH3 or —CF3; R4 is —CH3 or —CH2CH3; R5 is —CH2— or —CH2CH2CH2 NH—; X is 0 or NH: n=3˜200.

### Claim 2 (depends on 1)

The polyamino acid-grafted modified water-repellent fabric according to the claim 1, wherein: the fabric is one or more of cotton fabric, linen fabric, wool fabric and silk fabric; the fiber in the fabric is any one or more of cotton, linen, wool, silk, etc., which is subject to the polyamino acid grafting modification to modify the polyamino acid graft chain of the fiber surface.

### Claim 3 (depends on 1)

A method of preparing the polyamino acid-grafted modified water-repellent fabric according to the claim 1, wherein: the method comprises the following steps: mixing the amino-pretreated fabric with aniline acid anhydride to obtain the polyamino acid-grafted modified water-repellent fabric; the aniline acid anhydride is as follows:
wherein: R1, R2, R3 are independently selected from H, —CH3, —CH2CH3 or —CF3; R4 is —CH3 or —CH2CH3.

### Claim 4 (depends on 3)

The method of preparing the polyamino acid-grafted modified water-repellent fabric according to the claim 3, wherein: the temperature of the reaction is 0-80° C., and the time is 1-120 h; the fabric pretreated with amino group is a fabric treated with amino silane coupling agent.

### Claim 5 (depends on 4)

The method of preparing the polyamino acid-grafted modified water-repellent fabric according to the claim 4, wherein: the reaction temperature is a four-step temperature rise.

### Claim 6 (depends on 3)

The method of preparing the polyamino acid-grafted modified water-repellent fabric according to the claim 3, wherein: N-phenyl-tert-butyloxycarboxyglycine is subject to the cyclization reaction under nitrogen protection to obtain aniline acid anhydride; the N-phenyl-tert-butyloxycarboxyglycine is as follows:
wherein: R1, R2, R3 are independently selected from H, —CH3, —CH2CH3 or —CF3; R4 is —CH3 or —CH2CH3.

### Claim 7 (depends on 6)

The method of preparing the polyamino acid-grafted modified water-repellent fabric according to the claim 6, wherein: in the presence of acid binding agent, n-phenylglycine reacts with Boc acid anhydride to obtain N-phenyl-tert-butyloxycarboxyglycine.

### Claim 8 (depends on 7)

The method of preparing the polyamino acid-grafted modified water-repellent fabric according to the claim 7, wherein: the acid binding agent is triethylamine or pyridine; the temperature of the reaction is 5-45° C., and the time is 0.1-24 h.

### Claim 9 (depends on 1)

An application of polyamino acid-grafted modified water-repellent fabric according to the claim 1 in the preparation of water-repellent materials.

### Claim 10 (depends on 9)

The application according to the claim 9, wherein: the water-repellent material has washing durability and degradability.