# US 2023/0322619 A1 · Polluted co2 capturing with lime produced from phosphogypsum calcination using sulfur as non-co2 fuel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0322619 A1
- Document ID: US20230322619A1
- Status: Published application
- Kind: A1
- Application number: 17/707,144
- Filed: 2022-03-29
- Published: 2023-10-12
- Earliest claimed: 2022-03-28
- Assignees: Saudi Arabian Mining Company (Ma'aden)
- Applicants: Saudi Arabian Mining Company (Ma'aden)
- Inventors: Malik Mohammad Odeh AQEL
- Web page: https://patentgrep.com/patent/US20230322619A1

## CPC

- B01D 53/62: Carbon oxides
- C04B 7/367: {Avoiding or minimising carbon dioxide emissions}
- B01D 53/501: {by treating the gases with a solution or a suspension of an alkali or earth-alkali or ammonium compound}
- C04B 7/365: {by extracting part of the material from the process flow and returning it into the process after a separate treatment, e.g. in a separate retention unit under specific conditions}
- C04B 11/0283: {Fluidised beds}
- C04B 11/26: {strating from chemical gypsum}; starting from phosphogypsum or from waste, e.g. purification products of smoke (C04B11/02 takes precedence; chemical purification of smoke, fumes or exhaust gases B01D53/00 {purification of gypsum C01F11/46})
- B01D 2251/404: of calcium
- B01D 2251/602: Oxides
- B01D 2251/604: Hydroxides
- B01D 2257/502: Carbon monoxide
- B01D 2257/504: Carbon dioxide
- B01D 2258/02: Other waste gases
- B01D 2258/0283: Flue gases
- C04B 2111/00017: {Aspects relating to the protection of the environment}
- C04B 2111/00019: {Carbon dioxide sequestration}
- Y02P 20/129: Energy recovery, e.g. by cogeneration, H2recovery or pressure recovery turbines
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A new integrated method to capture polluted CO2 using CaO produced from phosphogypsum calcination using sulfur as non-CO2 fuel where (1) both pollutants of phosphogypsum and CO2 are transformed into environmentally neutral or useful products such as limestone or clinker and sulfuric acid; (2) low-CO2 CaO produced from calcination of phosphogypsum with sulfur as fuel can be used to produce low-CO2 clinker that replaces the use of high-CO2 limestone as raw material; (3) the use of sulfur as fuel to calcine phosphogypsum allows the production of low-cost sulfuric acid.

## Claims

### Claim 1

An integrated method to capture polluted CO2 with CaO produced from phosphogypsum calcination using sulfur as non-CO2 fuel, comprising the steps of:
(a) flowing exhaust gases in counter current first to a phosphogypsum calcination plant and second to a drying plant where phosphogypsum is fed from dry stack, as described in reactions (i), (ii), (iii), and (iv):
(i) sulfur burning: S + O2 = SO2 at an approximate temperature range of approximately 1100 to 1400° C.;
(ii) CaSO4 calcination: 2CaSO4 + C + heat = 2CaO + 2SO2 + CO2; where the reaction is carried out at an approximate temperature range of 1200 to 1400° C.;
(iii) pre-calcination of PG: CaSO4.2H2O + heat = CaSO4 + 2H2O(v); where the reaction is carried out at an approximate temperature range of approximately 650 to 950° C.;
(iv) drying of fee moisture: H2O(1) + heat = H2O(v); where the reaction is carried out at an approximate temperature range of approximately 350 to 650° C.;
(b) treating a SO2-rich stream flowing from the phosphogypsum drying plant in a plant using limited Ca(OH)2 washing, as described in reactions (v) and (vi):
where cooling is applied to carry out reactions (v) and (vi) at an approximate temperature range of 350 to 400° C.; and
feeding to a waste gas sulfuric acid plant;
(c) concentrating SO2-rich gas to a range of approximately 13 to 25% from the use of sulfur in the calcination plant with a reducing agent comprising C, and SO2 generated from PG calcination to a conventional sulfuric acid plant prior to the SO2 to SO3 conversion stage, where the SO2 is generated as described in reactions (vii) and (viii);
(vii) sulfur burning: S + O2 = SO2 carried out at a temperature range of approximately 1100-1400° C.;
(viii) CaSO4 calcination: 2CaSO4 + C + heat = 2CaO + 2SO2 + CO2; where the reaction is carried out at a temperature range of approximately 1200 to 1400° C.;
(d) sulfuric acid production in conventional SAP is carried as well defined in the reactions (ix) and (x):
where the reaction is carried out at an approximate temperature range of 350 to 500° C.;
where the reaction is conducted at an approximate temperature range of approximately 75 to 165° C.;
(e) utilizing sulfuric acid produced in the waste gas sulfuric acid plant for digesting phosphate rock to obtain phosphoric acid and byproduct phosphogypsum;
(f) stacking phosphogypsum for the drying plant;
(g) reacting CaO powder produced in the calcination plant with CO2 in a circular fluid bed reactor to obtain CaCO3, as described in reactions (xi):
where reaction is carried out at a temperature below approximately 650° C.;
(h) where the CO2 from step (f) is produced by acidic fumes from a source selected from the group consisting of a phosphoric acid plant, hydrocarbon fuel combustion, and hydrogen reformers;
(i) Utilizing CaO powder to precipitate acid fumes from phosphogypsum calcination, as described in reactions (xii), (xiii), and (xiv):
.

### Claim 2 (depends on 1)

The integrated method of claim 1, where the phosphogypsum is fed from dry stack at moisture level of 10 to 40%.

### Claim 3 (depends on 1)

The integrated method of claim 1, where the byproduct phosphogypsum is fed directly for the drying plant.

### Claim 4 (depends on 1)

The integrated method of claim 1, where reaction (ii) is carried out in the presence of a reducing agent at an approximate temperature range of 1100 to 1300° C. utilizing the heat generated by reaction (i).

### Claim 5 (depends on 1)

The integrated method of claim 1, where removal of crystalline and free water in (iii) and (iv), respectively, is carried out at an approximate temperature range of approximately 700 to 900° C. with waste heat from SO2 flues gases from reactions (i) and (ii).

### Claim 6 (depends on 1)

The integrated method of claim 1, where removal of crystalline and free water in (iii) and (iv), respectively, is utilized for cooling the SO2 flue gases below approximately 700° C.

### Claim 7 (depends on 1)

The integrated method of claim 1, where SO2 flue gases shall be cooled and dried to approximately 400° C.

### Claim 8 (depends on 1)

The integrated method of claim 1, where reaction (iv) is carried out at an approximate temperature range of 400-600° C.

### Claim 9 (depends on 1)

The integrated method of claim 1, where SO2-rich gas produced from reactions (i) and (ii) are concentrated to a range of approximately 16-20%.

### Claim 10 (depends on 1)

The integrated method of claim 1, where the reducing agent is a carbon source selected from the group consisting of coal, heavy fuel oil, crude oil, carbon mono-oxide and natural gas.

### Claim 11 (depends on 1)

The integrated method of claim 1, where reaction (xi) is carried out at a temperature below approximately 500° C. .

### Claim 12 (depends on 1)

The integrated method of claim 1, where the CaCO3 produced by reaction (xi) contains neutralized impurities coming originally from phosphogypsum and acidic fumes from polluted CO2.

### Claim 13 (depends on 12)

The integrated method of claim 12, where the impurities are selected from the group consisting of; CaSO4, CaF2, CaHPO4 and CaSiF6.

### Claim 14 (depends on 1)

The integrated method of claim 1, where sulfur is used as fuel for phosphogypsum calcination to produce sulfuric acid and lime to capture CO2 and produce limestone.

### Claim 15 (depends on 1)

The integrated method of claim 1, where the total consumption of sulfur in a waste gas sulfuric acid plant is reduced to below approximately 50% than the consumption of sulfur in a conventional sulfuric acid plant based on sulfur burning.

### Claim 16 (depends on 14)

The integrated method of claim 14, where approximately 75% excess energy is recovered, compared to the energy recovered from sulfur burning in a conventional sulfuric acid plant.

### Claim 17 (depends on 14)

The integrated method of claim 14, where the use of sulfur as fuel to calcine phosphogypsum allows the production of approximately 6 tons of sulfuric for every ton of sulfur.

### Claim 18 (depends on 14)

The integrated method of claim 14, where CaO produced from the calcination of phosphogypsum can be used in the production of low-CO2 clinker.

### Claim 19 (depends on 18)

The integrated method of claim 18, where the CaO utilized to produce low-CO2 clinker saves approximately 40-50% of the total energy required to produce clinker from phosphogypsum when sulfur is used as fuel compared to using only using hydrocarbon fuel.

### Claim 20 (depends on 18)

The integrated method of claim 18, where CaO utilized to produce low-CO2 clinker reduces clinker production’s net CO2 emissions by approximately 75% compared to conventional limestone-based clinker production.