# US 2023/0323507 A1 · Method of recycling nickel from waste battery material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0323507 A1
- Document ID: US20230323507A1
- Status: Published application
- Kind: A1
- Application number: 18/040,744
- Filed: 2021-08-11
- Published: 2023-10-12
- Earliest claimed: 2020-08-20
- Assignees: Johnson Matthey Public Limited Company
- Applicants: Johnson Matthey Public Limited Company
- Inventors: Barbara BREEZE; Michael BROWNE; Benjamin EADE; Emma SCHOFIELD; Koen VANDAELE
- Web page: https://patentgrep.com/patent/US20230323507A1

## CPC

- C22B 23/021: {by reduction in solid state, e.g. by segregation processes}
- C22B 23/065: {carbonyl methods}
- C01G 53/10: Sulfates
- C22B 7/001: {Dry processes}
- C22B 7/002: {by treating with halogens, sulfur or compounds thereof; by carburising, by treating with hydrogen (hydriding)}
- C22B 7/007: {by acid leaching}
- C22B 23/0415: {with acids or salt solutions except ammonium salts solutions}
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- Y02E 60/10: Energy storage using batteries
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method is described for recycling nickel from waste battery material. The method includes providing waste battery material comprising a nickel-containing oxide, reducing the nickel in the waste battery material to the zero oxidation state to provide a reduced waste battery material, reacting the reduced waste battery material with carbon monoxide to form Ni(CO)4, and reacting the Ni(CO)4 with a source of sulfate to form NiSO4. The NiSO4 product is useful as a nickel feedstock in various processes which require a nickel source, including processes which prepare new battery materials.

## Claims

### Claim 1

A method of recycling nickel from waste battery material comprising:
(a) providing waste battery material comprising a nickel-containing compound;
(b) reducing at least some of the nickel in the waste battery material to the zero oxidation state to provide a reduced waste battery material;
(c) reacting the reduced waste battery material with carbon monoxide to form Ni(CO)4; and
(d) reacting the Ni(CO)4 with a source of sulfate to form NiSO4.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The method according to claim 1, wherein the nickel-containing compound is a mixed oxide further comprising one or more of lithium, cobalt and manganese and optionally further comprising one or more of iron, aluminium, copper and carbon.

### Claim 4 (depends on 1)

The method according to claim 1, wherein reducing the nickel comprises contacting the waste battery material with a reducing gas comprising H2, wherein the contacting with the reducing gas is carried out at a temperature of at least 500° C.

### Claim 5 (depends on 4)

The method according to claim 4, further comprising cooling the reduced waste battery material from the temperature of at least 500° C. to a temperature of from 45 to 85° C. after reduction and before reacting the reduced waste battery material with carbon monoxide.

### Claim 6 (depends on 4)

The method according to claim 4, wherein the reducing gas further comprises carbon monoxide.

### Claim 7 (depends on 1)

The method according to claim 1, wherein reacting the reduced waste battery material with carbon monoxide is carried out at a temperature of from 45 to 85° C.

### Claim 8 (depends on 7)

The method according to claim 7, wherein reacting the reduced waste battery material with carbon monoxide is carried out at an absolute pressure of from 110 kPa to 200 kPa.

### Claim 9 (depends on 1)

The method according to claim 1, wherein reacting the reduced waste battery material with carbon monoxide is carried out at a temperature of from 140 to 200° C.

### Claim 10 (depends on 9)

The method according to claim 9, wherein reacting the reduced waste battery material with carbon monoxide is carried out at a pressure of from 6 MPa to 8 MPa.

### Claim 11

(canceled)

### Claim 12 (depends on 1)

The method according to claim 1, wherein the source of sulfate is H2SO4 such that the Ni(CO)4 is reacted with the H2SO4 to form the NiSO4.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the H2SO4 is an aqueous solution having a concentration of from 10 to 35% based on the total mass of the solution.

### Claim 14 (depends on 12)

The method according to claim 12, wherein reacting the Ni(CO)4 with H2SO4 is carried out at under the same pressure as applied during the reaction of the reduced waste battery material with carbon monoxide.

### Claim 15 (depends on 12)

The method according to claim 12, wherein reacting the Ni(CO)4 with H2SO4 is carried out under conditions of temperature and pressure in which Ni(CO)4 is gaseous.

### Claim 16 (depends on 12)

The method according to claim 12, further comprising recycling at least some of the H2 which is generated as a by-product of the reaction between Ni(CO)4 and H2SO4, wherein the recycled H2 is fed back into the process.

### Claim 17 (depends on 12)

The method according to claim 12, further comprising recycling at least some of the CO which is generated as a by-product of the reaction between Ni(CO)4 and H2SO4, wherein the recycled CO is fed back into the process to react with the reduced waste battery material.

### Claim 18

(canceled)

### Claim 19 (depends on 12)

The method according to claim 12, wherein reacting the Ni(CO)4 with the H2SO4 to form the NiSO4 is done in the presence of HNO3 in addition to the H2SO4.

### Claim 20

(canceled)

### Claim 21

(canceled)

### Claim 22 (depends on 1)

The method according to claim 1, further comprising a formic acid leaching process before or after step (b).

### Claim 23

A method of recycling nickel from a waste battery material, wherein the method comprises:
reacting a composition comprising reduced battery material with carbon monoxide to form Ni(CO)4, wherein the reduced battery material comprises nickel in the zero oxidation state; and
reacting the Ni(CO)4 with a source of sulfate to form NiSO4.