# US 2023/0321705 A1 · Mold for preparing large-size rare earth magnesium alloy ingot without tail shrinkage by back pressure severe plastic deformation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0321705 A1
- Document ID: US20230321705A1
- Status: Published application
- Kind: A1
- Application number: 17/944,197
- Filed: 2022-09-14
- Published: 2023-10-12
- Earliest claimed: 2022-04-12
- Assignees: Shanxi Zhongbei Ruizhi Jingcheng Technology Co., Ltd.
- Applicants: Shanxi Zhongbei Ruizhi Jingcheng Technology Co., Ltd.
- Inventors: Zhimin Zhang; Jianmin Yu; Mei Cheng; Zhe Chen; Zhen Wang
- Web page: https://patentgrep.com/patent/US20230321705A1

## CPC

- B21C 23/001: {to improve the material properties, e.g. lateral extrusion}
- B21C 25/02: Dies
- B21C 23/002: {Extruding materials of special alloys so far as the composition of the alloy requires or permits special extruding methods of sequences}
- B21C 26/00: Rams or plungers for metal extruding; Discs therefor
- B21C 35/04: Cutting-off or removing waste
- B21J 5/08: Upsetting
- Y02P 70/10: Greenhouse gas [GHG] capture, material saving, heat recovery or other energy efficient measures, e.g. motor control, characterised by manufacturing processes, e.g. for rolling metal or metal working
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- B21J: FORGING; HAMMERING; PRESSING METAL; RIVETING; FORGE FURNACES (rolling of metal B21B; making particular products by forging or pressing B21K; cladding or plating B23K; finishing surfaces by hammering B23P9/04; compacting surfaces by blasting with particulate material B24C1/10; general features of presses, presses for consolidating scrap B30B; furnaces in general F27)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure discloses a mold for preparing large-size rare earth magnesium alloy ingot without tail shrinkage by back pressure severe plastic deformation, which includes a male mold, a female mold, a recoverable discard block and a back pressure plate connected with a pushing cylinder of the press machine. The female mold is provided with an upper mold cavity and a lower mold cavity, an upper part of the upper mold cavity is configured for placing blanks, the recoverable discard block and the male mold, and a lower part of the upper mold cavity is inclined inward to form an extrusion deformation area. The recoverable discard block is configured to be filled in an extrusion deformation area and restored through deformation. The present disclosure can solve the existence of the discard in the traditional forward extrusion and the tail shrinking phenomenon caused by the uneven metal flow.

## Claims

### Claim 1

A mold for preparing large-size rare earth magnesium alloy ingot without tail shrinkage by back pressure severe plastic deformation, comprising a male mold installed on an upper workbench of a press machine, a female mold installed on a lower workbench of the press machine, a recoverable discard block and a back pressure plate connected with a pushing cylinder of the press machine, wherein the female mold is provided with an upper mold cavity and a lower mold cavity, an upper part of the upper mold cavity is configured for placing blanks, the recoverable discard block and the male mold, and a lower part of the upper mold cavity is inclined inward to form an extrusion deformation area communicated with the lower mold cavity;
the recoverable discard block is separated between the blank and the male mold, the recoverable discard block is made of deformable material, and the recoverable discard block is configured to be deformed and filled in an extrusion deformation area and restored through deformation;
an upper part of the back pressure plate is fitted in the lower mold cavity, a molding cavity is formed between the upper part of the back pressure plate and the lower mold cavity, and an upper surface of the back pressure plate is raised in a middle.

### Claim 2 (depends on 1)

The mold for preparing large-size rare earth magnesium alloy ingot without tail shrinkage by back pressure severe plastic deformation according to claim 1, wherein the recoverable discard block is in a molten state at high temperature, and the recoverable discard block is a brittle solid at low temperature and is broken into solid powder when pressed in the extrusion deformation area.

### Claim 3 (depends on 2)

The mold for preparing large-size rare earth magnesium alloy ingot without tail shrinkage by back pressure severe plastic deformation according to claim 2, wherein the mold further comprises an extrusion restoration mold, wherein the recoverable discard block is crushed into solid powder under pressure and then put into the extrusion restoration mold to recover into the recoverable discard block.

### Claim 4 (depends on 3)

The mold for preparing large-size rare earth magnesium alloy ingot without tail shrinkage by back pressure severe plastic deformation according to claim 3, wherein the extrusion restoration mold comprises a pressing box and a pressing block, the pressing box is provided with a groove, the recoverable discard block is crushed into solid powder under pressure and placed in the groove, and the solid powder is restored into recoverable discard block under high temperature.

### Claim 5 (depends on 1)

The mold for preparing large-size rare earth magnesium alloy ingot without tail shrinkage by back pressure severe plastic deformation according to claim 1, wherein the recoverable residue block is made of a mixture of fluorite powder and graphite.

### Claim 6 (depends on 1)

The mold for preparing large-size rare earth magnesium alloy ingot without tail shrinkage by back pressure severe plastic deformation according to claim 1, wherein an upper part of the lower mold cavity is inclined to expand outward from top to bottom, so that a side part of the extrusion deformation area forms an annular inner flange.

### Claim 7 (depends on 1)

The mold for preparing large-size rare earth magnesium alloy ingot without tail shrinkage by back pressure severe plastic deformation according to claim 1, wherein a width of the lower mold cavity is greater than that of the upper mold cavity.

### Claim 8 (depends on 1)

The mold for preparing large-size rare earth magnesium alloy ingot without tail shrinkage by back pressure severe plastic deformation according to claim 1, wherein the back pressure plate is in T-shape.